PURPOSE. The purpose of this study was to find out the effect of immediate dentin sealing (IDS) on bond strength of ceramic restoration under various thermocycling periods with DBA (dentin bonding agent system). MATERIALS AND METHODS. Fifty freshly extracted human mandibular third molars were divided into 5 groups (1 control and 4 experimental groups) of 10 teeth. We removed enamel layer of sound teeth and embedded them which will proceed to be IDS, using All Bond II. A thermocycling was applied to experimental groups for 1, 2, 7, 14 days respectively and was not applied to control group. IPS Empress II for ceramic was acid-etched with ceramic etchant (9.5% HF) and silane was applied. Each ceramic disc was bonded to specimens with Duo-link, dual curable resin cement by means of light curing for 100 seconds. After the cementation procedures, shear bond strength measurement and SEM analysis of the fractured surface were done. The data were analyzed with a one-way ANOVA and Tukey multiple comparison test (α=.05). RESULTS. There were no statistically significant differences between 4 experimental groups and control group, however the mean value started to decrease in group 7d, and group 14d showed the lowest mean bond strength in all groups. Also, group 7d and 14d showed distinct exposed dentin and collapsed hybrid layer was observed in SEM analysis. CONCLUSION. In the present study, it can be concluded that ceramic restorations like a laminate veneer restoration should be bonded using resin cement within one week after IDS procedure.
Abstract
PURPOSE. The purpose of this study was to find out the effect of immediate dentin sealing (IDS) on bond strength of ceramic restoration under various thermocycling periods with DBA (dentin bonding agent system). MATERIALS AND METHODS. Fifty freshly extracted human mandibular third molars were divided into 5 groups (1 control and 4 experimental groups) of 10 teeth. We removed enamel layer of sound teeth and embedded them which will proceed to be IDS, using All Bond II. A thermocycling was applied to experimental groups for 1, 2, 7, 14 days respectively and was not applied to control group. IPS Empress II for ceramic was acid-etched with ceramic etchant (9.5% HF) and silane was applied. Each ceramic disc was bonded to specimens with Duo-link, dual curable resin cement by means of light curing for 100 seconds. After the cementation procedures, shear bond strength measurement and SEM analysis of the fractured surface were done. The data were analyzed with a one-way ANOVA and Tukey multiple comparison test (α=.05). RESULTS. There were no statistically significant differences between 4 experimental groups and control group, however the mean value started to decrease in group 7d, and group 14d showed the lowest mean bond strength in all groups. Also, group 7d and 14d showed distinct exposed dentin and collapsed hybrid layer was observed in SEM analysis. CONCLUSION. In the present study, it can be concluded that ceramic restorations like a laminate veneer restoration should be bonded using resin cement within one week after IDS procedure.
참고문헌 (45)
- Magne P, "Immediate dentin sealing: a fundamental procedure for indirect bonded restorations", J Esthet Restor Dent, 17, pp.144~154 (2005)
- Paul SJ, "The dual bonding technique: a modified method to improve adhesive luting procedures", Int J Periodont Restor Dent, 17, pp.536~545 (1997)
- 박동진, "Esthetic improvement in the patient with one missing maxillary central incisor restored with porcelain laminate veneers", The Journal of Advanced of Prosthodontics, 2(3), pp.77~80 (2010), 대한치과보철학회
- Xie J, "In vitro bond strength of two adhesives to enamel and dentin under normal and contaminated conditions", Dent Mater, 9, pp.295~299 (1993)
- Magne P, "Immediate dentin sealing supports delayed restoration placement", J Prosthet Dent, 98, pp.166~174 (2007)
- Christensen GJ, "Resin cements and postoperative sensitivity", J Am Dent Assoc, 131, pp.1197~1199 (2000)
