PURPOSE. The aim of this study was to investigate and compare the color stability of provisional restorative materials fabricated by 3D printing, dental milling, and conventional materials. MATERIALS AND METHODS. For the experimental groups, two commercially available 3D-printing provisional resins (E-Dent 100; EnvisionTEC GmbH, Germany & VeroGlazeTM; Stratasys®, USA), two dental milling blocks (PMMA Disk; Yamahachi Dental Co., Japan & Telio®CAD; Ivoclar Vivadent AG, Liechtenstein), and two conventional materials (AlikeTM; GC Co., Japan & Luxatemp automix plus; DMG, Germany) were used. The water sorption and solubility test were (n=10, respectively) carried out according to ISO4049:2000 (International Standards Organization, Geneva, Switzerland). For the color stability test (n=10), coffee and black tea were used as staining solutions, and the specimens were stored for 12 weeks. Data were analyzed by one-way ANOVA and Tukey’s HSD using SPSS version 22.0 (SPSS Inc. Chicago, IL, USA) (P<.05). RESULTS. Alike and Veroglaze showed the highest values and Luxatemp showed the lowest water sorption. In the color stability test, the ΔE of conventional materials varied depending on the staining solution. PMMA milling blocks showed a relatively low ΔE up to 4 weeks, and then significantly increased after 8 weeks (P<.05). 3D-printed materials exhibited a high ΔE or a significant increase over time (P<.05). CONCLUSION. The degree of discoloration increased with time, and a visually perceptible color difference value (ΔE) was shown regardless of the materials and solutions. PMMA milled and 3 D-printed materials showed more rapid change in discoloration after 8 weeks.
Abstract
PURPOSE. The aim of this study was to investigate and compare the color stability of provisional restorative materials fabricated by 3D printing, dental milling, and conventional materials. MATERIALS AND METHODS. For the experimental groups, two commercially available 3D-printing provisional resins (E-Dent 100; EnvisionTEC GmbH, Germany & VeroGlazeTM; Stratasys®, USA), two dental milling blocks (PMMA Disk; Yamahachi Dental Co., Japan & Telio®CAD; Ivoclar Vivadent AG, Liechtenstein), and two conventional materials (AlikeTM; GC Co., Japan & Luxatemp automix plus; DMG, Germany) were used. The water sorption and solubility test were (n=10, respectively) carried out according to ISO4049:2000 (International Standards Organization, Geneva, Switzerland). For the color stability test (n=10), coffee and black tea were used as staining solutions, and the specimens were stored for 12 weeks. Data were analyzed by one-way ANOVA and Tukey’s HSD using SPSS version 22.0 (SPSS Inc. Chicago, IL, USA) (P<.05). RESULTS. Alike and Veroglaze showed the highest values and Luxatemp showed the lowest water sorption. In the color stability test, the ΔE of conventional materials varied depending on the staining solution. PMMA milling blocks showed a relatively low ΔE up to 4 weeks, and then significantly increased after 8 weeks (P<.05). 3D-printed materials exhibited a high ΔE or a significant increase over time (P<.05). CONCLUSION. The degree of discoloration increased with time, and a visually perceptible color difference value (ΔE) was shown regardless of the materials and solutions. PMMA milled and 3 D-printed materials showed more rapid change in discoloration after 8 weeks.
참고문헌 (19)
- Rosenstiel S, "Contemporary fixed prosthodontics", pp.381~ (2000), Elsevier
- Anusavice KJ, "Phillips’ Science of Dental Materials", pp.145~146 (2003), Elsevier
- Sham AS, "Color stability of provisional prosthodontic materials", J Prosthet Dent, 91, pp.447~452 (2004)
- Rutkunas V, "Effects of different food colorants and polishing techniques on color stability of provisional prosthetic materials", Dent Mater J, 29, pp.167~176 (2010)
- Guler AU, "Effects of different drinks on stainability of resin composite provisional restorative materials", J Prosthet Dent, 94, pp.118~124 (2005)
- Samra AP, "Color stability evaluation of aesthetic restorative materials", Braz Oral Res, 22, pp.205~210 (2008)
- Rayyan MM, "Comparison of interim restorations fabricated by CAD", CAM with those fabricated manually, 2015, pp.114, 414~419
- Elagra MI, "Color stability and marginal integrity of interim crowns : An in vitro study", Eur J Dent, 11, pp.330~334 (2017)
- Dawood A, "3D printing in dentistry", Br Dent J, 219, pp.521~529 (2015)
- Abduo J, "Trends in computer-aided manufacturing in prosthodontics : a review of the available streams", Int J Dent, 2014, pp.783948~ (2014)
- "ISO 4049. Dentistry-Polymerbased restorative materials", International Standards Organization (ISO), ~ (2009)
- Swaney AC, "American Dental Association specification No. 12 for denture base resin: second revision", J Am Dent Assoc, 46, pp.54~66 (1953)
- Carter EC, "Commission Internationale de l’eclairage (CIE) 15:2004", CIE Central Bureau, ~ (2004)
- Ergün G, "In vitro color stability of provisional crown and bridge restoration materials", Dent Mater J, 24, pp.342~350 (2005)
- Mickeviciute E, "In vitro color and roughness stability of different temporary restorative materials", Stomatologija, 18, pp.66~72 (2016)
- Haselton DR, "Color stability of provisional crown and fixed partial denture resins", J Prosthet Dent, 93, pp.70~75 (2005)
- Eldiwany M, "Color stability of lightcured and post-cured composites", Am J Dent, 8, pp.179~181 (1995)
- Goldstein GR, "Repeatability of a specially designed intraoral colorimeter", J Prosthet Dent, 69, pp.616~619 (1993)
- Akashi A, "The relationship between water absorption characteristics and the mechanical strength of resin-modified glass-ionomer cements in long-term water storage", Biomaterials, 20, pp.1573~1578 (1999)