Effect of repetitive firing on passive fit of metal substructure produced by the laser sintering in implantsupported fixed prosthesis

2

조회

0

다운로드

0

인용

0

참고문헌

키워드

초록

PURPOSE. The aim of the present study was to investigate the passive fit of metal substructure after repetitive firing processes in implant-supposed prosthesis. MATERIALS AND METHODS. Five implants (4 mm diameter and 10 mm length) were placed into the resin-based mandibular model and 1-piece of screw-retained metal substructure was produced with the direct metal laser sintering (DMSL) method using Co-Cr compound (n = 10). The distance between the marked points on the multiunit supports and the marginal end of the substructure was measured using a scanning electron microscope (SEM) at each stage (metal, opaque, dentin, and glaze). 15 measurements were taken from each prosthesis, and 150 measurements from 10 samples were obtained. In total, 600 measurements were carried out at 4 stages. One-way ANOVA test was used for statistical evaluation of the data. RESULTS. When the obtained marginal range values were examined, differences between groups were found to be statistically significant (P<.001). The lowest values were found in the metal stage (172.4 ± 76.5 μm) and the highest values (238.03 ± 118.92 μm) were determined after glaze application. When the interval values for groups are compared with pairs, the differences between metal with dentin, metal with glaze, opaque with dentin, opaque with glaze, and dentin with glaze were found to be significant (P<.05), whereas the difference between opaque with metal was found to be insignificant (P=.992). CONCLUSION. Passive fit of 1-piece designed implant-retained fixed prosthesis that is supported by multiple implants is negatively affected by repetitive firing processes.

Abstract

PURPOSE. The aim of the present study was to investigate the passive fit of metal substructure after repetitive firing processes in implant-supposed prosthesis. MATERIALS AND METHODS. Five implants (4 mm diameter and 10 mm length) were placed into the resin-based mandibular model and 1-piece of screw-retained metal substructure was produced with the direct metal laser sintering (DMSL) method using Co-Cr compound (n = 10). The distance between the marked points on the multiunit supports and the marginal end of the substructure was measured using a scanning electron microscope (SEM) at each stage (metal, opaque, dentin, and glaze). 15 measurements were taken from each prosthesis, and 150 measurements from 10 samples were obtained. In total, 600 measurements were carried out at 4 stages. One-way ANOVA test was used for statistical evaluation of the data. RESULTS. When the obtained marginal range values were examined, differences between groups were found to be statistically significant (P<.001). The lowest values were found in the metal stage (172.4 ± 76.5 μm) and the highest values (238.03 ± 118.92 μm) were determined after glaze application. When the interval values for groups are compared with pairs, the differences between metal with dentin, metal with glaze, opaque with dentin, opaque with glaze, and dentin with glaze were found to be significant (P<.05), whereas the difference between opaque with metal was found to be insignificant (P=.992). CONCLUSION. Passive fit of 1-piece designed implant-retained fixed prosthesis that is supported by multiple implants is negatively affected by repetitive firing processes.

참고문헌 (33)

