RF-MEMS 소자의 웨이퍼 레벨 밀봉 패키징을 위한 열압축 본딩

Thermocompression bonding for wafer level hermetic packaging of RF-MEMS devices

1

조회

0

다운로드

1

인용

0

참고문헌

주제분류공학일반

초록

Abstract

In this study, we describe a low-temperature wafer-level thermocompression bonding using electroplated gold seal line and bonding pads by electroplating method for RF-MEMS devices. Silicon wafers, electroplated with gold (Au), were completely bonded at 320oC for 30min at a pressure of 2.5MPa. The through-hole interconnection between the packaged devices and external terminal did not need metal filling process and was made by gold films deposited on the sidewall of the through-hole. This process was low-cost and short in duration. Helium leak rate, which is measured to evaluate the reliability of bonded wafers, was 2.740.61410-10 Pam3/s. The insertion loss of the CPW packaged was 0.069~0.085dB. The difference of the insertion loss between the unpackaged and packaged CPW was less than -0.03. These values show very good RF characteristics of the packaging. Therefore, gold thermocompression bonding can be applied to high quality hermetic wafer level packaging of RF-MEMS devices.

참고문헌 (14)

  1. 주병권, "실리콘 직접 접합", 전기화학적 식각정지를 이용한 실리콘 다이아프램의 형성과 실리콘 압력센서 제조에의 응용, 1994., pp.3(3), 45~53
  2. 주병권, "실리콘 기판과 ITO가 코팅된 #7059 유리 기판간의 정전 열 접합", 7(3), pp.65~71 (1998)
  3. R. F. Wolffenbuttel, "Low-temperature intermediate Au-Si wafer bonding", 62(1), pp.680~686 (1997)
  4. A.-L. Tiensuu, "Assembling three-dimensional microstructures using gold-silicon eutectic bonding", 45(3), pp.227~236 (1994)
  5. F. Niklaus, "Low-temperature full wafer adhesive bonding", 11(2), pp.100~107 (2001)
  6. S. C. Chong, "Effect of passivation on frit glass bonding method for wafer level hermetic sealing on devices", pp.307~310 (2003)
  7. S. Siau, "Processing quality results for electroless", electroplating of high-aspect ratio plated through holes in industrially produced printed circuit boards, 2005, pp.45(3), 675~687
  8. D. H. Seah, "DC", pulse plating of copper for trench, pp.2001., 114(3)[DOI]
  9. W. P. Dow, "A novel copper electroplating formula for laser-drilled micro via and through hole filling", 30(3), pp.33~36 (2004)
  10. C. H. Tsau, "Fabrication of wafer-level thermocompression bonds", 11(6), pp.641~647 (2002)
  11. D. Sparks, "Wafer-to-wafer bonding of nonplanarized MEMS surfaces using solder", 11(6), pp.630~634 (2001)
  12. W. H. Ko, "Packaging of microfabricated devices and systems", 42(2), pp.169~175 (1995)
  13. T. J. Harpster, "Field-assisted bonding of glass to Si-Au eutectic solder for packaging applications", pp.630~633 (2003)
  14. A. Fan, "Copper wafer bonding", 2(10), pp.534~536 (1999)

관련 논문AI추천

이 간행물의 다른 논문 (11건)