The effect of various veneering techniques on the marginal fit of zirconia copings
2
조회
0
다운로드
2
인용
0
참고문헌
키워드
초록
PURPOSE. This study aimed to evaluate the fit of zirconia ceramics before and after veneering, using 3 different veneering processes (layering, press-over, and CAD-on techniques). MATERIALS AND METHODS. Thirty standardized zirconia CAD/CAM frameworks were constructed and divided into three groups of 10 each. The first group was veneered using the traditional layering technique. Press-over and CAD-on techniques were used to veneer second and third groups. The marginal gap of specimens was measured before and after veneering process at 18 sites on the master die using a digital microscope. Paired t-test was used to evaluate mean marginal gap changes. One-way ANOVA and post hoc tests were also employed for comparison among 3 groups (α=.05). RESULTS. Marginal gap of 3 groups was increased after porcelain veneering. The mean marginal gap values after veneering in the layering group (63.06 μm) was higher than press-over (50.64 μm) and CAD-on (51.50 μm) veneered groups (P<.001). CONCLUSION. Three veneering methods altered the marginal fit of zirconia copings. Conventional layering technique increased the marginal gap of zirconia framework more than pressing and CAD on techniques. All ceramic crowns made through three different veneering methods revealed clinically acceptable marginal fit.
Abstract
PURPOSE. This study aimed to evaluate the fit of zirconia ceramics before and after veneering, using 3 different veneering processes (layering, press-over, and CAD-on techniques). MATERIALS AND METHODS. Thirty standardized zirconia CAD/CAM frameworks were constructed and divided into three groups of 10 each. The first group was veneered using the traditional layering technique. Press-over and CAD-on techniques were used to veneer second and third groups. The marginal gap of specimens was measured before and after veneering process at 18 sites on the master die using a digital microscope. Paired t-test was used to evaluate mean marginal gap changes. One-way ANOVA and post hoc tests were also employed for comparison among 3 groups (α=.05). RESULTS. Marginal gap of 3 groups was increased after porcelain veneering. The mean marginal gap values after veneering in the layering group (63.06 μm) was higher than press-over (50.64 μm) and CAD-on (51.50 μm) veneered groups (P<.001). CONCLUSION. Three veneering methods altered the marginal fit of zirconia copings. Conventional layering technique increased the marginal gap of zirconia framework more than pressing and CAD on techniques. All ceramic crowns made through three different veneering methods revealed clinically acceptable marginal fit.
참고문헌 (47)
- Sadowsky SJ, "An overview of treatment considerations for esthetic restorations: a review of the literature", J Prosthet Dent, 96, pp.433~442 (2006)
- Liu PR, "A panorama of dental CAD", CAM restorative systems, 2005, pp.26, 507~508
- Miyazaki T, "A review of dental CAD", CAM: current status and future perspectives from 20 years of experience, 2009, pp.28, 44~56
- Bachhav VC, "Zirconia-based fixed partial dentures:a clinical review", Quintessence Int, 42, pp.173~182 (2011)
- Contrepois M, "Marginal adaptation of ceramic crowns: a systematic review", J Prosthet Dent, 110, pp.447~454 (2013)
- Jacobs MS, "An investigation of dental luting cement solubility as a function of the marginal gap", J Prosthet Dent, 65, pp.436~442 (1991)
- Björn AL, "Marginal fit of restorations and its relation to periodontal bone level. II. Crowns", Odontol Revy, 21, pp.337~346 (1970)
- Schwartz NL, "Unserviceable crowns and fixed partial dentures: life-span and causes for loss of serviceability", J Am Dent Assoc, 81, pp.1395~1401 (1970)
- Bergenholtz G, "Bacterial leakage around dental restorations: its effect on the dental pulp", J Oral Pathol, 11, pp.439~450 (1982)
- Heintze SD, "Systematic reviews: I. The correlation between laboratory tests on marginal quality and bond strength. II. The correlation between marginal quality and clinical outcome", J Adhes Dent, 9, pp.77~106 (2007)
- McLean JW, "The estimation of cement film thickness by an in vivo technique", Br Dent J, 131, pp.107~111 (1971)
- Euán R, "Marginal adaptation of zirconium dioxide copings:influence of the CAD", CAM system and the finish line design, 2014, pp.112, 155~162
- Holmes JR, "Marginal fit of castable ceramic crowns", J Prosthet Dent, 67, pp.594~599 (1992)
- Holmes JR, "Considerations in measurement of marginal fit", J Prosthet Dent, 62, pp.405~408 (1989)
