PURPOSE. One of the most important factors in evaluating the quality of fixed dental prostheses (FDPs) is their gap. The purpose of this study was to compare the marginal and internal gap of two different metal-ceramic crowns, casting and selective laser sintering (SLS), before and after porcelain firing. Furthermore, this study evaluated whether metal-ceramic crowns made using the SLS have the same clinical acceptability as crowns made by the traditional casting. MATERIALS AND METHODS. The 10 study models were produced using stone. The 20 specimens were produced using the casting and the SLS methods; 10 samples were made in each group. After the core gap measurements, 10 metal-ceramic crowns in each group were finished using the conventional technique of firing porcelain. The gap of the metal-ceramic crowns was measured. The marginal and internal gaps were measured by two-dimensional and three-dimensional replica techniques, respectively. The Wilcoxon signed-rank test, the Wilcoxon rank-sum test and nonparametric ANCOVA were used for statistical analysis (α=.05). RESULTS. In both groups, the gap increased after completion of the metal-ceramic crown compared to the core. In all measured areas, the gap of the metal cores and metal-ceramic crowns produced by the SLS was greater than that of the metal cores and metal-ceramic crowns produced using the casting. Statistically significant differences were found between cast and SLS (metal cores and metal-ceramic crown). CONCLUSION. Although the gap of the FDPs produced by the SLS was greater than that of the FDPs produced by the conventional casting in all measured areas, none exceeded the clinically acceptable range.

Abstract

PURPOSE. One of the most important factors in evaluating the quality of fixed dental prostheses (FDPs) is their gap. The purpose of this study was to compare the marginal and internal gap of two different metal-ceramic crowns, casting and selective laser sintering (SLS), before and after porcelain firing. Furthermore, this study evaluated whether metal-ceramic crowns made using the SLS have the same clinical acceptability as crowns made by the traditional casting. MATERIALS AND METHODS. The 10 study models were produced using stone. The 20 specimens were produced using the casting and the SLS methods; 10 samples were made in each group. After the core gap measurements, 10 metal-ceramic crowns in each group were finished using the conventional technique of firing porcelain. The gap of the metal-ceramic crowns was measured. The marginal and internal gaps were measured by two-dimensional and three-dimensional replica techniques, respectively. The Wilcoxon signed-rank test, the Wilcoxon rank-sum test and nonparametric ANCOVA were used for statistical analysis (α=.05). RESULTS. In both groups, the gap increased after completion of the metal-ceramic crown compared to the core. In all measured areas, the gap of the metal cores and metal-ceramic crowns produced by the SLS was greater than that of the metal cores and metal-ceramic crowns produced using the casting. Statistically significant differences were found between cast and SLS (metal cores and metal-ceramic crown). CONCLUSION. Although the gap of the FDPs produced by the SLS was greater than that of the FDPs produced by the conventional casting in all measured areas, none exceeded the clinically acceptable range.

참고문헌 (30)

