PURPOSE. The aim of this study was to evaluate the effect of occlusal adjustments on the surface roughness of Yttria-tetragonal zirconia polycrystal (Y-TZP) and wear of opposing artificial enamel. MATERIALS AND METHODS. Twenty-five Y-TZP slabs from each brand (Lava, 3M and Bruxzir, Glidewell Laboratories) with different surface conditions (Control polished - CPZ; Polished/ground - GRZ; Polished/ground/repolished – RPZ; Glazed - GZ; Porcelain-veneered - PVZ; n=5) were abraded (500,000 cycles, 80 N) against artificial enamel (6 mm diameter steatite). Y-TZP roughness (in μm) before and after chewing simulation (CS) and antagonist steatite volume loss (in mm3) were evaluated using a contact surface profilometer. Y-TZP roughness was analyzed by three-way analysis of variance (ANOVA) and steatite wear by two-way ANOVA and Tukey Honest Difference (HSD) (P=.05). RESULTS. There was no effect of Y-TZP brand on surface roughness (P=.216) and steatite loss (P=.064). A significant interaction effect (P<.001) between surface condition and CS on Y-TZP roughness was observed. GZ specimens showed higher roughness after CS (before CS - 3.7 ± 1.8 um; after CS - 13.54 ± 3.11 um), with partial removal of the glaze layer. Indenters abraded against CPZ (0.09 ± 0.03 mm3) were worn more than those abraded against PVZ (0.02 ± 0.01 mm3) and GZ (0.02 ± 0.01 mm3). Higher wear caused by direct abrasion against zirconia was confirmed by SEM. CONCLUSION. Polishing with an intra-oral polishing system did not reduce the roughness of zirconia. Wear of the opposing artificial enamel was affected by the material on the surface rather than the finishing technique applied, indicating that polished zirconia is more deleterious to artificial enamel than are glazed and porcelain-veneered restorations.
Abstract
PURPOSE. The aim of this study was to evaluate the effect of occlusal adjustments on the surface roughness of Yttria-tetragonal zirconia polycrystal (Y-TZP) and wear of opposing artificial enamel. MATERIALS AND METHODS. Twenty-five Y-TZP slabs from each brand (Lava, 3M and Bruxzir, Glidewell Laboratories) with different surface conditions (Control polished - CPZ; Polished/ground - GRZ; Polished/ground/repolished – RPZ; Glazed - GZ; Porcelain-veneered - PVZ; n=5) were abraded (500,000 cycles, 80 N) against artificial enamel (6 mm diameter steatite). Y-TZP roughness (in μm) before and after chewing simulation (CS) and antagonist steatite volume loss (in mm3) were evaluated using a contact surface profilometer. Y-TZP roughness was analyzed by three-way analysis of variance (ANOVA) and steatite wear by two-way ANOVA and Tukey Honest Difference (HSD) (P=.05). RESULTS. There was no effect of Y-TZP brand on surface roughness (P=.216) and steatite loss (P=.064). A significant interaction effect (P<.001) between surface condition and CS on Y-TZP roughness was observed. GZ specimens showed higher roughness after CS (before CS - 3.7 ± 1.8 um; after CS - 13.54 ± 3.11 um), with partial removal of the glaze layer. Indenters abraded against CPZ (0.09 ± 0.03 mm3) were worn more than those abraded against PVZ (0.02 ± 0.01 mm3) and GZ (0.02 ± 0.01 mm3). Higher wear caused by direct abrasion against zirconia was confirmed by SEM. CONCLUSION. Polishing with an intra-oral polishing system did not reduce the roughness of zirconia. Wear of the opposing artificial enamel was affected by the material on the surface rather than the finishing technique applied, indicating that polished zirconia is more deleterious to artificial enamel than are glazed and porcelain-veneered restorations.