- Balkaya MC, "Influence of firing cycles on the margin distortion of 3 all-ceramic crown systems", J Prosthet Dent, 93, pp.346~355 (2005)
- Luthardt RG, "An innovative method for evaluation of the 3-D internal fit of CAD", CAM crowns fabricated after direct optical versus indirect laser scan digitizing, 2004, pp.17, 680~685
- Pelekanos S, "Micro-CT evaluation of the marginal fit of different In-Ceram alumina copings", Eur J Esthet Dent, 4, pp.278~292 (2009)
- Sorensen JA, "A standardized method for determination of crown margin fidelity", J Prosthet Dent, 64, pp.18~24 (1990)
- Kanat B, "Effect of various veneering techniques on mechanical strength of computer-controlled zirconia framework designs", J Prosthodont, 23, pp.445~455 (2014)
- Wimmer T, "Influence of abutment model materials on the fracture loads of three-unit fixed dental prostheses", Dent Mater J, 33, pp.717~724 (2014)
- Tsalouchou E, "Fatigue and fracture properties of yttria partially stabilized zirconia crown systems", Dent Mater, 24, pp.308~318 (2008)
- Beuer F, "High-strength CAD", CAM-fabricated veneering material sintered to zirconia copings-a new fabrication mode for all-ceramic restorations, 2009, pp.25, 121~128
- Pera P, "In vitro marginal adaptation of alumina porcelain ceramic crowns", J Prosthet Dent, 72, pp.585~590 (1994)
- Shearer B, "Influence of marginal configuration and porcelain addition on the fit of In-Ceram crowns", Biomaterials, 17, pp.1891~1895 (1996)
- Castellani D, "Thermal distortion of different materials in crown construction", J Prosthet Dent, 72, pp.360~366 (1994)
- 박현순, "Influence of porcelain veneering on the marginal fit of Digident and Lava CAD", CAM zirconia ceramic crowns, 2010, pp.2(2), 33~38[DOI]
- Fahmy NZ, "Influence of veneering materials on the marginal fit and fracture resistance of an alumina core system", J Prosthodont, 20, pp.45~51 (2011)
- Kohorst P, "Influence of the veneering process on the marginal fit of zirconia fixed dental prostheses", J Oral Rehabil, 37, pp.283~291 (2010)
- Sulaiman F, "A comparison of the marginal fit of In-Ceram, IPS Empress, and Procera crowns", Int J Prosthodont, 10, pp.478~484 (1997)
- Cho SH, "The effect of multiple firings on the marginal integrity of pressable ceramic single crowns", J Prosthet Dent, 107, pp.17~23 (2012)
- Miura S, "Fit of zirconia allceramic crowns with different cervical margin designs, before and after porcelain firing and glazing", Dent Mater J, 33, pp.484~489 (2014)
- Rosensteil SF, "Contemporary fixed prosthodontics. Tooth preparation for All-ceramic restorations", pp.326~ (2006), Elsevier
- Alghazzawi TF, "The effect of different fabrication steps on the marginal adaptation of two types of glass-infiltrated ceramic crown copings fabricated by CAD", CAM technology, 2012, pp.21, 167~172
- Sorensen JA, "A standardized method for determination of crown margin fidelity", J Prosthet Dent, 64, pp.18~24 (1990)
- Ushiwata O, "Method for marginal measurements of restorations: accessory device for toolmakers microscope", J Prosthet Dent, 83, pp.362~366 (2000)
- Christensen GJ, "Marginal fit of gold inlay castings", J Prosthet Dent, 16, pp.297~305 (1966)
- Euán R, "Comparison of the marginal adaptation of zirconium dioxide crowns in preparations with two different finish lines", J Prosthodont, 21, pp.291~295 (2012)
- Kokubo Y, "Clinical marginal and internal gaps of Procera AllCeram crowns", J Oral Rehabil, 32, pp.526~530 (2005)
- Lee KB, "Marginal and internal fit of all-ceramic crowns fabricated with two different CAD", CAM systems, 2008, pp.27, 422~426
- Hirasankar Bhowmik, "A comparison of marginal fit of glass infiltrated alumina copings fabricated using two different techniques and the effect of firing cycles over them", The Journal of Advanced of Prosthodontics, 3(4), pp.196~203 (2011), 대한치과보철학회
- Weaver JD, "Marginal adaptation of castable ceramic crowns", J Prosthet Dent, 66, pp.747~753 (1991)
- DeHoff PH, "Thermal compatibility of dental ceramic systems using cylindrical and spherical geometries", Dent Mater, 24, pp.744~752 (2008)
- Nielsen JP, "Calculation of interfacial stress in dental porcelain bonded to gold alloy substrate", J Dent Res, 51, pp.1043~1047 (1972)
- Aboushelib MN, "Prestresses in bilayered all-ceramic restorations", J Biomed Mater Res B Appl Biomater, 87, pp.139~145 (2008)
- Isgrò G, "The effects of thermal mismatch and fabrication procedures on the deflection of layered all-ceramic discs", Dent Mater, 21, pp.649~655 (2005)
- Fairhurst CW, "Thermal expansion of dental alloys and porcelains", J Biomed Mater Res, 14, pp.435~446 (1980)
- Isgrò G, "Thermal dimensional behavior of dental ceramics", Biomaterials, 25, pp.2447~2453 (2004)