Clinical performance and failures of zirconia-based fixed partial dentures: a review literature

2

조회

0

다운로드

15

인용

0

참고문헌

키워드

초록

PURPOSE. Zirconia has been used in clinical dentistry for approximately a decade, and there have been several reports regarding the clinical performance and survival rates of zirconia-based restorations. The aim of this article was to review the literatures published from 2000 to 2010 regarding the clinical performance and the causes of failure of zirconia fixed partial dentures (FPDs). MATERIALS AND METHODS. An electronic search of English peer-reviewed dental literatures was performed through PubMed to obtain all the clinical studies focused on the performance of the zirconia FPDs. The electronic search was supplemented by manual searching through the references of the selected articles for possible inclusion of some articles. Randomized controlled clinical trials, longitudinal prospective and retrospective cohort studies were the focuses of this review. Articles that did not focus on the restoration of teeth using zirconia-based restorations were excluded from this review. RESULTS. There have been three studies for the study of zirconia single crowns. The clinical outcome was satisfactory (acceptable) according to the CDA evaluation. There have been 14 studies for the study of zirconia FPDs. The survival rates of zirconia anterior and posterior FPDs ranged between 73.9% - 100% after 2 - 5 years. The causes of failure were veneer fracture, ceramic core fracture, abutment tooth fracture, secondary caries, and restoration dislodgment. CONCLUSION. The overall performance of zirconia FPDs was satisfactory according to either USPHS criteria or CDA evaluations. Fracture resistance of core and veneering ceramics, bonding between core and veneering materials, and marginal discrepancy of zirconia-based restorations were discussed as the causes of failure. Because of its repeated occurrence in many studies, future researches are essentially required to clarify this problem and to reduce the fracture incident.

Abstract

PURPOSE. Zirconia has been used in clinical dentistry for approximately a decade, and there have been several reports regarding the clinical performance and survival rates of zirconia-based restorations. The aim of this article was to review the literatures published from 2000 to 2010 regarding the clinical performance and the causes of failure of zirconia fixed partial dentures (FPDs). MATERIALS AND METHODS. An electronic search of English peer-reviewed dental literatures was performed through PubMed to obtain all the clinical studies focused on the performance of the zirconia FPDs. The electronic search was supplemented by manual searching through the references of the selected articles for possible inclusion of some articles. Randomized controlled clinical trials, longitudinal prospective and retrospective cohort studies were the focuses of this review. Articles that did not focus on the restoration of teeth using zirconia-based restorations were excluded from this review. RESULTS. There have been three studies for the study of zirconia single crowns. The clinical outcome was satisfactory (acceptable) according to the CDA evaluation. There have been 14 studies for the study of zirconia FPDs. The survival rates of zirconia anterior and posterior FPDs ranged between 73.9% - 100% after 2 - 5 years. The causes of failure were veneer fracture, ceramic core fracture, abutment tooth fracture, secondary caries, and restoration dislodgment. CONCLUSION. The overall performance of zirconia FPDs was satisfactory according to either USPHS criteria or CDA evaluations. Fracture resistance of core and veneering ceramics, bonding between core and veneering materials, and marginal discrepancy of zirconia-based restorations were discussed as the causes of failure. Because of its repeated occurrence in many studies, future researches are essentially required to clarify this problem and to reduce the fracture incident.

참고문헌 (50)

