The effect of continuous application of MDP-containing primer and luting resin cement on bond strength to tribochemical silica-coated Y-TZP
1
조회
0
다운로드
2
인용
0
참고문헌
키워드
초록
Objectives This study investigated the effect of continuous application of 10-methacryloyloxydecyldihydrogen phosphate (MDP)-containing primer and luting resin cement on bond strength to tribochemical silica-coated yttria-stabilized tetragonal zirconia polycrystal (Y-TZP). Materials and Methods Forty bovine teeth and Y-TZP specimens were prepared. The dentin specimens were embedded in molds, with one side of the dentin exposed for cementation with the zirconia specimen. The Y-TZP specimen was prepared in the form of a cylinder with a diameter of 3 mm and a height of 10 mm. The bonding surface of the Y-TZP specimen was sandblasted with silica-coated aluminium oxide particles. The forty tribochemical silica-coated Y-TZP specimens were cemented to the bovine dentin (4 groups; n = 10) with either an MDP-free primer or an MDP-containing primer and either an MDP-free resin cement or an MDP-containing resin cement. After a shear bond strength (SBS) test, the data were analyzed using 1-way analysis of variance and the Tukey test (α = 0.05). Results The group with MDP-free primer and resin cement showed significantly lower SBS values than the MDP-containing groups (p < 0.05). Among the MDP-containing groups, the group with MDP-containing primer and resin cement showed significantly higher SBS values than the other groups (p < 0.05). Conclusions The combination of MDP-containing primer and luting cement following tribochemical silica coating to Y-TZP was the best choice among the alternatives tested in this study.
Abstract
Objectives This study investigated the effect of continuous application of 10-methacryloyloxydecyldihydrogen phosphate (MDP)-containing primer and luting resin cement on bond strength to tribochemical silica-coated yttria-stabilized tetragonal zirconia polycrystal (Y-TZP). Materials and Methods Forty bovine teeth and Y-TZP specimens were prepared. The dentin specimens were embedded in molds, with one side of the dentin exposed for cementation with the zirconia specimen. The Y-TZP specimen was prepared in the form of a cylinder with a diameter of 3 mm and a height of 10 mm. The bonding surface of the Y-TZP specimen was sandblasted with silica-coated aluminium oxide particles. The forty tribochemical silica-coated Y-TZP specimens were cemented to the bovine dentin (4 groups; n = 10) with either an MDP-free primer or an MDP-containing primer and either an MDP-free resin cement or an MDP-containing resin cement. After a shear bond strength (SBS) test, the data were analyzed using 1-way analysis of variance and the Tukey test (α = 0.05). Results The group with MDP-free primer and resin cement showed significantly lower SBS values than the MDP-containing groups (p < 0.05). Among the MDP-containing groups, the group with MDP-containing primer and resin cement showed significantly higher SBS values than the other groups (p < 0.05). Conclusions The combination of MDP-containing primer and luting cement following tribochemical silica coating to Y-TZP was the best choice among the alternatives tested in this study.
