초록

PURPOSE. To evaluate the effect of surface treatments and repair materials on the shear bond strength and to measure the fracture toughness of CAD/CAM provisional restoration materials. MATERIALS AND METHODS. Four CAD/CAM (3D printing: Nextdent C&B and ZMD-1000B Temporary, CAD/CAM resin block: Yamahachi PMMA disk and Huge PMMA block) and four conventional (monometacrylate: Jet and Alike, dimetacrylate: Luxatemp and Protemp 4) materials were selected to fabricate disk-shaped specimens and divided into six groups according to surface treatment (n=10). CAD/CAM materials were repaired with Jet or Luxatemp, while conventional materials were repaired with their own materials. The shear bond strength was measured by using universal testing machine. Ten rectangular column-shaped specimens for each material were fabricated to measure the fracture toughness by single edge v notched beam technique. Statistical analysis was performed by one-way ANOVA. RESULTS. The highest shear bond strength of CAD/CAM materials was achieved by SiC paper + sandblasting. It was also accomplished when repairing 3D printing materials with Luxatemp, and repairing CAD/CAM resin blocks with Jet. Yamahachi PMMA disk showed the highest fracture toughness. Nextdent C&B showed the lowest fracture toughness value but no statistically significant difference from Alike and Luxatemp (P>.05). CONCLUSION. In order to successfully repair the CAD/CAM provisional restoration, mechanical surface treatment and appropriate repair material according to the CAD/CAM material type should be selected. The CAD/CAM provisional materials have proper mechanical properties for clinical use as compared to conventional materials.

Abstract

PURPOSE. To evaluate the effect of surface treatments and repair materials on the shear bond strength and to measure the fracture toughness of CAD/CAM provisional restoration materials. MATERIALS AND METHODS. Four CAD/CAM (3D printing: Nextdent C&B and ZMD-1000B Temporary, CAD/CAM resin block: Yamahachi PMMA disk and Huge PMMA block) and four conventional (monometacrylate: Jet and Alike, dimetacrylate: Luxatemp and Protemp 4) materials were selected to fabricate disk-shaped specimens and divided into six groups according to surface treatment (n=10). CAD/CAM materials were repaired with Jet or Luxatemp, while conventional materials were repaired with their own materials. The shear bond strength was measured by using universal testing machine. Ten rectangular column-shaped specimens for each material were fabricated to measure the fracture toughness by single edge v notched beam technique. Statistical analysis was performed by one-way ANOVA. RESULTS. The highest shear bond strength of CAD/CAM materials was achieved by SiC paper + sandblasting. It was also accomplished when repairing 3D printing materials with Luxatemp, and repairing CAD/CAM resin blocks with Jet. Yamahachi PMMA disk showed the highest fracture toughness. Nextdent C&B showed the lowest fracture toughness value but no statistically significant difference from Alike and Luxatemp (P>.05). CONCLUSION. In order to successfully repair the CAD/CAM provisional restoration, mechanical surface treatment and appropriate repair material according to the CAD/CAM material type should be selected. The CAD/CAM provisional materials have proper mechanical properties for clinical use as compared to conventional materials.

참고문헌 (46)

