Influence of polishing systems on roughness and color change of two dental ceramics
2
조회
0
다운로드
0
인용
0
참고문헌
키워드
초록
PURPOSE. To evaluate the polishing effect on roughness and color change of pressed and layering ceramics after immersion in coffee solution. MATERIALS AND METHODS. 88 ceramic discs (1.0 mm × 10.0 mm) were manufactured - 44 nano-fluorapatite layering ceramics (IPS e.max Ceram. Group C) and 44 pressed lithium disilicate ceramic discs (IPS e. max Press - Group P). Each group was divided into 4 subgroups according to surface treatments: (G) Glaze, (S) Shofu polishing system (Shofu Inc.), (E) Edenta AG polishing System, (KG) 30-μm diamond granulation tip. Surface roughness (Ra) and color change (ΔE) measurings after the surface treatments were performed, before and 12 days after the immersion in coffee solution. A samples’ qualitative analysis was conducted with a scanning electron microscopy (SEM). Data were statistically-treated with oneway-ANOVA and Duncan’s tests, apart from paired t-test and Pearson’s correlation test (α=5%). RESULTS. The decrescent order, both for surface roughness (Ra) and ΔE for both ceramics were: KG > E > S > G (P<.05). With exception for PG and CG subgroups, which did not present statistical difference between them, all other pressed ceramics subgroups presented smaller Ra values and greater ΔE values than the layering ceramics subgroups (P<.05). CONCLUSION. Although mechanical polishing systems presented intermediate Ra values, their colors were considered clinically acceptable. There is a strong correlation between the surface roughness and the color change of tested ceramics.
Abstract
PURPOSE. To evaluate the polishing effect on roughness and color change of pressed and layering ceramics after immersion in coffee solution. MATERIALS AND METHODS. 88 ceramic discs (1.0 mm × 10.0 mm) were manufactured - 44 nano-fluorapatite layering ceramics (IPS e.max Ceram. Group C) and 44 pressed lithium disilicate ceramic discs (IPS e. max Press - Group P). Each group was divided into 4 subgroups according to surface treatments: (G) Glaze, (S) Shofu polishing system (Shofu Inc.), (E) Edenta AG polishing System, (KG) 30-μm diamond granulation tip. Surface roughness (Ra) and color change (ΔE) measurings after the surface treatments were performed, before and 12 days after the immersion in coffee solution. A samples’ qualitative analysis was conducted with a scanning electron microscopy (SEM). Data were statistically-treated with oneway-ANOVA and Duncan’s tests, apart from paired t-test and Pearson’s correlation test (α=5%). RESULTS. The decrescent order, both for surface roughness (Ra) and ΔE for both ceramics were: KG > E > S > G (P<.05). With exception for PG and CG subgroups, which did not present statistical difference between them, all other pressed ceramics subgroups presented smaller Ra values and greater ΔE values than the layering ceramics subgroups (P<.05). CONCLUSION. Although mechanical polishing systems presented intermediate Ra values, their colors were considered clinically acceptable. There is a strong correlation between the surface roughness and the color change of tested ceramics.
참고문헌 (47)
- Höland W, "Future perspectives of biomaterials for dental restoration", J European Ceram Soc, 29, pp.1291~1297 (2009)
- Bayne SC, "The evolution of dental materials over the past century : Silver and gold to tooth color and beyond", J Dent Res, 98, pp.257~265 (2019)
- de Kok P, "The effect of internal roughness and bonding on the fracture resistance and structural reliability of lithium disilicate ceramic", Dent Mater, 33, pp.1416~1425 (2017)
- Dalkiz M, "Effects of six surface treatment methods on the surface roughness of a low-fusing and an ultra low-fusing feldspathic ceramic material", J Prosthodont, 18, pp.217~222 (2009)
- Kelly JR, "Ceramic materials in dentistry : historical evolution and current practice", Aust Dent J, 56, pp.84~96 (2011)
- Anusavice KJ, "Phillips' science of dental materials", pp.2012, Elsevier
- Wright MD, "Comparison of three systems for the polishing of an ultra-low fusing dental porcelain", J Prosthet Dent, 92, pp.486~490 (2004)
- Chang CW, "Cracking of porcelain surfaces arising from abrasive grinding with a dental air turbine", J Prosthodont, 20, pp.613~620 (2011)
- al-Wahadni A, "Glazing and finishing dental porcelain : a literature review", J Can Dent Assoc, 64, pp.580~583 (1998)
- Rashid H, "The effect of surface roughness on ceramics used in dentistry : A review of literature", Eur J Dent, 8, pp.571~579 (2014)
- Yilmaz C, "Color stability of glazed and polished dental porcelains", J Prosthodont, 17, pp.20~24 (2008)
- Vichi A, "Effect of finishing and polishing on roughness and gloss of lithium disilicate and lithium silicate zirconia reinforced glass ceramic for CAD", CAM systems, 2018, pp.43, 90~100
- Yuzugullu B, "The effects of ex-traoral porcelain polishing sequences on surface roughness and color of feldspathic porcelain", Int J Prosthodont, 22, pp.472~475 (2009)
