PURPOSE. The purpose of this study was to evaluate and compare three polishing systems on the surface roughness and phase transformation of monolithic zirconia. MATERIALS AND METHODS. 100 disk shaped specimens (10 mm diameter, 3 mm thickness) were fabricated from monolithic zirconia blocks. 20 specimens were left as a control group and remaining specimens were grinded by diamond bur to simulate the occlusal adjustments. Grinded specimens were randomly divided into 4 groups: group G (no polishing), group M (Meisinger, zirconia polishing kit), group E (EVE Diacera, zirconia polishing kit), and group P (EVE Diapol, porcelain polishing kit). Surface roughness was measured with profilometer and surface topography was observed with SEM. XRD analysis was performed to investigate the phase transformation. Statistical analysis was performed with one-way ANOVA and Tukey’s post hoc tests at a significance level of P=.05. RESULTS. All polishing groups showed a smoother surface than group G. Among 3 polishing systems, group M and group E exhibited a smoother surface than the group P. However, no significant differences were observed between group M and group E (P˃.05). Grinding and polishing did not cause phase transformations in zirconia specimens. CONCLUSION. Zirconia polishing systems created a smoother surface on zirconia than the porcelain polishing system. Phase transformation did not occur during the polishing procedure.
Abstract
PURPOSE. The purpose of this study was to evaluate and compare three polishing systems on the surface roughness and phase transformation of monolithic zirconia. MATERIALS AND METHODS. 100 disk shaped specimens (10 mm diameter, 3 mm thickness) were fabricated from monolithic zirconia blocks. 20 specimens were left as a control group and remaining specimens were grinded by diamond bur to simulate the occlusal adjustments. Grinded specimens were randomly divided into 4 groups: group G (no polishing), group M (Meisinger, zirconia polishing kit), group E (EVE Diacera, zirconia polishing kit), and group P (EVE Diapol, porcelain polishing kit). Surface roughness was measured with profilometer and surface topography was observed with SEM. XRD analysis was performed to investigate the phase transformation. Statistical analysis was performed with one-way ANOVA and Tukey’s post hoc tests at a significance level of P=.05. RESULTS. All polishing groups showed a smoother surface than group G. Among 3 polishing systems, group M and group E exhibited a smoother surface than the group P. However, no significant differences were observed between group M and group E (P˃.05). Grinding and polishing did not cause phase transformations in zirconia specimens. CONCLUSION. Zirconia polishing systems created a smoother surface on zirconia than the porcelain polishing system. Phase transformation did not occur during the polishing procedure.
참고문헌 (32)
- Pereira GK, "Mechanical behavior of a Y-TZP ceramic for monolithic restorations: effect of grinding and low-temperature aging", Mater Sci Eng C Mater Biol Appl, 63, pp.70~77 (2016)[DOI]
- Piconi C, "Zirconia as a ceramic biomaterial", Biomaterials, 20, pp.1~25 (1999)[DOI]
- Zhang Y, "Making yttria-stabilized tetragonal zirconia translucent", Dent Mater, 30, pp.1195~1203 (2014)[DOI]
- Lazar DR, "Y-TZP ceramic processing from coprecipitated powders: a comparative study with three commercial dental ceramics", Dent Mater, 24, pp.1676~1685 (2008)[DOI]
- Rosentritt M, "Two-body wear of dental porcelain and substructure oxide ceramics", Clin Oral Investig, 16, pp.935~943 (2012)[DOI]
- Park C, "Effect of various polishing systems on the surface roughness and phase transformation of zirconia and the durability of the polishing systems", J Prosthet Dent, 117, pp.430~437 (2017)[DOI]
- Raigrodski AJ, "Clinical efficacy of veneered zirconium dioxide- based posterior partial fixed dental prostheses: five-year results", J Prosthet Dent, 108, pp.214~222 (2012)[DOI]