참고문헌 (43)
- Ilkin Tuncel, "The effect of coloring liquids on the translucency of zirconia framework", The Journal of Advanced of Prosthodontics, 5(4), pp.448~451 (2013), 대한치과보철학회[DOI]
- Beuer F, "In vitro performance of full-contour zirconia single crowns", Dent Mater, 28, pp.449~456 (2012)
- Alghazzawi TF, "Correlation of flexural strength of coupons versus strength of crowns fabricated with different zirconia materials with and without aging", J Am Dent Assoc, 146, pp.904~912 (2015)
- Guess PC, "Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling", Dent Mater, 24, pp.1556~1567 (2008)
- Long HA, "Monolithic zirconia crowns and bridges", Inside Dent, 8, pp.60~66 (2012)
- Stawarczyk B, "Comparison of four monolithic zirconia materials with conventional ones: Contrast ratio, grain size, four-point flexural strength and two-body wear", J Mech Behav Biomed Mater, 59, pp.128~138 (2016)
- Tong H, "Characterization of three commercial Y-TZP ceramics produced for their high-translucency, high-strength and high-surface area", Ceram Int, 42, pp.1077~1085 (2016)
- Johansson C, "Fracture strength of monolithic all-ceramic crowns made of high translucent yttrium oxide-stabilized zirconium dioxide compared to porcelain-veneered crowns and lithium disilicate crowns", Acta Odontol Scand, 72, pp.145~153 (2014)
- Kontos L, "Influence of surface treatment on the wear of solid zirconia", Acta Odontol Scand, 71, pp.482~487 (2013)
- Tholt de Vasconcellos B, "Surface roughness in ceramics with different finishing techniques using atomic force microscope and profilometer", Oper Dent, 31, pp.442~449 (2006)
- Raigrodski AJ, "Concepts of design for contemporary anterior all-ceramic restorations", J Cosme Dent, 28, pp.46~58 (2013)
- Sorrentino R, "Fiveyear prospective clinical study of posterior three-unit zirconia-based fixed dental prostheses", Clin Oral Investig, 16, pp.977~985 (2012)
- Candido L, "Surface roughness and hardness of yttria stabilized zirconia(Y-TZP)after 10years of simulated brushing", Rev Odontol UNESP, 43, pp.379~383 (2014)
- Kwon MS, "Two-body wear comparison of zirconia crown, gold crown, and enamel against zirconia", J Mech Behav Biomed Mater, 47, pp.21~28 (2015)
- Albashaireh ZS, "Two-body wear of different ceramic materials opposed to zirconia ceramic", J Prosthet Dent, 104, pp.105~113 (2010)
- Stawarczyk B, "Two-body wear of monolithic, veneered and glazed zirconia and their corresponding enamel antagonists", Acta Odontol Scand, 71, pp.102~112 (2013)
- Ghazal M, "The influence of antagonistic surface roughness on the wear of human enamel and nanofilled composite resin artificial teeth", J Prosthet Dent, 101, pp.342~349 (2009)
- Stober T, "Enamel wear caused by monolithic zirconia crowns after 6 months of clinical use", J Oral Rehabil, 41, pp.314~322 (2014)
- Preis V, "Wear performance of monolithic dental ceramics with different surface treatments", Quintessence Int, 44, pp.393~405 (2013)
- Preis V, "Wear performance of dental ceramics after grinding and polishing treatments", J Mech Behav Biomed Mater, 10, pp.13~22 (2012)
- Rashid H, "The effect of surface roughness on ceramics used in dentistry : A review of literature", Eur J Dent, 8, pp.571~579 (2014)
- Etman MK, "Confocal examination of subsurface cracking in ceramic materials", J Prosthodont, 18, pp.550~559 (2009)
- Lawson NC, "Wear of enamel opposing zirconia and lithium disilicate after adjustment, polishing and glazing", J Dent, 42, pp.1586~1591 (2014)
- 정유석, "A study on the in-vitro wear of the natural tooth structure by opposing zirconia or dental porcelain", The Journal of Advanced of Prosthodontics, 2(3), pp.111~115 (2010), 대한치과보철학회[DOI]
- Luangruangrong P, "Influence of full-contour zirconia surface roughness on wear of glass-ceramics", J Prosthodont, 23, pp.198~205 (2014)
- Janyavula S, "The wear of polished and glazed zirconia against enamel", J Prosthet Dent, 109, pp.22~29 (2013)
- Steiner M, "In vitro evaluation of a mechanical testing chewing simulator", Dent Mater, 25, pp.494~499 (2009)
- Kim MJ, "Wear evaluation of the human enamel opposing different Y-TZP dental ceramics and other porcelains", J Dent, 40, pp.979~988 (2012)
- Kelly JR, "Clinically relevant approach to failure testing of allceramic restorations", J Prosthet Dent, 81, pp.652~661 (1999)
- DeLong R, "The wear of dental porcelain in an artificial mouth", Dent Mater, 2, pp.214~219 (1986)
- Magne P, "Wear of enamel and veneering ceramics after laboratory and chairside finishing procedures", J Prosthet Dent, 82, pp.669~679 (1999)
- Shortall AC, "Potential countersample materials for in vitro simulation wear testing", Dent Mater, 18, pp.246~254 (2002)
- Hmaidouch R, "Surface roughness of zirconia for full-contour crowns after clinically simulated grinding and polishing", Int J Oral Sci, 6, pp.241~246 (2014)
- Ablal MA, "The erosive potential of some alcopops using bovine enamel : an in vitro study", J Dent, 37, pp.835~839 (2009)
- Lameira DP, "Fracture strength of aged monolithic and bilayer zirconia-based crowns", Biomed Res Int, 2015, pp.418641~ (2015)
- Ludovichetti FS, "Wear resistance and abrasiveness of CAD-CAM monolithic materials", J Prosthet Dent, 120, pp.318.e1~318.e8 (2018)
- Pereira GKR, "Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations", J Mech Behav Biomed Mater, 85, pp.57~65 (2018)
- Barghi N, "When to glaze-An electron microscope study", J Prosthet Dent, 35, pp.648~653 (1976)
- Roselino Lde M, "Effect of brushing and accelerated ageing on color stability and surface roughness of composites", J Dent, 41, pp.e54~e61 (2013)
- Tortopidis D, "The variability of bite force measurement between sessions, in different positions within the dental arch", J Oral Rehabil, 25, pp.681~686 (1998)
- Aydın B, "Effect of storage solutions on microhardness of crown enamel and dentin", Eur J Dent, 9, pp.262~266 (2015)
- Camposilvan E, "Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications", Dent Mater, 34, pp.879~890 (2018)
- Pinto PA, "Surface and mechanical characterization of dental yttria-stabilized tetragonal zirconia polycrystals(3Y-TZP)after different aging processes", Microsc Microanal, 22, pp.1179~1188 (2016)