해수배관 내부 에폭시 코팅재의 캐비테이션 및 침지 열화에 따른 압입인장특성
Indentation Tensile Properties of Seawater Piping with Cavitation and Immersion Degradation
0
조회
0
다운로드
0
인용
0
참고문헌
키워드
초록
Seawater has been used to cool devices in nuclear power plants. However, the pipes used to transport seawater are vulnerable to corrosion; hence, the inner side of pipelines is coated with an epoxy layer as prevention. Upon coating damage, the pipe becomes exposed, and corrosion progresses. The major cause is widely known as cavitation corrosion, causing the degradation of mechanical properties. In this study, corroded specimens were prepared using cavitation and immersion methods to clarify the degradation trend of mechanical properties with corrosion. Three different types of epoxy coatings were used, and accelerated cavitation procedures were composed of amplitudes of 15 µm, 50 µm, and 85 µm for 2 h, 4 h, and 6 h. The immersion periods were 3 and 6 weeks. We conducted instrumented indentation tests on all degradation samples to measure mechanical properties. The results showed that higher cavitation amplitudes and longer cavitation or immersion times led to more degradation in the samples, which, in turn, decreased the yield strength. Of the three samples, the C coating had the highest resistance to cavitation and immersion degradation.
Abstract
Seawater has been used to cool devices in nuclear power plants. However, the pipes used to transport seawater are vulnerable to corrosion; hence, the inner side of pipelines is coated with an epoxy layer as prevention. Upon coating damage, the pipe becomes exposed, and corrosion progresses. The major cause is widely known as cavitation corrosion, causing the degradation of mechanical properties. In this study, corroded specimens were prepared using cavitation and immersion methods to clarify the degradation trend of mechanical properties with corrosion. Three different types of epoxy coatings were used, and accelerated cavitation procedures were composed of amplitudes of 15 µm, 50 µm, and 85 µm for 2 h, 4 h, and 6 h. The immersion periods were 3 and 6 weeks. We conducted instrumented indentation tests on all degradation samples to measure mechanical properties. The results showed that higher cavitation amplitudes and longer cavitation or immersion times led to more degradation in the samples, which, in turn, decreased the yield strength. Of the three samples, the C coating had the highest resistance to cavitation and immersion degradation.
참고문헌 (22)
- 이승준, "해양 금속재료의 부식속도와 방식전류에 미치는 유속의 영향", CORROSION SCIENCE AND TECHNOLOGY, 14(5), pp.226~231 (2015), 한국부식방식학회[DOI]
- 부명환, "해수분위기에서 스테인리스강 배관 소켓 용접부의 선택적 부식", CORROSION SCIENCE AND TECHNOLOGY, 19(4), pp.224~230 (2020), 한국부식방식학회[DOI]
- J. M. Han, "A Study on Corrosion Behavior of Coated Steel Pipes for Seawater Service", Corrosion Science and Technology, 26, pp.41~ (1997)
- 이형준, "지역난방수 공급관 에어벤트 부식 파손 분석", CORROSION SCIENCE AND TECHNOLOGY, 19(4), pp.189~195 (2020), 한국부식방식학회[DOI]
- Christian Vargel, "Introducton to The Corrosion of Aluminium", Corrosion of Aluminium, pp.81~109 (2004), Elsevier[DOI]
- 이성열, "선박 해수배관에서 용접봉의 종류에 따라 직류 아크 용접한 용접부위의 부식특성에 관한 전기화학적 평가", 한국해양공학회지, 27(3), pp.79~84 (2013), 한국해양공학회
- Roland T Loto, "Corrosion resistance study of UNS A93105 aluminum alloy in neutral chloride and acid chloride solution", IOP Conference Series: Materials Science and Engineering, 872(1), pp.012052~ (2020), IOP Publishing
- 김성종, "선박의 해양 부식과 부식방지 장치", 한국표면공학회지, 44(3), pp.105~116 (2011), 한국표면공학회
- Hongbo Gu, "An overview of multifunctional epoxy nanocomposites", Journal of Materials Chemistry C, 4(25), pp.5890~5906 (2016), Royal Society of Chemistry (RSC)[DOI]
- Jaworski C. Capricho, "Multifunctionality in Epoxy Resins", Polymer Reviews, 60(1), pp.1~41 (2019), Informa UK Limited[DOI]
- 윤준용, "공동 현상 방지를 위한 버터플라이 밸브의 유동장 해석", 한국유체기계학회 논문집, 7(1), pp.9~16 (2004), 한국유체기계학회
- 손손, "수력학적 공동현상을 이용한 온수 발생 장치에서의 회전체 형상에 대한 수치해석적 연구", 한국유체기계학회 논문집, 20(2), pp.75~81 (2017), 한국유체기계학회[DOI]
- S. H. Kim, "Standardization of Residual Stress Evaluation Technique for Weldment of Metallic Materials Using Continuous Indentation Test", The Korean Institute of GAS, 2, pp.497~ (2017)
- U. J. Lim, "A Study on the Corrosion Control of Glass Flake Lining for Mild Steel in Marine Environment", Journal of Fisheries and Marine Sciences Education, 12, pp.164~ (2000)
- "ASTM G32-16, Standard Test Method for Cavitation Erosion Using Vibratory Apparatus", ASTM International, ~ (2016)
- J. H. Hahn, "Nanoindentation experiments on some thin films on silicon", Journal of the Korean Ceramics Society, 37, pp.596~ (2000)
- Y. C. Kim, "Calibration of Contact Depth for Evaluating Residual Stress using Instrumented Indentation Testing", Korean Society of Pressure Vessels and Piping, 7, pp.41~ (2011)
- 송원석, "원전 구조물의 가동 중 건전성 평가를 위한 연속압입시험법의 활용에 관한 연구", 비파괴검사학회지, 33(2), pp.165~172 (2013), 한국비파괴검사학회[DOI]
- "ISO", TR29381: Metallic materials – Measurement of mechanical properties by an instrumented indentation test – indentation tensile properties, 2008
- Ju-Young Kim, "Determination of tensile properties by instrumented indentation technique: Representative stress and strain approach", Surface and Coatings Technology, 201(7), pp.4278~4283 (2006), Elsevier BV[DOI]
- Seung-Kyun Kang, "Extended expanding cavity model for measurement of flow properties using instrumented spherical indentation", International Journal of Plasticity, 49, pp.1~15 (2013), Elsevier BV[DOI]
- 전종모, "Effect of Solution Temperature on the Cavitation Degradation Properties of Epoxy Coatings for Seawater Piping", CORROSION SCIENCE AND TECHNOLOGY, 20(6), pp.335~346 (2021), 한국부식방식학회[DOI]