Objectives: To compare the flexural cyclic fatigue resistance and the length of the fractured segments (FLs) of recently introduced M-Pro rotary files with that of RaCe rotary files in curved canals and to evaluate the fracture surface by scanning electron microscopy (SEM). Materials and Methods: Thirty-six endodontic files with the same tip size and taper (size 25, 0.06 taper) were used. The samples were classified into 2 groups (n = 18): the M-Pro group (M-Pro IMD) and the RaCe group (FKG). A custom-made simulated canal model was fabricated to evaluate the total number of cycles to failure and the FL. SEM was used to examine the fracture surfaces of the fragmented segments. The data were statistically analyzed and comparisons between the 2 groups for normally distributed numerical variables were carried out using the independent Student's t-test. A p value less than 0.05 was considered to indicate statistical significance. Results: The M-Pro group showed significantly higher resistance to flexural cyclic fatigue than the RaCe group (p < 0.05), but there was no significant difference in the FLs between the 2 groups (p ≥ 0.05). Conclusions: Thermal treatment of nickel-titanium instruments can improve the flexural cyclic fatigue resistance of rotary endodontic files, and the M-Pro rotary system seems to be a promising rotary endodontic file.
Abstract
Objectives: To compare the flexural cyclic fatigue resistance and the length of the fractured segments (FLs) of recently introduced M-Pro rotary files with that of RaCe rotary files in curved canals and to evaluate the fracture surface by scanning electron microscopy (SEM). Materials and Methods: Thirty-six endodontic files with the same tip size and taper (size 25, 0.06 taper) were used. The samples were classified into 2 groups (n = 18): the M-Pro group (M-Pro IMD) and the RaCe group (FKG). A custom-made simulated canal model was fabricated to evaluate the total number of cycles to failure and the FL. SEM was used to examine the fracture surfaces of the fragmented segments. The data were statistically analyzed and comparisons between the 2 groups for normally distributed numerical variables were carried out using the independent Student's t-test. A p value less than 0.05 was considered to indicate statistical significance. Results: The M-Pro group showed significantly higher resistance to flexural cyclic fatigue than the RaCe group (p < 0.05), but there was no significant difference in the FLs between the 2 groups (p ≥ 0.05). Conclusions: Thermal treatment of nickel-titanium instruments can improve the flexural cyclic fatigue resistance of rotary endodontic files, and the M-Pro rotary system seems to be a promising rotary endodontic file.
참고문헌 (37)
- Saunders Elizabeth M, "Hand instrumentation in root canal preparation", Endod Topics, 10, pp.163~167 (2005)
- Stavileci M, "Evaluation of root canal preparation using rotary system and hand instruments assessed by micro-computed tomography", Med Sci Monit Basic Res, 21, pp.123~130 (2015)
- Zupanc J, "New thermomechanically treated NiTi alloys-a review", Int Endod J, 51, pp.1088~1103 (2018)
- Parashos P, "Rotary NiTi instrument fracture and its consequences", J Endod, 32, pp.1031~1043 (2006)
- Yao JH, "Cyclic fatigue of three types of rotary nickel-titanium files in a dynamic model", J Endod, 32, pp.55~57 (2006)
- Martín B, "Factors influencing the fracture of nickel-titanium rotary instruments", Int Endod J, 36, pp.262~266 (2003)
- Gao Y, "Evaluation of the impact of raw materials on the fatigue and mechanical properties of ProFile Vortex rotary instruments", J Endod, 38, pp.398~401 (2012)
- Gambarini G, "Influence of different angles of reciprocation on the cyclic fatigue of nickel-titanium endodontic instruments", J Endod, 38, pp.1408~1411 (2012)
- Tripi TR, "Cyclic fatigue of different nickel-titanium endodontic rotary instruments", Oral Surg Oral Med Oral Pathol Oral Radiol Endod, 102, pp.e106~e114 (2006)
- Azimi S, "Cyclic fatigue resistance and fractographic analysis of RaCe and Protaper rotary NiTi instruments", Iran Endod J, 6, pp.80~86 (2011)
- "M-Pro rotary endodontic system"[URL]