  1. Orsi IA, "Evaluation of the flexural strength and elastic modulus of resins used for temporary restorations reinforced with particulate glass fibre", Gerodontology, 29, pp.e63~e68 (2012)
  2. Regish KM, "Techniques of fabrication of provisional restoration : an overview", Int J Dent, 2011, pp.134659~ (2011)
  3. Alharbi N, "Effects of build direction on the mechanical properties of 3D-printed complete coverage interim dental restorations", J Prosthet Dent, 115, pp.760~767 (2016)
  4. Davidowitz G, "The use of CAD", CAM in dentistry, 2011, pp.55, 559~570
  5. 이완선, "Evaluation of internal fit of interim crown fabricated with CAD", CAM milling and 3D printing system, 2017, pp.9(4), 265~270[DOI]
  6. Stansbury JW, "3D printing with polymers : Challenges among expanding options and opportunities", Dent Mater, 32, pp.54~64 (2016)
  7. Shamseddine L, "Marginal and internal fit of pressed ceramic crowns made from conventional and computer-aided design and computer-aided manufacturing wax patterns : An in vitro comparison", J Prosthet Dent, 116, pp.242~248 (2016)
  8. Park JM, "Clinical evaluations of cast gold alloy, machinable zirconia, and semiprecious alloy crowns : A multicenter study", J Prosthet Dent, 115, pp.684~691 (2016)
  9. Koch GK, "Accuracy in the digital workflow : From data acquisition to the digitally milled cast", J Prosthet Dent, 115, pp.749~754 (2016)
  10. Berman B, "3-D printing : The new industrial revolution", Business Horizons, 55, pp.155~162 (2012)
  11. Burns DR, "A review of selected dental literature on contemporary provisional fixed prosthodontic treatment : report of the Committee on Research in Fixed Prosthodontics of the Academy of Fixed Prosthodontics", J Prosthet Dent, 90, pp.474~497 (2003)
  12. Mai HN, "Fit of interim crowns fabricated using photopolymer-jetting 3D printing", J Prosthet Dent, 118, pp.208~215 (2017)
  13. Koumjian JH, "Evaluation of fracture resistance of resins used for provisional restorations", J Prosthet Dent, 64, pp.654~657 (1990)
  14. Gegauff AG, "Fracture toughness testing of visible light-and chemical-initiated provisional restoration resins", Int J Prosthodont, 8, pp.62~68 (1995)
  15. Moon JE, "Effects of airborne-particle abrasion protocol choice on the surface characteristics of monolithic zirconia materials and the shear bond strength of resin cement", Ceram Int, 42, pp.1552~1562 (2016)
  16. Ha SR, "Improving shear bond strength of temporary crown and fixed dental prosthesis resins by surface treatments", J Mater Sci, 51, pp.1463~1475 (2016)
  17. Chen HL, "Shear bond strength of provisional restoration materials repaired with light-cured resins", Oper Dent, 33, pp.508~515 (2008)
  18. 임용운, "치과 보철", 수복재료의 기계적 특성에 대한 규격화 시험법과 응용, 2015, pp.42(3), 259~270[DOI]
  19. Brosh T, "Effect of combinations of surface treatments and bonding agents on the bond strength of repaired composites", J Prosthet Dent, 77, pp.122~126 (1997)
  20. Ozcan M, "Evaluation of alternative intra-oral repair techniques for fractured ceramic-fused-to-metal restorations", J Oral Rehabil, 30, pp.194~203 (2003)
  21. Shahverdi S, "Effects of different surface treatment methods on the bond strength of composite resin to porcelain", J Oral Rehabil, 25, pp.699~705 (1998)
  22. Suliman AH, "Effects of surface treatment and bonding agents on bond strength of composite resin to porcelain", J Prosthet Dent, 70, pp.118~120 (1993)
  23. Cavalcanti AN, "Effect of surface treatments and bonding agents on the bond strength of repaired composites", J Esthet Restor Dent, 19, pp.90~98 (2007)
  24. Ayse Seda Ataol, "Repair bond strength of resin composite to bilayer dental ceramics", The Journal of Advanced of Prosthodontics, 10(2), pp.101~112 (2018), 대한치과보철학회[DOI]
  25. 이영곤, "상아질 표면 거칠기, 자가부식 접착제, 결합강도, 다이아몬드 포인트, 카바이드 버, SiC paper", Restorative Dentistry and Endodontics, 35(1), pp.13~19 (2010), 대한치과보존학회
  26. Gregory WA, "Bond strengths of chemically dissimilar repaired composite resins", J Prosthet Dent, 64, pp.664~668 (1990)
  27. da Costa TR, "Durability of composite repair using different surface treatments", J Dent, 40, pp.513~521 (2012)
  28. Özcan M, "Repair bond strength of microhybrid, nanohybrid and nanofilled resin composites : effect of substrate resin type, surface conditioning and ageing", Clin Oral Investig, 17, pp.1751~1758 (2013)
  29. Bacchi A, "Repair bond strength in aged methacrylate-and silorane-based composites", J Adhes Dent, 15, pp.447~452 (2013)
  30. Kimyai S, "Effect of different mechanical and chemical surface treatments on the repaired bond strength of an indirect composite resin", Lasers Med Sci, 30, pp.653~659 (2015)
  31. Ozcan M, "Effect of three surface conditioning methods to improve bond strength of particulate filler resin composites", J Mater Sci Mater Med, 16, pp.21~27 (2005)
  32. Swift EJ Jr, "Evaluation of new methods for composite repair", Dent Mater, 8, pp.362~365 (1992)
  33. Lucena-Martín C, "The effect of various surface treatments and bonding agents on the repaired strength of heat-treated composites", J Prosthet Dent, 86, pp.481~488 (2001)
  34. Oztas N, "The effect of air abrasion with two new bonding agents on composite repair", Oper Dent, 28, pp.149~154 (2003)
  35. Azarbal P, "The effect of bonding agents on the interfacial bond strength of repaired composites", Dent Mater, 2, pp.153~155 (1986)
  36. Saunders WP1, "Effect of fatigue upon the interfacial bond strength of repaired composite resins", J Dent, 18, pp.158~162 (1990)
  37. Crumpler DC, "Bonding to resurfaced posterior composites", Dent Mater, 5, pp.417~424 (1989)
  38. Eli I, "Bond strength of joined posterior light-cured composites : comparison of surface treatments", J Prosthet Dent, 60, pp.185~189 (1988)
  39. Hisamatsu N, "Effect of silane primers and unfilled resin bonding agents on repair bond strength of a prosthodontic microfilled composite", J Oral Rehabil, 29, pp.644~648 (2002)
  40. Ozcan M, "Effect of surface conditioning methods on the microtensile bond strength of resin composite to composite after aging conditions", Dent Mater, 23, pp.1276~1282 (2007)
  41. 이현영, "Bonding of the silane containing multi-mode universal adhesive for lithium disilicate ceramics", Restorative Dentistry and Endodontics, 42(2), pp.95~104 (2017), 대한치과보존학회
  42. El Zohairy AA, "The effect of adhesives with various degrees of hydrophilicity on resin ceramic bond durability", Dent Mater, 20, pp.778~787 (2004)
  43. Takahashi M1, "Long-term evaluation of water sorption and ultimate tensile strength of HEMA-containing", -free one-step self-etch adhesives, 2011, pp.39, 506~512
  44. Fahmy NZ, "Effect of two methods of reinforcement on the fracture strength of interim fixed partial dentures", J Prosthodont, 18, pp.512~520 (2009)
  45. Balkenhol M, "Fracture toughness of cross-linked and non-cross-linked temporary crown and fixed partial denture materials", Dent Mater, 25, pp.917~928 (2009)
  46. Tahayeri A, "3D printed versus conventionally cured provisional crown and bridge dental materials", Dent Mater, 34, pp.192~200 (2018)