  1. Haselton DR, "Clinical assessment of high-strength all-ceramic crowns", J Prosthet Dent, 83, pp.396~401 (2000)
  2. Olsson KG, "A long-term retrospective and clinical follow-up study of In-ceram alumina FPDs", Int J Prosthodont, 16, pp.150~156 (2003)
  3. Denry I, "State of the art of zirconia for dental applications", Dent Mater, 24, pp.299~307 (2008)
  4. Guazzato M, "Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics", Dent Mater, 20, pp.449~456 (2004)
  5. O¨rtorp A, "A 3-year retrospective and clinical follow-up study of zirconia single crowns performed in a private practice", J Dent, 37, pp.731~736 (2009)
  6. Çehreli MC, "CAD", CAM Zirconia vs. slip-cast glass-infiltrated Alumina, J Appl Oral Sci, pp.2009, 17[DOI]
  7. Beuer F, "Prospective study of zirconia-based restorations: 3-year clinical results", Quintessence Int, 41, pp.631~637 (2010)
  8. Sua′rez MJ, "Three-year clinical evaluation of In-Ceram Zirconia posterior FPDs", Int J Prosthodont, 17, pp.35~38 (2004)
  9. Vult von Steyern P, "All-ceramic fixed partial dentures designed according to the DC-Zirkon technique. A 2-year clinical study", J Oral Rehabil, 32, pp.180~187 (2005)
  10. Raigrodski AJ, "The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: a prospective clinical pilot study", J Prosthet Dent, 96, pp.237~244 (2006)
  11. Sailer I, "Prospective clinical study of zirconia posterior fixed partial dentures: 3-year follow-up", Quintessence Int, 37, pp.685~693 (2006)
  12. Sailer I, "Five-year clinical results of zirconia frameworks for posterior fixed partial dentures", Int J Prosthodont, 20, pp.383~388 (2007)
  13. Edelhoff D, "HIP zirconia fixed partial dentures-clinical results after 3 years of clinical service", Quintessence Int, 39, pp.459~471 (2008)
  14. Molin MK, "Five-year clinical prospective evaluation of zirconia-based Denzir 3-unit FPDs", Int J Prosthodont, 21, pp.223~227 (2008)
  15. Tinschert J, "Clinical behavior of zirconia-based fixed partial dentures made of DC-Zirkon: 3-year results", Int J Prosthodont, 21, pp.217~222 (2008)
  16. Beuer F, "Three-year clinical prospective evaluation of zirconia-based posterior fixed dental prostheses (FDPs)", Clin Oral Investig, 13, pp.445~451 (2009)
  17. Sailer I, "Randomized controlled clinical trial of zirconia-ceramic and metal-ceramic posterior fixed dental prostheses: a 3-year follow-up", Int J Prosthodont, 22, pp.553~560 (2009)
  18. Schmitt J, "Zirconia posterior fixed partial dentures: a prospective clinical 3-year follow-up", Int J Prosthodont, 22, pp.597~603 (2009)
  19. Schmitter M, "Clinical performance of extended zirconia frameworks for fixed dental prostheses: two-year results", J Oral Rehabil, 36, pp.610~615 (2009)
  20. Roediger M, "Prospective evaluation of zirconia posterior fixed partial dentures: four-year clinical results", Int J Prosthodont, 23, pp.141~148 (2010)
  21. Tsumita M, "Clinical evaluation of posterior all-ceramic FPDs (Cercon): a prospective clinical pilot study", J Prosthodont Res, 54, pp.102~105 (2010)
  22. Hertzberg RW, "Deformation and fracture mechanics of engineering materials. 4th ed", pp.326~327 (1995), John Wiley & Sons Inc
  23. Tinschert J, "Lifetime of alumina- and zirconia ceramics used for crown and bridge restorations", J Biomed Mater Res B Appl Biomater, 80, pp.317~321 (2007)
  24. Wang H, "Fracture toughness comparison of three test methods with four dental porcelains", Dent Mater, 23, pp.905~910 (2007)
  25. Suputtamongkol K, "Composition and properties of three dental porcelains", Mahidol Dent J, 28, pp.1~8 (2008)
  26. Cesar PF, "Correlation between fracture toughness and leucite content in dental porcelains", J Dent, 33, pp.721~729 (2005)
  27. Ong JL, "Quantification of leucite concentration using X-ray diffraction", Dent Mater, 16, pp.20~25 (2000)
  28. Taskonak B, "The effects of viscoelastic parameters on residual stress development in a zirconia", glass bilayer dental ceramic, 2008, pp.24, 1149~1155
  29. DeHoff PH, "Viscoelastic finite element stress analysis of the thermal compatibility of dental bilayer ceramic systems", Int J Prosthodont, 22, pp.56~61 (2009)
  30. Fischer J, "Effect of thermal misfit between different veneering ceramics and zirconia frameworks on in vitro fracture load of single crowns", Dent Mater J, 26, pp.766~772 (2007)
  31. Aboushelib MN, "Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: Zirconia veneering ceramics", Dent Mater, 22, pp.857~863 (2006)
  32. Aboushelib MN, "Effect of zirconia type on its bond strength with different veneer ceramics", J Prosthodont, 17, pp.401~408 (2008)
  33. Aboushelib MN, "Microtensile bond strength of different components of core veneered all-ceramic restorations", Dent Mater, 21, pp.984~991 (2005)
  34. Go¨stemeyer G, "Influence of cooling rate on zirconia", veneer interfacial adhesion, 2010, pp.6, 4532~4538
  35. Felton DA, "Effect of in vivo crown margin discrepancies on periodontal health", J Prosthet Dent, 65, pp.357~364 (1991)
  36. Tinschert J, "Marginal fit of alumina-and zirconia-based fixed partial dentures produced by a CAD", CAM system, 2001, pp.26, 367~374
  37. Bindl A, "Marginal and internal fit of all-ceramic CAD", CAM crown-copings on chamfer preparations, 2005, pp.32, 441~447
  38. Komine F, "Influence of framework configuration on the marginal adaptation of zirconium dioxide ceramic anterior four-unit frameworks", Acta Odontol Scand, 63, pp.361~366 (2005)
  39. Reich S, "Clinical fit of all-ceramic three-unit fixed partial dentures, generated with three different CAD", CAM systems, 2005, pp.113, 174~179
  40. Bindl A, "Fit of all-ceramic posterior fixed partial denture frameworks in vitro", Int J Periodontics Restorative Dent, 27, pp.567~575 (2007)
  41. Gonzalo E, "Marginal fit of zirconia posterior fixed partial dentures", Int J Prosthodont, 21, pp.398~399 (2008)
  42. Reich S, "Clinical fit of fourunit zirconia posterior fixed dental prostheses", Eur J Oral Sci, 116, pp.579~578 (2008)
  43. Vigolo P, "An in vitro evaluation of fit of zirconium-oxide- based ceramic four-unit fixed partial dentures, generated with three different CAD", CAM systems, before and after porcelain firing cycles and after glaze cycles, 2008, pp.17, 621~626
  44. Att W, "Marginal adaptation of three different zirconium dioxide three-unit fixed dental prostheses", J Prosthet Dent, 101, pp.239~247 (2009)
  45. Beuer F, "Marginal and internal fits of fixed dental prostheses zirconia retainers", Dent Mater, 25, pp.94~102 (2009)
  46. Beuer F, "Precision of fit: zirconia three-unit fixed dental prostheses", Clin Oral Investig, 13, pp.343~349 (2009)
  47. Dittmer MP, "Stresses and distortions within zirconia-fixed dental prostheses due to the veneering process", Acta Biomater, 5, pp.3231~3239 (2009)
  48. Gonzalo E, "A comparison of the marginal vertical discrepancies of zirconium and metal ceramic posterior fixed dental prostheses before and after cementation", J Prosthet Dent, 102, pp.378~384 (2009)
  49. Kohorst P, "Marginal accuracy of four-unit zirconia fixed dental prostheses fabricated using different computer-aided design", computer-aided manufacturing systems, 2009, pp.117, 319~325
  50. Kohorst P, "Influence of the veneering process on the marginal fit of zirconia fixed dental prostheses", J Oral Rehabil, 37, pp.283~291 (2010)