- AlShwaimi E, "Cyclic fatigue resistance of a novel rotary file manufactured using controlled memory Ni-Ti technology compared to a file made from M-wire file", Int Endod J, 51, pp.112~117 (2018)
- Pruett JP, "Cyclic fatigue testing of nickel-titanium endodontic instruments", J Endod, 23, pp.77~85 (1997)
- Parashos P, "Factors influencing defects of rotary nickel-titanium endodontic instruments after clinical use", J Endod, 30, pp.722~725 (2004)
- Shen Y, "Defects in nickel-titanium instruments after clinical use. Part 2: fractographic analysis of fractured surface in a cohort study", J Endod, 35, pp.133~136 (2009)
- Yared GM, "Cyclic fatigue of Profile rotary instruments after simulated clinical use", Int Endod J, 32, pp.115~119 (1999)
- Plotino G, "A review of cyclic fatigue testing of nickel-titanium rotary instruments", J Endod, 35, pp.1469~1476 (2009)
- Elnaghy AM, "Cyclic fatigue resistance of ProTaper Next nickel-titanium rotary files", Int Endod J, 47, pp.1034~1039 (2014)
- Plotino G, "Blue treatment enhances cyclic fatigue resistance of vortex nickel-titanium rotary files", J Endod, 40, pp.1451~1453 (2014)
- Shen Y, "Fatigue testing of controlled memory wire nickel-titanium rotary instruments", J Endod, 37, pp.997~1001 (2011)
- Turpin YL, "Impact of two theoretical cross-sections on torsional and bending stresses of nickel-titanium root canal instrument models", J Endod, 26, pp.414~417 (2000)
- Chang SW, "Cyclic fatigue resistance, torsional resistance, and metallurgical characteristics of V taper 2 and V taper 2H rotary NiTi files", Scanning, 38, pp.564~570 (2016)
- Pedullà E, "Cyclic fatigue resistance of four nickel-titanium rotary instruments: a comparative study", Ann Stomatol (Roma), 3, pp.59~63 (2012)
- Plotino G, "Influence of size and taper of artificial canals on the trajectory of NiTi rotary instruments in cyclic fatigue studies", Oral Surg Oral Med Oral Pathol Oral Radiol Endod, 109, pp.e60~e66 (2010)
- Çapar ID, "Comparison of cyclic fatigue resistance of novel nickel-titanium rotary instruments", Aust Endod J, 41, pp.24~28 (2015)
- Çapar ID, "Comparison of the cyclic fatigue resistance of 5 different rotary pathfinding instruments made of conventional nickel-titanium wire, M-wire, and controlled memory wire", J Endod, 41, pp.535~538 (2015)
- Pedullà E, "Torsional and cyclic fatigue resistance of a new nickel titanium instrument manufactured by electrical discharge machining", J Endod, 42, pp.156~159 (2016)
- Topçuoğlu HS, "In vitro comparison of cyclic fatigue resistance of ProTaper Next, HyFlex CM, OneShape, and ProTaper Universal instruments in a canal with a double curvature", J Endod, 42, pp.969~971 (2016)
- Amato M, "Evaluation of cyclic fatigue resistance of modern nickel–titanium rotary instruments with continuous rotation", G Ital Endod, 31, pp.78~82 (2017)
- Karataşlıoglu E, "Cyclic fatigue resistance of novel rotary files manufactured from different thermal treated nickel-titanium wires in artificial canals", Niger J Clin Pract, 21, pp.231~235 (2018)
- Shen Y, "Current challenges and concepts of the thermomechanical treatment of nickel-titanium instruments", J Endod, 39, pp.163~172 (2013)
- Srivastava S, "Current strategies in metallurgical advances of 450 rotary NiTi instruments : a review", J Dent Health Oral Disord Ther, 9, pp.00333~ (2018)
- Subramaniam V, "Stress distribution in rotary nickel titanium instruments-a finite element analysis", J Conserv Dent, 10, pp.112~118 (2007)
- Plotino G, "A comparison of cyclic fatigue between used and new Mtwo Ni-Ti rotary instruments", Int Endod J, 39, pp.716~723 (2006)
- Oh SR, "A comparison of nickel-titanium rotary instruments manufactured using different methods and cross-sectional areas : ability to resist cyclic fatigue", Oral Surg Oral Med Oral Pathol Oral Radiol Endod, 109, pp.622~628 (2010)
- Grande NM, "Cyclic fatigue resistance and three-dimensional analysis of instruments from two nickel-titanium rotary systems", Int Endod J, 39, pp.755~763 (2006)
- Cheung GS, "Fatigue testing of a NiTi rotary instrument. Part 2: fractographic analysis", Int Endod J, 40, pp.619~625 (2007)