초록

Objectives : The purpose of this in vitro study was to evaluate the effect of firing cycles on the marginal and internal fit of metal ceramic crown. Methods : Ten same cases of stone models (abutment teeth 11) were manufactured. Ten cobalt-chrome cores were made per each models and the marginal and internal fit was evaluated through a silicone replica technique. The marginal and internal fit of specimens was measured twice. The first measurement was done after manufacturing cobalt-chrome alloy core and the second measurement was done after porcelain firing. T-test of paired sample for statistical analysis was executed with SPSS 12.0K for Windows (α=0.05). Results : Mean(SD) marginal and internal fit were 77.1(23.3) ㎛ for the cobalt-chrome alloy core group and 84.4(21.9) ㎛ for the metal-ceramic crown group. They were statistically significant differences between groups for marginal and internal fit (p<.05). Conclusions : All metal ceramic crowns showed marginal and internal fit ranged within the current clinical recommendations.

Abstract

Objectives : The purpose of this in vitro study was to evaluate the effect of firing cycles on the marginal and internal fit of metal ceramic crown. Methods : Ten same cases of stone models (abutment teeth 11) were manufactured. Ten cobalt-chrome cores were made per each models and the marginal and internal fit was evaluated through a silicone replica technique. The marginal and internal fit of specimens was measured twice. The first measurement was done after manufacturing cobalt-chrome alloy core and the second measurement was done after porcelain firing. T-test of paired sample for statistical analysis was executed with SPSS 12.0K for Windows (α=0.05). Results : Mean(SD) marginal and internal fit were 77.1(23.3) ㎛ for the cobalt-chrome alloy core group and 84.4(21.9) ㎛ for the metal-ceramic crown group. They were statistically significant differences between groups for marginal and internal fit (p<.05). Conclusions : All metal ceramic crowns showed marginal and internal fit ranged within the current clinical recommendations.

참고문헌 (31)

  1. 김영숙, "의치 장착 노인과 임플란트 장착 노인의 저작능력 및 삶의 질 비교 연구", 한국치위생학회지, 11(5), pp.629~636 (2011), 한국치위생학회
  2. 박은미, "치과심미치료 만족도가 구강건강관련 삶의 질(OHIP-14)에 미치는 영향", 한국치위생학회지, 11(6), pp.863~870 (2011), 한국치위생학회
  3. Petteno D, "Comparison of marginal fit of 3 different metal-ceramic systems: an in vitro study", Int J Prosthodont, 13(5), pp.405~408 (2000)
  4. Rosenstiel SF, "Contemporary fixed prosthodontics", pp.606~608 (2006), Mosby
  5. Anusavice KJ, "Phillips’science of dental materials", pp.621~654 (2003), W.B. Saunders
  6. Pierce LH, "A status report of possible risks of base metal alloys and their components", J Prosthet Dent, 62(2), pp.234~238 (1989)
  7. Wassell RW, "Crowns and extra-coronal restorations: materials selection", Br Dent J, 192(4), pp.199~211 (2002)
  8. Vigolo P, "An in vitro evaluation of fit of zirconium -oxide-based ceramic four-unit fixed partial dentures, generated with three different CAD", CAM systems, before and after porcelain firing cycles and after glaze cycles, 2008, pp.17(8), 621~626
  9. Jahangiri L, "Assessment of sensitivity and specificity of clinical evaluation of cast restoration marginal accuracy compared to stereomicroscopy", J Prosthet Dent, 93(2), pp.138~142 (2005)
  10. Mejia R, "Marginal fit of metal ceramic restorations subjected to a standardized postsoldering technique", J Prosthet Dent, 83(5), pp.535~539 (2000)
  11. Limkangwalmongkol P, "Precision of fit of two margin designs for metal–ceramic crowns", J Prosthodont, 16(4), pp.233~237 (2007)
  12. Foster LV, "Failed conventional bridge work from general dental practice: clinical aspects and treatment needs of 142 cases", Br Dent J, 168(5), pp.199~201 (1990)
  13. Tjan AH, "Marginal accuracy of complete crowns made from alternative casting alloys", J Prosthet Dent, 66(2), pp.157~164 (1991)
  14. Soriani NC, "Effect of the use of die spacer on the marginal fit of copings cast in Ni-Cr, Ni-Cr-Be and commercially pure titanium", Braz Dent J, 18(3), pp.225~230 (2007)
  15. Campbell SD, "Thermal cycling distortion of metal ceramics: part I-metal collar width", J Prosthet Dent, 67(5), pp.603~608 (1992)
  16. Fonseca JC, "Stress-relieving and porcelain firing cycle influence on marginal fit of commercially pure titanium and titanium-aluminium -vanadium copings", Dent Mater, 19(7), pp.686~691 (2003)
  17. Lakhani SA, "Influence of cold working and thermal treatment on the fit of implant supported metal ceramic fixed partial dentures", J Prosthet Dent, 88(2), pp.159~169 (2002)
  18. Hasanreisoglu U, "An analysis of maxillary anterior teeth: facial and dental proportions", J Prosthet Dent, 94(6), pp.530~538 (2005)
  19. Holmes JR, "Considerations in measurement of marginal fit", J Prosthet Dent, 62(4), pp.405~408 (1989)
  20. Reich S, "Clinical fit of fourunit zirconia posterior fixed dental prostheses", Eur J Oral Sci, 116(6), pp.579~584 (2008)
  21. Wettstein F, "Clinical study of the internal gaps of zirconia and metal frameworks for fixed partial dentures", Eur J Oral Sci, 116(3), pp.272~279 (2008)
  22. Harris IR, "A comparison of the fit of sparkeroded titanium copings and cast gold alloy copings", Int J Prosthodont, 7(4), pp.348~355 (1994)
  23. McLean JM, "The estimation of cement film thickness by an in vivo technique", Br Dent J, 131(3), pp.107~111 (1971)
  24. Fransson B, "The fit of metal-ceramic crowns, a clinical study", Dent Mater, 1(5), pp.197~199 (1985)
  25. Strating H, "Evaluation of the marginal integrity of ceramometal restorations: part I", J Prosthet Dent, 46(1), pp.59~65 (1981)
  26. Buchanan WT, "The effect of repeated firings and strength on marginal distortion in two ceramometal systems", J Prosthet Dent, 45(5), pp.502~506 (1981)
  27. Bridger DV, "Distortion of ceramometal fixed partial dentures during the firing cycle", J Prosthet Dent, 45(5), pp.507~514 (1981)
  28. Campbell SD, "Thermal cycling distortion of metal ceramics: part I—metal collar width", J Prosthet Dent, 67(5), pp.603~608 (1992)
  29. Balkaya MC, "Influence of firing cycles on the margin distortion of 3 all-ceramic crown systems", J Prosthet Dent, 93(4), pp.346~355 (2005)
  30. Komine F, "Influence of porcelain-firing procedures on the marginal distortion of electroformed metal-ceramic restorations", Quintessence Int, 38(10), pp.E583~E588 (2007)
  31. Prakash P, "Effect of firing cycle and surface finishing on the sag resistance of long-span metal ceramic framework using base metal alloys—an in vitro study", MJAFI, 68(2), pp.142~150 (2012)

관련 논문AI추천

이 간행물의 다른 논문 (19건)