  1. Miyazaki T, "A review of dental CAD", CAM: current status and future perspectives from 20 years of experience, 2009, pp.28, 44~56
  2. Akova T, "Comparison of the bond strength of laser-sintered and cast base metal dental alloys to porcelain", Dent Mater, 24, pp.1400~1404 (2008)
  3. Campbell SD, "Thermal cycling distortion of metal ceramics: Part I--Metal collar width", J Prosthet Dent, 67, pp.603~608 (1992)
  4. Fonseca JC, "Stress-relieving and porcelain firing cycle influence on marginal fit of commercially pure titanium and titanium-aluminum-vanadium copings", Dent Mater, 19, pp.686~691 (2003)
  5. Lakhani SA, "Tallents RH. Influence of cold working and thermal treatment on the fit of implant-supported metal-ceramic fixed partial dentures", J Prosthet Dent, 88, pp.159~169 (2002)
  6. Pierce LH, "A status report of possible risks of base metal alloys and their components", J Prosthet Dent, 62, pp.234~238 (1989)
  7. Wassell RW, "Crowns and extra-coronal restorations: materials selection", Br Dent J, 192, pp.199~211 (2002)
  8. Vigolo P, "An in vitro evaluation of fit of zirconiumoxide-based ceramic four-unit fixed partial dentures, generated with three different CAD", CAM systems, before and after porcelain firing cycles and after glaze cycles, 2008, pp.17, 621~626
  9. 박현순, "Influence of porcelain veneering on the marginal fit of Digident and Lava CAD", CAM zirconia ceramic crowns, 2010, pp.2(2), 33~38[DOI]
  10. Foster LV, "Failed conventional bridge work from general dental practice: clinical aspects and treatment needs of 142 cases", Br Dent J, 168, pp.199~201 (1990)
  11. Beuer F, "Marginal and internal fits of fixed dental prostheses zirconia retainers", Dent Mater, 25, pp.94~102 (2009)
  12. Kohorst P, "Influence of the veneering process on the marginal fit of zirconia fixed dental prostheses", J Oral Rehabil, 37, pp.283~291 (2010)
  13. Laurent M, "Clinical evaluation of the marginal fit of cast crowns--validation of the silicone replica method", J Oral Rehabil, 35, pp.116~122 (2008)
  14. Groten M, "Determination of the minimum number of marginal gap measurements required for practical in-vitro testing", J Prosthet Dent, 83, pp.40~49 (2000)
  15. Hung SH, "Marginal fit of porcelain-fused-to-metal and two types of ceramic crown", J Prosthet Dent, 63, pp.26~31 (1990)
  16. Luthardt RG, "An innovative method for evaluation of the 3-D internal fit of CAD", CAM crowns fabricated after direct optical versus indirect laser scan digitizing, 2004, pp.17, 680~685
  17. Pelekanos S, "Micro-CT evaluation of the marginal fit of different In-Ceram alumina copings", Eur J Esthet Dent, 4, pp.278~292 (2009)
  18. Ucar Y, "Internal fit evaluation of crowns prepared using a new dental crown fabrication technique: laser-sintered Co-Cr crowns", J Prosthet Dent, 102, pp.253~259 (2009)
  19. ÖOrtorp A, "The fit of cobalt-chromium three-unit fixed dental prostheses fabricated with four different techniques: a comparative in vitro study", Dent Mater, 27, pp.356~363 (2011)
  20. Holmes JR, "Considerations in measurement of marginal fit", J Prosthet Dent, 62, pp.405~408 (1989)
  21. Bonate PL, "Analysis of pretest-posttest designs", pp.2000, Chapman and Hall
  22. White SN, "Microleakage of new crown and fixed partial denture luting agents", J Prosthet Dent, 67, pp.156~161 (1992)
  23. Moldovan O, "Threedimensional fit of CAD", CAM-made zirconia copings, 2011, pp.27, 1273~1278
  24. Laurent M, "Clinical evaluation of the marginal fit of cast crowns--validation of the silicone replica method", J Oral Rehabil, 35, pp.116~122 (2008)
  25. Rahme HY, "In vitro evaluation of the «replica technique» in the measurement of the fit of Procera crowns", J Contemp Dent Pract, 9, pp.25~32 (2008)
  26. Buchanan WT, "The effect of repeated firings and strength on marginal distortion in two ceramometal systems", J Prosthet Dent, 45, pp.502~506 (1981)
  27. Shokry TE, "Effect of metal selection and porcelain firing on the marginal accuracy of titanium-based metal ceramic restorations", J Prosthet Dent, 103, pp.45~52 (2010)
  28. Ostlund LE, "Cavity design and mathematics: their effect on gaps at the margins of cast restorations", Oper Dent, 10, pp.122~137 (1985)
  29. Sulaiman F, "A comparison of the marginal fit of In-Ceram, IPS Empress, and Procera crowns", Int J Prosthodont, 10, pp.478~484 (1997)
  30. McLean JW, "The estimation of cement film thickness by an in vivo technique", Br Dent J, 131, pp.107~111 (1971)

관련 논문AI추천

Accuracy evaluation of metal copings fabricated by computer-aided milling and direct metal laser sintering systems김웅철, 김지환, 김혜영, 박종경, 이완선대한치과보철학회 · The Journal of Advanced of Prosthodontics2015 · 제7권 제2호Evaluation of marginal and internal gaps of Ni-Cr and Co-Cr alloy copings manufactured by microstereolithography김동연, 김웅철, 김지환, 김총명, 김혜영대한치과보철학회 · The Journal of Advanced of Prosthodontics2017 · 제9권 제3호Fitting accuracy of ceramic veneered Co-Cr crowns produced by different manufacturing processesFlorian Bernhard, Nadine Freifrau von Maltzahn, Philipp Kohorst대한치과보철학회 · The Journal of Advanced of Prosthodontics2020 · 제12권 제2호Evaluation of the marginal and internal gaps of three different dental prostheses: comparison of the silicone replica technique and three-dimensional superimposition analysis김웅철, 김지환, 김혜영, 박진영, 배소연, 이재준대한치과보철학회 · The Journal of Advanced of Prosthodontics2017 · 제9권 제3호Comparative clinical study of the marginal discrepancy of fixed dental prosthesis fabricated by the millingsintering method using a presintered alloy권태엽, 김미주, 김재원, 이두형, 이청희, 최용도, Hang-Nga Mai대한치과보철학회 · The Journal of Advanced of Prosthodontics2019 · 제11권 제5호Effect of different tooth preparation designs on the marginal and internal fit discrepancies of cobalt-chromium crowns produced by computer-aided designing and selective laser melting processesChao-Yi Ma, Fa-Bing Tan, Hong-Wei Dai, Jin-Lin Song, Na Yu, Xue-Lu Tong대한치과보철학회 · The Journal of Advanced of Prosthodontics2021 · 제13권 제5호

이 간행물의 다른 논문 (19건)