- Sarikaya I, "Effects of different polishing techniques on the surface roughness of dental porcelains", J Appl Oral Sci, 18, pp.10~16 (2010)
- Al-Shammery HA, "The use of confocal microscopy to assess surface roughness of two milled CAD-CAM ceramics following two polishing techniques", Dent Mater, 23, pp.736~741 (2007)
- Mohammadibassir M, "Effect of two polishing systems on surface roughness, topography, and flexural strength of a monolithic lithium disilicate ceramic", J Prosthodont, 28, pp.e172~e1180 (2019)
- Turgut S, "Colour stability of laminate veneers : an in vitro study", J Dent, 39, pp.e57~64 (2011)
- Lee YK, "Perceived color shift of a shade guide according to the change of illuminant", J Prosthet Dent, 105, pp.91~99 (2011)
- Kelly JR, "Ceramics in restorative and prosthetic dentistry", Annual Rev Mater Sci, 27, pp.443~468 (1997)
- Sarikaya I, "Effects of different surface treatments on the color stability of various dental porcelains", J Dent Sci, 6, pp.65~71 (2011)
- Motro PF, "Effects of different surface treatments on stainability of ceramics", J Prosthet Dent, 108, pp.231~237 (2012)
- Kursoglu P, "Correlation of surface texture with the stainability of ceramics", J Prosthet Dent, 112, pp.306~313 (2014)
- Sarıkaya I, "Effect of surface finishing on the colour stability and translucency of dental ceramics", BMC Oral Health, 18, pp.40~ (2018)
- Sarac D, "The effects of porcelain polishing systems on the color and surface texture of feldspathic porcelain", J Prosthet Dent, 96, pp.122~128 (2006)
- Camacho GB, "Surface roughness of a dental ceramic after polishing with different vehicles and diamond pastes", Braz Dent J, 17, pp.191~194 (2006)
- Saraç D, "Comparison of 3polishing techniques for 2 all-ceramic materials", Int J Prosthodont, 20, pp.465~468 (2007)
- Boaventura JM, "Effect finishing and polishing procedures on the surface roughness of IPS Empress 2 ceramic", Acta Odontol Scand, 71, pp.438~443 (2013)
- Carrabba M, "Effect of finishing and polishing on the surface roughness and gloss of feldspathic ceramic for chairside CAD", CAM systems, 2017, pp.42, 175~184
- Ertan AA, "Colour stability of low fusing porcelains : an in vitro study", J Oral Rehabil, 32, pp.358~361 (2005)
- Samra AP, "Color stability evaluation of aesthetic restorative materials", Braz Oral Res, 22, pp.205~210 (2008)
- Niu E, "Color match of machinable lithium disilicate ceramics : effects of foundation restoration", J Prosthet Dent, 110, pp.501~509 (2013)
- Akar GC, "Effects of surface-finishing protocols on the roughness, color change, and translucency of different ceramic systems", J Prosthet Dent, 112, pp.314~321 (2014)
- Niu E, "Color match of machinable lithium disilicate ceramics : Effects of cement color and thickness", J Prosthet Dent, 111, pp.42~50 (2014)
- Alp G, "Effect of surface treatments and coffee thermocycling on the color and translucency of CAD-CAM monolithic glass-ceramic", J Prosthet Dent, 120, pp.263~268 (2018)
- Atay A, "Effect of colored beverages on the color stability of feldspathic porcelain subjected to various surface treatments", Quintessence Int, 40, pp.e41~8 (2009)
- Omer Sagsoz, "The effects of different polishing techniques on the staining resistance of CAD", CAM resin-ceramics, 2016, pp.8(6), 417~422[DOI]
- Guler AU, "Effects of different drinks on stainability of resin composite provisional restorative materials", J Prosthet Dent, 94, pp.118~124 (2005)
- Raimondo RL Jr, "Polished versus autoglazed dental porcelain", J Prosthet Dent, 64, pp.553~557 (1990)
- Patterson CJ, "Efficacy of a porcelain refinishing system in restoring surface finish after grinding with fine and extra-fine diamond burs", J Prosthet Dent, 68, pp.402~406 (1992)
- Goldstein GR, "Profilometer, SEM, and visual assessment of porcelain polishing methods", J Prosthet Dent, 65, pp.627~634 (1991)
- Manjuran NG, "An in vitro study to identify a ceramic polishing protocol effecting smoothness superior to glazed surface", J Indian Prosthodont Soc, 14, pp.219~227 (2014)
- Steiner R, "Adjusting dental ceramics : An in vitro evaluation of the ability of various ceramic polishing kits to mimic glazed dental ceramic surface", J Prosthet Dent, 113, pp.616~622 (2015)
- Fuzzi M, "Scanning electron microscopy and profilometer evaluation of glazed and polished dental porcelain", Int J Prosthodont, 9, pp.452~458 (1996)
- Bottino MC, "Polishing methods of an alumina-reinforced feldspar ceramic", Braz Dent J, 17, pp.285~289 (2006)
- Seghi RR, "Visual and instrumental colorimetric assessments of small color differences on translucent dental porcelain", J Dent Res, 68, pp.1760~1764 (1989)
- Gupta R, "A spectrophotometric evaluation of color changes of various tooth colored veneering materials after exposure to commonly consumed beverages", J Indian Prosthodont Soc, 5, pp.72~78 (2005)
- Heffernan MJ, "Relative translucency of six all-ceramic systems. Part II: core and veneer materials", J Prosthet Dent, 88, pp.10~15 (2002)