본문 바로가기
KERD
논문KCI 등재

소성인장변형 몇 아연도금된 Fe-Mn-C계 TWIP 강의 전기화학적 수소투과거동

Electrochemical Hydrogen Permeation Behaviors of Pre-Strained Fe-Mn-C TWIP Steel With or Without Zn Coating

1

조회

0

다운로드

1

인용

0

참고문헌

키워드

주제분류금속공학

초록

This study aimed to evaluate hydrogen permeation behaviors of pre-strained twinning-induced plasticity steel with or without Zn coating using electrochemical permeation technique. In contrast to un-strained and 30% strained samples, permeation current density was measured in the 60% strained sample. Tensile prestraining at 60% involved microstructural modifications, including a high level of dislocation density and stacking fault with a semi-coherent twin boundary, which might provide a high diffusion path for hydrogen atoms. However, reproducibility of measurements of hydrogen permeation current was low due to nonuniform deformation and localized stress concentration. On the other hand, the permeation current was not measured in pre-strained TWIP steel with Zn coating. Instead, numerous blisters with some cracks were observed on the surface of the coating layer. In locally damaged Zn coating under tensile straining, hydrogen atoms could relatively easily permeate through the coating layer. However, they were trapped at the interface between the coating layer and the substrate, which might delay hydrogen penetration into the steel substrate.

Abstract

This study aimed to evaluate hydrogen permeation behaviors of pre-strained twinning-induced plasticity steel with or without Zn coating using electrochemical permeation technique. In contrast to un-strained and 30% strained samples, permeation current density was measured in the 60% strained sample. Tensile prestraining at 60% involved microstructural modifications, including a high level of dislocation density and stacking fault with a semi-coherent twin boundary, which might provide a high diffusion path for hydrogen atoms. However, reproducibility of measurements of hydrogen permeation current was low due to nonuniform deformation and localized stress concentration. On the other hand, the permeation current was not measured in pre-strained TWIP steel with Zn coating. Instead, numerous blisters with some cracks were observed on the surface of the coating layer. In locally damaged Zn coating under tensile straining, hydrogen atoms could relatively easily permeate through the coating layer. However, they were trapped at the interface between the coating layer and the substrate, which might delay hydrogen penetration into the steel substrate.

참고문헌 (15)

  1. 이오연, "고 Mn계 TRIP", TWIP 강의 수소취성 거동, 2008, pp.18(7), 394~399[DOI]
  2. O Grässel, "High strength Fe–Mn–(Al, Si) TRIP", TWIP steels development — properties — application, 2000, pp.16(10-11), 1391~1409[DOI]
  3. O. Bouaziz, "High manganese austenitic twinning induced plasticity steels: A review of the microstructure properties relationships", Current Opinion in Solid State and Materials Science, 15(4), pp.141~168 (2011), Elsevier BV[DOI]
  4. Young Soo Chun, "Delayed static failure of twinning-induced plasticity steels", Scripta Materialia, 66(12), pp.960~965 (2012), Elsevier BV[DOI]
  5. Kyung-Shik Kim, "Nitrogen effect on hydrogen diffusivity and hydrogen embrittlement behavior in austenitic stainless steels", Scripta Materialia, 184, pp.70~73 (2020), Elsevier BV[DOI]
  6. Hyunju Ji, "The effect of pre-strain on hydrogen embrittlement in 310S stainless steel", Journal of Alloys and Compounds, 598, pp.205~212 (2014), Elsevier BV[DOI]
  7. Kwang-Geun Chin, "Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels", Materials Science and Engineering: A, 528(6), pp.2922~2928 (2011), Elsevier BV[DOI]
  8. "ISO 17081:2004 (E), Method of Measurement of Hydrogen Permeation and Determination of Hydrogen Uptake and Transport in Metals by an Electrochemical Technique", ISO, ~ (2004)
  9. Sung Jin Kim, "Electrochemical hydrogen permeation measurement through high-strength steel under uniaxial tensile stress in plastic range", Scripta Materialia, 66(12), pp.1069~1072 (2012), Elsevier BV[DOI]
  10. 박진성, "아연 및 알루미늄이 도금된 Hot-Press Forming 강의 염화물 환경 내전기화학적 부식 및 수소확산거동", 한국재료학회지, 28(5), pp.286~294 (2018), 한국재료학회
  11. M. Kurkela, "Influence of plastic deformation on hydrogen transport in 2 Cr-1Mo steel", Scripta Metallurgica, 16(4), pp.455~459 (1982), Elsevier BV[DOI]
  12. 정종구, "Fe-Mn-C계 TWIP강의 재질특성에 미치는 소둔온도와 첨가원소의 영향", 한국재료학회지, 20(7), pp.385~391 (2010), 한국재료학회
  13. Hyung-Jun Cho, "Origin of deformation twins and their influence on hydrogen embrittlement in cold-rolled austenitic stainless steel", International Journal of Hydrogen Energy, 46(42), pp.22195~22207 (2021), Elsevier BV[DOI]
  14. A. Saeed-Akbari, "Derivation and Variation in Composition-Dependent Stacking Fault Energy Maps Based on Subregular Solution Model in High-Manganese Steels", Metallurgical and Materials Transactions A, 40(13), pp.3076~3090 (2009), Springer Science and Business Media LLC[DOI]
  15. S. K. Rajagopalan, , pp.2012

관련 논문AI추천

이 간행물의 다른 논문 (8건)