관련 논문AI추천

Bonding of conventional provisional resin to 3D printed resin: the role of surface treatments and type of repair resins신수연, 임나경대한치과보철학회 · The Journal of Advanced of Prosthodontics2020 · 제12권 제5호Shear bond strengths of aged and non-aged CAD/CAM materials after different surface treatmentsFatma Ayse Sanal, Hamiyet Kilinc, Sedanur Turgut대한치과보철학회 · The Journal of Advanced of Prosthodontics2020 · 제12권 제5호Influence of different surface treatments on bond strength of novel CAD/CAM restorative materials to resin cementAyça Tulga, Elçin Sağırkaya, Meltem Bektaş Kömürcüoğlu대한치과보철학회 · The Journal of Advanced of Prosthodontics2017 · 제9권 제6호Effect of surface treatments and universal adhesive application on the microshear bond strength of CAD/CAM materialsAliye Tuğçe Gürcan, Burak Gümüştaş, Rana Turunç-Oğuzman, Soner Şişmanoğlu, Zuhal Yıldırım-Bilmez대한치과보철학회 · The Journal of Advanced of Prosthodontics2020 · 제12권 제1호Comparison of fracture strength after thermo-mechanical aging between provisional crowns made with CAD/CAM and conventional methodOnauma Angwaravong, Tanapon Reeponmaha, Thidarat Angwarawong대한치과보철학회 · The Journal of Advanced of Prosthodontics2020 · 제12권 제4호Effect of surface treatments on shear bond strength of resin composite bonded to CAD/CAM resin-ceramic hybrid materialsAylin Doğan, Bilge Turhan Bal, Merve Bankoğlu Güngör, Seçil Karakoca Nemli, Senem Ünver대한치과보철학회 · The Journal of Advanced of Prosthodontics2016 · 제8권 제4호

이 간행물의 다른 논문 (8건)