  1. Sailer I, "Cemented and screw-retained implant reconstructions : a systematic review of the survival and complication rates", Clin Oral Implants Res, 23, pp.163~201 (2012)
  2. Wittneben JG, "Clinical performance of screw-versus cement-retained fixed implant-supported reconstructions-a systematic review", Int J Oral Maxillofac Implants, 29, pp.84~98 (2014)
  3. Millen C, "Influence of prosthesis type and retention mechanism on complications with fixed implant-supported prostheses : a systematic review applying multivariate analyses", Int J Oral Maxillofac Implants, 30, pp.110~124 (2015)
  4. Yannikakis S, "Improving the fit of implant prosthetics : an in vitro study", Int J Oral Maxillofac Implants, 28, pp.126~134 (2013)
  5. Rungruanganunt P, "The effect of static load on dental implant survival : a systematic review", Int J Oral Maxillofac Implants, 28, pp.1218~1225 (2013)
  6. Al-Otaibi HN, "The effects of two torque values on the screw preload of implant-supported prostheses with passive fit or misfit", Int J Oral Maxillofac Implants, 29, pp.1058~1063 (2014)
  7. Ucar Y, "Internal fit evaluation of crowns prepared using a new dental crown fabrication technique : laser-sintered Co-Cr crowns", J Prosthet Dent, 102, pp.253~259 (2009)
  8. Witkowski S, "CAM in dental technology", Quintessence Dent Technol, 128, pp.169~184 (2005)
  9. Wu L, "Evaluation of the mechanical properties and porcelain bond strength of cobalt-chromium dental alloy fabricated by selective laser melting", J Prosthet Dent, 111, pp.51~55 (2014)
  10. Shillingburg HT, "Fundamentals of fixed prosthodontics" (2010), Quintessence Publishing Company
  11. Colpani JT, "Evaluation of marginal and internal fit of ceramic crown copings", Dent Mater, 29, pp.174~180 (2013)
  12. Zeng L, "Effects of repeated firing on the marginal accuracy of Co-Cr copings fabricated by selective laser melting", J Prosthet Dent, 113, pp.135~139 (2015)
  13. Quante K, "Marginal and internal fit of metal-ceramic crowns fabricated with a new laser melting technology", Dent Mater, 24, pp.1311~1315 (2008)
  14. Lakhani SA, "Influence of cold working and thermal treatment on the fit of implant-supported metal-ceramic fixed partial dentures", J Prosthet Dent, 88, pp.159~169 (2002)
  15. Gemalmaz D, "Distortion of metal-ceramic fixed partial dentures resulting from metal-conditioning firing", Quintessence Int, 27, pp.193~201 (1996)
  16. Gemalmaz D, "Marginal fit changes during porcelain firing cycles", J Prosthet Dent, 73, pp.49~54 (1995)
  17. Balkaya MC, "Influence of firing cycles on the margin distortion of 3 all-ceramic crown systems", J Prosthet Dent, 93, pp.346~355 (2005)
  18. Shillingburg HT Jr, "Preparation design and margin distortion in porcelain-fused-to-metal restorations", J Prosthet Dent, 29, pp.276~284 (1973)
  19. DeHoff PH, "Analysis of thermallyinduced stresses in porcelain-metal systems", J Dent Res, 62, pp.593~597 (1983)
  20. Campbell SD, "Effects of firing cycle and surface finishing on distortion of metal ceramic castings", J Prosthet Dent, 74, pp.476~481 (1995)
  21. Ando N, "Deformation of porcelain bonded gold alloys", J Jpn Soc Appar Mater, 13, pp.237~248 (1972)
  22. Dederich DN, "The effect of repeated firings on the margins of nonprecious ceramometals", J Prosthet Dent, 51, pp.628~630 (1984)
  23. Hamaguchi H, "Marginal distortion of the porcelain-bonded-to-metal complete crown : an SEM study", J Prosthet Dent, 47, pp.146~153 (1982)
  24. DeHoff PH, "Effect of metal design on marginal distortion of metal-ceramic crowns", J Dent Res, 63, pp.1327~1331 (1984)
  25. Anusavice KJ, "Effect of incompatibility stress on the fit of metal-ceramic crowns", J Dent Res, 66, pp.1341~1345 (1987)
  26. Harish V, "Evaluation of internal and marginal fit of two metal ceramic system-in vitro study", J Clin Diag Res, 8, pp.53~56 (2014)
  27. Pompa G, "Comparison of conventional methods and laser-assisted rapid prototyping for manufacturing fixed dental prostheses: An in vitro study", Biomed Res Int, 2015, pp.318097~ (2015)
  28. Castillo-Oyagüe R, "The effect of surface treatments on the microroughness of laser-sintered and vacuum-cast base metal alloys for dental prosthetic frameworks", Microsc Res Tech, 75, pp.1206~1212 (2012)
  29. Örtorp A, "The fit of cobalt-chromium three-unit fixed dental prostheses fabricated with four different techniques : a comparative in vitro study", Dent Mater, 27, pp.356~363 (2011)
  30. Xu D, "The marginal fit of selective laser melting-fabricated metal crowns : an in vitro study", J Prosthet Dent, 112, pp.1437~1440 (2014)
  31. Iseri U, "Shear bond strengths of veneering porcelain to cast, machined and laser-sintered titanium", Dent Mater J, 30, pp.274~280 (2011)
  32. Xiang N, "Metal-ceramic bond strength of Co-Cr alloy fabricated by selective laser melting", J Dent, 40, pp.453~457 (2012)
  33. Almeida e Silva JS, "Marginal and internal fit of four-unit zirconia fixed dental prostheses based on digital and conventional impression techniques", Clin Oral Investig, 18, pp.515~523 (2014)

관련 논문AI추천

Role of span length in the adaptation of implant-supported cobalt chromium frameworks fabricated by three techniquesHuang Yiqing, Li Yong, Ma Xiao, Wang Jiawei, Zhou Ying대한치과보철학회 · The Journal of Advanced of Prosthodontics2017 · 제9권 제2호Prosthetic misfit of implant-supported prosthesis obtained by an alternative section methodFa′bio Afra∧nio de Aguiar Ju′nior, Hilmo Barreto Leite Falcão-Filho, Maria da Gloria Chiarello de Mattos, Renata Cristina Silveira Rodrigues, Ricardo Faria Ribeiro, Rodrigo Tiossi대한치과보철학회 · The Journal of Advanced of Prosthodontics2012 · 제4권 제2호Fit analysis of implant-supported Co-Cr bars fabricated using casting, selective laser sintering, soft and dense milling techniquesElif Yiğit, Volkan Şahin대한치과보철학회 · The Journal of Advanced of Prosthodontics2025 · 제17권 제4호Clinical gap changes after porcelain firing cycles of zirconia fixed denturesBugurman Burcu Bugurman, Sebnem Begum Turker대한치과보철학회 · The Journal of Advanced of Prosthodontics2014 · 제6권 제3호Evaluation and comparison of the marginal adaptation of two different substructure materialsAli Ihsan Zengingul, Ebru Sumer, Sabiha Zelal Ulku, Sedat Guven, Tahir Karaman, Veysel Eratilla대한치과보철학회 · The Journal of Advanced of Prosthodontics2015 · 제7권 제3호Comparative clinical study of the marginal discrepancy of fixed dental prosthesis fabricated by the millingsintering method using a presintered alloy권태엽, 김미주, 김재원, 이두형, 이청희, 최용도, Hang-Nga Mai대한치과보철학회 · The Journal of Advanced of Prosthodontics2019 · 제11권 제5호

이 간행물의 다른 논문 (8건)