Recently, as people’s interest in wood has increased, the use of wood as household and landscape decking materials has increased. As the deck material, imported wood such as synthetic wood, Ipe, and Malas was used in addition to the existing preserved wood, but recently deck use has been activated as part of the activation of domestic materials. As an important quality factor in the selection of such decking material, various durability along with weatherability for long - term use is required for maintenance. Generally used tropical hardwoods have excellent weatherability and durability without additional preservative treatment. However, the domestic larch is a wood species with a higher specific gravity and durability than ordinary conifers. However, it has not yet been used as a deck material due to lack of comparative studies on its characteristics. Therefore, hardness and durability of wood were measured using six specimens of Ipe, Massaranduba, Malas, Douglas-fir, Larch and Torrefied-Larch. Density Profile was used to measure the density, and Brinell hardness test and resistance test against momentary impact were carried out for the test of resistance to static load. Also, The hardness and durability of wood were measured by castor test with resistance test against dynamic load, as well as, nail down test by experiment on surface hardness and durability. As a result of the experiment, the hardness was increased in proportion to the density, and it was confirmed that the imported lumber was harder and durable than the domestic larch.

Abstract

Recently, as people’s interest in wood has increased, the use of wood as household and landscape decking materials has increased. As the deck material, imported wood such as synthetic wood, Ipe, and Malas was used in addition to the existing preserved wood, but recently deck use has been activated as part of the activation of domestic materials. As an important quality factor in the selection of such decking material, various durability along with weatherability for long - term use is required for maintenance. Generally used tropical hardwoods have excellent weatherability and durability without additional preservative treatment. However, the domestic larch is a wood species with a higher specific gravity and durability than ordinary conifers. However, it has not yet been used as a deck material due to lack of comparative studies on its characteristics. Therefore, hardness and durability of wood were measured using six specimens of Ipe, Massaranduba, Malas, Douglas-fir, Larch and Torrefied-Larch. Density Profile was used to measure the density, and Brinell hardness test and resistance test against momentary impact were carried out for the test of resistance to static load. Also, The hardness and durability of wood were measured by castor test with resistance test against dynamic load, as well as, nail down test by experiment on surface hardness and durability. As a result of the experiment, the hardness was increased in proportion to the density, and it was confirmed that the imported lumber was harder and durable than the domestic larch.

참고문헌 (10)

  1. "Hardness test method of wood, General method, KS F 2212", Korea Standard, ~ (2004)
  2. "Test method for resistance to drawing nails or screws of wood, General method, KS F ISO 9087", Korea Standard, ~ (2004)
  3. Jang, S. S, "Impact-Response of Floor Construction Materials", Journal of the Korean Wood Science and Technology, pp.83~87 (1995)
  4. Cha, J. K, "Comparative study on nail and wood screw withdrawal behavior for domestic small diameter logs", Journal of the Korean Wood Science and Technology, pp.85~91 (2003)
  5. "Elastic, textiles and laminated flooring - castor chair test, General method, KS K ISO 4918", Korea Standard, ~ (2011)
  6. Alper Aytekin., "Determination of Screw and Nail Withdrawal Resistance of Some Important Wood Species", International Journal of Molecular Sciences, pp.626~637 (2008)
  7. Bror Sundqvist, "Determination of formic-acid and acetic acid concentrations formed during hydrothermal treatment of birch wood and its relation to colour, strength and hardness", Wood Sci Technol, pp.549~561 (2006)
  8. H. Holmberg, "Influence of grain angle on Brinell hardness of Scots pine (Pinus sylvestris L.)", Holz als Roh - und Werkstoff, 58, pp.91~95 (2000)
  9. Murat KILIC, "Comparative Analysis of the Nail and Screw Withdrawal Resistances of Fir (Abies Mill.), Cherry (Prunus Avium L.), Walnut (Juglans Regia L.) and Oak (Quercus L.) Wood", European Coatings Journal, pp.106~ (2007)
  10. Seiji Hirata, "Hardness distribution on wood surface", J Wood Sci, 47, pp.1~7 (2001)

관련 논문AI추천

이 간행물의 다른 논문 (4건)