참고문헌 (35)
- Piconi C, "Zirconia as a ceramic biomaterial", Biomaterials, 20, pp.1~25 (1999)[DOI]
- Denry I, "State of the art of zirconia for dental applications", Dent Mater, 24, pp.299~307 (2008)[DOI]
- Manicone PF, "An overview of zirconia ceramics: basic properties and clinical applications", J Dent, 35, pp.819~826 (2007)[DOI]
- Beuer F, "Digital dentistry: an overview of recent developments for CAD", CAM generated restorations, 2008, pp.204, 505~511
- Gomes AL, "Zirconia implant abutments: a review", Med Oral Patol Oral Cir Bucal, 16, pp.e50~e55 (2011)
- Badwal SP, "Zirconia-based solid electrolytes: microstructure, stability and ionic conductivity", Solid State Ion, 52, pp.23~32 (1992)[DOI]
- Mondal P, "Investigation of the complex conductivity of nanocrystalline <TEX>$Y_{2}O_{3}$<", TEX>-stabilized zirconia, 1997, pp.101, 1765~1768
- Amaral R, "Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: the effect of surface conditioning", Dent Mater, 22, pp.283~290 (2006)[DOI]
- Valandro LF, "Microtensile bond strength of a resin cement to silica-coated and silanized In-Ceram Zirconia before and after aging", Int J Prosthodont, 20, pp.70~72 (2007)
- Tanaka R, "Cooperation of phosphate monomer and silica modification on zirconia", J Dent Res, 87, pp.666~670 (2008)[DOI]
- Ruttermann S, "The effect of different bonding techniques on ceramic", resin shear bond strength, 2008, pp.10, 197~203
- Piwowarczyk A, "The shear bond strength between luting cements and zirconia ceramics after two pre-treatments", Oper Dent, 30, pp.382~388 (2005)
- Lehmann F, "Durability of resin bonding to zirconia ceramic using different primers", J Adhes Dent, 11, pp.479~483 (2009)
- Kitayama S, "Effect of primer treatment on bonding resin cements to zirconia ceramic", Dent Mater, 26, pp.426~432 (2010)[DOI]
- Kern M, "Surface conditioning influences zirconia ceramic bonding", J Dent Res, 88, pp.817~822 (2009)[DOI]
- Ozcan M, "Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging", Dent Mater J, 27, pp.99~104 (2008)[DOI]
- Karimipour-Saryazdi M, "Influence of surface treatment of yttrium-stabilized tetragonal zirconium oxides and cement type on crown retention after artificial aging", J Prosthet Dent, 111, pp.395~403 (2014)[DOI]
- Blatz MB, "In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling", J Prosthet Dent, 91, pp.356~362 (2004)[DOI]
- Kern M, "Bonding to zirconia ceramic: adhesion methods and their durability", Dent Mater, 14, pp.64~71 (1998)[DOI]
- Yoshida K, "Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler", J Biomed Mater Res B Appl Biomater, 77, pp.28~33 (2006)
- Palacios RP, "Retention of zirconium oxide ceramic crowns with three types of cement", J Prosthet Dent, 96, pp.104~114 (2006)[DOI]
- Valandro LF, "Bond strength of a resin cement to high-alumina and zirconia-reinforced ceramics: the effect of surface conditioning", J Adhes Dent, 8, pp.175~181 (2006)
- Thompson JY, "Adhesion", cementation to zirconia and other non-silicate ceramics: where are we now?, 2011, pp.27, 71~82
- Shin YJ, "Evaluation of the shear bond strength of resin cement to Y-TZP ceramic after different surface treatments", Scanning, 36, pp.479~486 (2014)[DOI]
- Kosmac T, "The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic", Dent Mater, 15, pp.426~433 (1999)[DOI]
- Guazzato M, "Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina", zirconia-reinforced dental ceramic, 2005, pp.21, 454~463
- Wolfart M, "Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods", Dent Mater, 23, pp.45~50 (2007)[DOI]
- Akgungor G, "Influence of different surface treatments on the short-term bond strength and durability between a zirconia post and a composite resin material", J Prosthet Dent, 99, pp.388~399 (2008)[DOI]
- Matinlinna JP, "Evaluation of resin adhesion to zirconia ceramic using some organosilanes", Dent Mater, 22, pp.824~831 (2006)[DOI]
- Wegner SM, "Long-term resin bond strength to zirconia ceramic", J Adhes Dent, 2, pp.139~147 (2000)
- Yanagida H, "Adhesive bonding of composite material to cast titanium with varying surface preparations", J Oral Rehabil, 29, pp.121~126 (2002)[DOI]
- Fonseca RG, "Effect of metal primers on bond strength of resin cements to base metals", J Prosthet Dent, 101, pp.262~268 (2009)[DOI]
- Byeon SM, "Shear bond strength of <TEX>$Al_{2}O_{3}$<", TEX> sandblasted Y-TZP ceramic to the orthodontic metal bracket, 2017, pp.10, 148~
- Cavalcanti AN, "Bond strength of resin cements to a zirconia ceramic with different surface treatments", Oper Dent, 34, pp.280~287 (2009)[DOI]
- Zandparsa R, "An in vitro comparison of shear bond strength of zirconia to enamel using different surface treatments", J Prosthodont, 23, pp.117~123 (2014)[DOI]