초록

One factor for successful prognosis of finished dental prosthesis is good marginal fit. The purpose of this study in vitro investigation was to compare the marginal fit of all-ceramic crown before and after porcelain veneering, to evaluate the influence of high temperature of the porcelain firing on the fit. For this experiment, model of abutment tooth of maxillary right central incisor was prepared. Ten working models were produced. Ten zirconia cores were made by dental computer aided design/computer aided manufacturing system. The marginal fit of specimens were examined using silicone replica technique. Silicone replicas were sectioned four times and were measured through a digital microscope (x160). Marginal fit is a distance connected between edge end part of specimen and abutment margin. Each specimens was measured twice, the first measurement was done prior to veneering porcelain firing, while the second measurement was done after the porcelain firing to evaluate this process. Statistical analyses were performed with paired t-test. Mean±SD marginal fit was 60.8±14.2 mm for zirconia core and 86.1±13.3 mm for all-ceramic crown. They were statistically significant differences (p<0.001). But all specimens showed a marginal fit where the gap widths ranged within the clinical recommendation (120 mm), all-ceramic crown production using the zirconia core was adequate.

Abstract

One factor for successful prognosis of finished dental prosthesis is good marginal fit. The purpose of this study in vitro investigation was to compare the marginal fit of all-ceramic crown before and after porcelain veneering, to evaluate the influence of high temperature of the porcelain firing on the fit. For this experiment, model of abutment tooth of maxillary right central incisor was prepared. Ten working models were produced. Ten zirconia cores were made by dental computer aided design/computer aided manufacturing system. The marginal fit of specimens were examined using silicone replica technique. Silicone replicas were sectioned four times and were measured through a digital microscope (x160). Marginal fit is a distance connected between edge end part of specimen and abutment margin. Each specimens was measured twice, the first measurement was done prior to veneering porcelain firing, while the second measurement was done after the porcelain firing to evaluate this process. Statistical analyses were performed with paired t-test. Mean±SD marginal fit was 60.8±14.2 mm for zirconia core and 86.1±13.3 mm for all-ceramic crown. They were statistically significant differences (p<0.001). But all specimens showed a marginal fit where the gap widths ranged within the clinical recommendation (120 mm), all-ceramic crown production using the zirconia core was adequate.

참고문헌 (22)

  1. Conrad HJ, "Current ceramic materials and systems with clinical recommendations: a systematic review", J Prosthet Dent, 98, pp.389~404 (2007)
  2. Rosenstiel SF, "Contemporary fixed prosthodontics", pp.774~ (2006), Elsevier, St. Louis
  3. Denry I, "State of the art of zirconia for dental applications", Dent Mater, 24, pp.299~307 (2008)
  4. 김기백, "전악의 디지털 인상 채득 시 치과용 모형재가 디지털 모형 정확성에 미치는 영향", 치위생과학회지, 12(6), pp.617~623 (2012), 한국치위생과학회
  5. Luthardt RG, "Reliability and properties of ground Y-TZP-zirconia ceramics", J Dent Res, 81, pp.487~491 (2002)
  6. Tuntiprawon M, "The effect of cement thickness on the fracture strength of all-ceramic crowns", Aust Dent J, 40, pp.17~21 (1995)
  7. Faucher RR, "Distortion related to margin design in porcelain-fused-to metal restorations", J Prosthet Dent, 43, pp.149~155 (1980)
  8. Dederich DN, "The effect of repeated firings on the margins of nonprecious ceramometals", J Prosthet Dent, 51, pp.628~630 (1984)
  9. Hamaguchi H, "Marginal distortion of the porcelain bonded-to-metal complete crown: an SEM study", J Prosthet Dent, 47, pp.146~153 (1982)
  10. Bridger DV, "Distortion of ceramometal fixed partial dentures during the firing cycle", J Prosthet Dent, 45, pp.507~514 (1981)
  11. Buchanan WT, "The effect of repeated firings and strength on marginal distortion in two ceramometal systems", J Prosthet Dent, 45, pp.502~506 (1981)
  12. Komine F, "Influence of porcelain-firing procedures on the marginal distortion of electroformed metal-ceramic restorations", Quintessence Int, 38, pp.E583~E588 (2007)
  13. Sarver DM, "The importance of incisor positioning in the esthetic smile: the smile arc", Am J Orthod Dentofacial Orthop, 120, pp.98~111 (2001)
  14. 한만소, "주조에 의한 Core와 CAD-CAM에 의한 Core의 적합도 비교평가", 치위생과학회지, 12(4), pp.368~374 (2012), 한국치위생과학회
  15. 김재홍, "고정성 보철물의 적합도 측정 시 사용하는 실리콘 복제본 기술의 정확도 평가", 치위생과학회지, 12(6), pp.566~571 (2012), 한국치위생과학회
  16. Reich S, "Clinical fit of all-ceramic three-unit fixed partial dentures, generated with three different CAD", CAM systems, 2005, pp.113, 174~179
  17. Vigolo P, "An in vitro evaluation of fit of zirconium-oxide-based ceramic four-unit fixed partial dentures, generated with three different CAD", CAM systems, before and after porcelain firing cycles and after glaze cycles, 2008, pp.17, 621~626
  18. McLean JW, "The estimation of cement film thickness by an in vivo technique", Br Dent J, 131, pp.107~111 (1971)
  19. Ostlund LE, "Cavity design and mathematics: their effect on gaps at the margins of cast restorations", Oper Dent, 10, pp.122~137 (1985)
  20. Sulaiman F, "A comparison of the marginal fit of in-ceram, IPS empress, and procera crowns", Int J Prosthodont, 10, pp.478~484 (1997)
  21. Gulker I, "Margins", NY State Dent J, 51, pp.213~217 (1985)
  22. Moldovan O, "Internal and external fit of CAM-made zirconia bridge frameworks-a pilot study", Dtsch Zahnarztl Z, 61, pp.38~42 (2006)

관련 논문AI추천

이 간행물의 다른 논문 (12건)