2205 duplex stainless steels have been used for the construction of the marine environment, because oftheir excellent corrosion resistance and high strength. However, the resistance to hydrogen embrittlement(HE) may be less than that of 316L austenitic stainless steel. The reason why 316L stainless steels havebetter resistance to HE is associated with crystal structure (FCC, face centered cubic) and the higher stackingfaults energy than 2205 duplex stainless steels. Furthermore 2205 stainless steels with or without tungstenwere also examined in terms of HE. 2205 stainless steels containing tungsten is less resistible to HE. Itis because dislocation tangle was formed in 2205 duplex stainless steels. Slow strain-rate tensile test (SSRT)was conducted to measure the resistance to HE under the cathodic applied potential. Hydrogen embrittlementindex (HEI) was used to evaluate HE resistance through the quantitative calculation.
Abstract
2205 duplex stainless steels have been used for the construction of the marine environment, because oftheir excellent corrosion resistance and high strength. However, the resistance to hydrogen embrittlement(HE) may be less than that of 316L austenitic stainless steel. The reason why 316L stainless steels havebetter resistance to HE is associated with crystal structure (FCC, face centered cubic) and the higher stackingfaults energy than 2205 duplex stainless steels. Furthermore 2205 stainless steels with or without tungstenwere also examined in terms of HE. 2205 stainless steels containing tungsten is less resistible to HE. Itis because dislocation tangle was formed in 2205 duplex stainless steels. Slow strain-rate tensile test (SSRT)was conducted to measure the resistance to HE under the cathodic applied potential. Hydrogen embrittlementindex (HEI) was used to evaluate HE resistance through the quantitative calculation.
참고문헌 (11)
- M. C. Young, , Mater. Chem. Phys, 91, pp.21~ (2005)
- D. M. Bromley, , Ph. D, pp.2008
- J. Michalska, , Mater, Sci. Eng, 35, pp.1~ (2012)
- Z. Jingwei, , Corros. Sci, 82, pp.380~ (2014)
- K. Alfons H. M, , Metall. Mater. Trans. B, 31, pp.1475~ (2000)
- "ASTM Standard E8", E8M, Standard Test Methods for Tensile Testing of Metallic Materials, 2009
- "ASTM Standard G129, Slow Strain Rate Testing to Evaluate the Susceptibility of Metallic Materials to Environmentally Assisted Cracking", ~ (2013)
- L. Erik, , springer sci. & business media, 1, pp.133~ (2012)
- W. Songqing, "Metallurgical Evaluation of Cast Duplex Stainless Steels and Their Weldments", Ph. D, pp.2001
- G. Almaida, , Mater & Tech, 46, pp.519~ (2012)
- S. M. Teus, , Mater. Sci. Eng. A, 497, pp.290~ (2008)