관련 논문AI추천

Survival rate of modern all-ceramic FPDs during an observation period from 2011 to 2016Meike Stiesch, Michael Eisenburger, Philipp-Cornelius Pott대한치과보철학회 · The Journal of Advanced of Prosthodontics2018 · 제10권 제1호In vitro evaluation of fracture strength of zirconia restoration veneered with various ceramic materials김성훈, 여인성, 이재봉, 최유성, 한중석대한치과보철학회 · The Journal of Advanced of Prosthodontics2012 · 제4권 제3호Success rate of all-ceramic FPDs depending on the time of restoration between 2011 and 2023Meike Stiesch, Michael Eisenburger, Philipp-Cornelius Pott대한치과보철학회 · The Journal of Advanced of Prosthodontics2024 · 제16권 제5호In-vitro performance and fracture strength of thin monolithic zirconia crownsAnna Sander, Hans-Christoph Lauer, Martin Rosentritt, Paul Weigl, Roland Felber, Yanyun Wu대한치과보철학회 · The Journal of Advanced of Prosthodontics2018 · 제10권 제2호The effect of zirconia framework design on the failure of all-ceramic crown under static loadingPakamard Taenguthai, Somchai Urapepon대한치과보철학회 · The Journal of Advanced of Prosthodontics2015 · 제7권 제2호In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses김소연, 배은빈, 배지현, 최재원, 허중보대한치과보철학회 · The Journal of Advanced of Prosthodontics2017 · 제9권 제4호

이 간행물의 다른 논문 (9건)