Objective: The purpose of this study was to determine the feasibility of an artificial esophagus using a silk fibroin (SF) scaffold. Method: The artificial esophagus was a three-layered, hybrid-type prosthesis composed of an outer and inner layer of poly(ε-caprolactone) (PCL) with a middle layer of SF. After depositing the inner layer of the PCL scaffold by electrospinning, the lyophilized middle SF layer was created. The outer layer of PCL was produced following the same procedure used to make the inner PCL layer. Result: In the cross-sectional image of the PCL-SF scaffold, we can clearly observe the nanofiber structure and the porous structure of the middle silk layer. The average stress values for the PCL-silk scaffold were 2.3460.12 MPa (dry) and 2.2660.23 MPa (wet). The CCK-8 assay results showed that prepared scaffolds modified with SF are generously nontoxic to the cells and that the presence of silk favored the growth of fibroblasts; therefore, this material is compatible with biomedical applications. Conclusion: Our study proposes a more practical experimental model for studying a three-layered PCL-SF scaffold in the esophagus.
Abstract
Objective: The purpose of this study was to determine the feasibility of an artificial esophagus using a silk fibroin (SF) scaffold. Method: The artificial esophagus was a three-layered, hybrid-type prosthesis composed of an outer and inner layer of poly(ε-caprolactone) (PCL) with a middle layer of SF. After depositing the inner layer of the PCL scaffold by electrospinning, the lyophilized middle SF layer was created. The outer layer of PCL was produced following the same procedure used to make the inner PCL layer. Result: In the cross-sectional image of the PCL-SF scaffold, we can clearly observe the nanofiber structure and the porous structure of the middle silk layer. The average stress values for the PCL-silk scaffold were 2.3460.12 MPa (dry) and 2.2660.23 MPa (wet). The CCK-8 assay results showed that prepared scaffolds modified with SF are generously nontoxic to the cells and that the presence of silk favored the growth of fibroblasts; therefore, this material is compatible with biomedical applications. Conclusion: Our study proposes a more practical experimental model for studying a three-layered PCL-SF scaffold in the esophagus.
참고문헌 (8)
- Zhang R, "Poly(alpha-hydroxyl acids)", hydroxyapatite porous composites for bone-tissue engineering. I. Preparation and morphology, 1999, pp.44, 446~455
- Lv Q, "The preparation of insoluble fibroin films induced by degummed fibroin or fibroin microspheres", J Mater Sci Mater Med, 15, pp.1193~1197 (2004)
- Kuppan P, "Tissue engineering interventions for esophageal disorders—Promises and challenges", Biotechnol Adv, 30, pp.1481~1492 (2012)
- Yamamoto Y1, "Intrathoracic esophageal replacement in the dog with the use of an artificial esophagus composed of a collagen sponge with a double-layered silicone tube", J Thorac Cardiovasc Surg, 118, pp.276~286 (1999)
- Takimoto Y, "qThe experimental replacement of a cervical esophageal segment with an artificial prosthesis with the use of collagen matrix and a silicone stent", J Thorac Cardiovasc Surg, 116, pp.98~106 (1998)
- Shao ZZ, "Materials: Surprising strength of silkworm silk", Nature, 418, pp.741~ (2002)
- Wang YZ, "Cartilage tissue engineering with silk scaffolds and human articular chondrocytes", Biomaterials, 27, pp.4434~4442 (2006)
- Kim J, "Comparison of methods for the repair of acute tympanic mem membrane perforations: Silk patch vs. paper patch", Wound Rep Reg, 18, pp.132~138 (2010)