- Kokubo Y, "Five-year clinical evaluation of In-Ceram crowns fabricated using GN-I (CAD", CAM) system, 2011, pp.38, 601~607
- Ortorp A, "A 3-year retrospective and clinical follow-up study of zirconia single crowns performed in a private practice", J Dent, 37, pp.731~736 (2009)[DOI]
- Etman MK, "Three-year clinical evaluation of two ceramic crown systems: a preliminary study", J Prosthet Dent, 103, pp.80~90 (2010)[DOI]
- Guilardi LF, "Surface micro-morphology, phase transformation, and mechanical reliability of ground and aged monolithic zirconia ceramic", J Mech Behav Biomed Mater, 65, pp.849~856 (2017)[DOI]
- Etman MK, "Quantitative measurement of tooth and ceramic wear: in vivo study", Int J Prosthodont, 21, pp.245~252 (2008)
- Preis V, "Wear performance of dental ceramics after grinding and polishing treatments", J Mech Behav Biomed Mater, 10, pp.13~22 (2012)[DOI]
- Preis V, "Wear performance of substructure ceramics and veneering porcelains", Dent Mater, 27, pp.796~804 (2011)[DOI]
- Cotes C, "Effects of aging procedures on the topographic surface, structural stability, and mechanical strength of a ZrO2-based dental ceramic", Dent Mater, 30, pp.e396~e404 (2014)[DOI]
- Amaral M, "Lowtemperature degradation of a Y-TZP ceramic after surface treatments", J Biomed Mater Res B Appl Biomater, 101, pp.1387~1392 (2013)[DOI]
- Ozcan M, "Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading", J Mech Behav Biomed Mater, 20, pp.19~28 (2013)[DOI]
- Caglar I, "The effect of sandblasting, Er:YAG laser, and heat treatment on the mechanical properties of different zirconia cores", Photomed Laser Surg, 34, pp.17~26 (2016)[DOI]
- Glavina D, "Surface quality of Cerec CAD", CAM ceramic veneers treated with four different polishing systems, 2004, pp.5, 30~34
- Mohammadi-Bassir M, "Effect of coarse grinding, overglazing, and 2 polishing systems on the flexural strength, surface roughness, and phase transformation of yttrium-stabilized tetragonal zirconia", J Prosthet Dent, 118, pp.658~665 (2017)
- Karakoca S, "Influence of surface treatments on surface roughness, phase transformation, and biaxial flexural strength of Y-TZP ceramics", J Biomed Mater Res B Appl Biomater, 91, pp.930~937 (2009)
- Kosmac T, "The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic", Dent Mater, 15, pp.426~433 (1999)[DOI]
- Motro PF, "Effects of different surface treatments on stainability of ceramics", J Prosthet Dent, 108, pp.231~237 (2012)[DOI]
- Wright MD, "Comparison of three systems for the polishing of an ultra-low fusing dental porcelain", J Prosthet Dent, 92, pp.486~490 (2004)[DOI]
- Huh YH, "Evaluation of various polishing systems and the phase transformation of monolithic zirconia", J Prosthet Dent, 116, pp.440~449 (2016)[DOI]
- Sabrah AH, "Full-contour Y-TZP ceramic surface roughness effect on synthetic hydroxyapatite wear", Dent Mater, 29, pp.666~673 (2013)[DOI]
- Heintze SD, "Wear of ceramic and antagonist-a systematic evaluation of influencing factors in vitro", Dent Mater, 24, pp.433~449 (2008)[DOI]
- Camacho GB, "Surface roughness of a dental ceramic after polishing with different vehicles and diamond pastes", Braz Dent J, 17, pp.191~194 (2006)[DOI]
- Aravind P, "Comparative evaluation of the efficiency of four ceramic finishing systems", J Int Oral Health, 5, pp.59~64 (2013)
- Bollen CM, "Comparison of surface roughness of oral hard materials to the threshold surface roughness for bacterial plaque retention: a review of the literature", Dent Mater, 13, pp.258~269 (1997)[DOI]
- Kyung-Rok Lee, "Effect of different grinding burs on the physical properties of zirconia", The Journal of Advanced of Prosthodontics, 8(2), pp.137~143 (2016), 대한치과보철학회[DOI]
- Al-Haj Husain N, "Effect of polishing instruments and polishing regimens on surface topography and phase transformation of monolithic zirconia: An evaluation with XPS and XRD analysis", J Mech Behav Biomed Mater, 64, pp.104~112 (2016)[DOI]