- Gresnigt M, "Esthetic rehabilitation of worn anterior teeth with thin porcelain laminate veneers", Eur J Esthet Dent, 6, pp.298~313 (2011)
- 문지은, "Esthetic restorations of maxillary anterior teeth with orthodontic treatment and porcelain laminate veneers: a case report", The Journal of Advanced of Prosthodontics, 2(2), pp.61~63 (2010), 대한치과보철학회
- Usumez A, "The efficiency of different light sources to polymerize resin cement beneath porcelain laminate veneers", J Oral Rehabil, 31, pp.160~165 (2004)
- Nagayassu MP, "Effect of surface treatment on the shear bond strength of a resinbased cement to porcelain", Braz Dent J, 17, pp.290~295 (2006)
- Rosenbach G, "Effect of enamel etching on tensile bond strength of brackets bonded in vivo with a resin-reinforced glass ionomer cement", Angle Orthod, 77, pp.113~116 (2007)
- Correia SL, "Effect of quartz sand replacement by agate rejects in triaxial porcelain", J Hazard Mater, 163, pp.315~322 (2009)
- Ibarra G, "Microleakage of porcelain veneer restorations bonded to enamel and dentin with a new self-adhesive resin-based dental cement", Dent Mater, 23, pp.218~225 (2007)
- Guarda GB, "Effects of surface treatments, thermocycling, and cyclic loading on the bond strength of a resin cement bonded to a lithium disilicate glass ceramic", Oper Dent, 38, pp.208~217 (2013)
- Braga RR, "Influence of time and adhesive system on the extrusion shear strength between feldspathic porcelain and bovine dentin", Dent Mater, 16, pp.303~310 (2000)
- Drummond JL, "Testing mode and surface treatment effects on dentin bonding", J Biomed Mater Res, 32, pp.533~541 (1996)
- Kato H, "Improved bonding of adhesive resin to sintered porcelain with the combination of acid etching and a two-liquid silane conditioner", J Oral Rehabil, 28, pp.102~108 (2001)
- Kato H, "Effect of etching and sandblasting on bond strength to sintered porcelain of unfilled resin", J Oral Rehabil, 27, pp.103~110 (2000)
- Chen JR, "Carbon dioxide laser application enhances the effect of silane primer on the shear bond strength between porcelain and composite resin", Dent Mater J, 29, pp.731~737 (2010)
- Matsumura H, "Effect of a silane coupling agent and ferric chloride on the bonding of porcelain, quartz and alumina with 4-META", MMA-TBB resin, 1987, pp.6, 135~139
- 최유성, "An effect of immediate dentin sealing on the shear bond strength of resin cement to porcelain restoration", The Journal of Advanced of Prosthodontics, 2(2), pp.39~45 (2010), 대한치과보철학회
- Dozic A, "Color management of porcelain veneers: influence of dentin and resin cement colors", Quintessence Int, 41, pp.567~573 (2010)
- Witzel MF, "Bond strength between polymer resin-based cement and porcelaindentin surfaces: influence of polymerization mode and early cyclic loading", Int J Prosthodont, 16, pp.145~149 (2003)
- Madani M, "Effects of surface treatments on shear bond strengths between a resin cement and an alumina core", J Prosthet Dent, 83, pp.644~647 (2000)
- Dietschi D, "Marginal and internal adaptation of class II restorations after immediate or delayed composite placement", J Dent, 30, pp.259~269 (2002)
- Dietschi D, "In vitro evaluation of marginal and internal adaptation of class II resin composite restorations after thermal and occlusal stressing", Eur J Oral Sci, 106, pp.1033~1042 (1998)
- Ozturk N, "Dentin bond strengths of two ceramic inlay systems after cementation with three different techniques and one bonding system", J Prosthet Dent, 89, pp.275~281 (2003)
- Jayasooriya PR, "Efficacy of a resin coating on bond strengths of resin cement to dentin", J Esthet Restor Dent, 15, pp.105~113 (2003)
- Rueggeberg FA, "The effect of oxygen inhibition on an unfilled", filled composite system, 1990, pp.69, 1652~1658
- Park JW, "Measuring the residual stress in dental composites using a ring slitting method", Dent Mater, 21, pp.882~889 (2005)
- Pashley EL, "Dentin permeability: sealing the dentin in crown preparations", Oper Dent, 17, pp.13~20 (1992)
- Suh BI, "Oxygen-inhibited layer in adhesion dentistry", J Esthet Restor Dent, 16, pp.316~323 (2004)
- Papacchini F, "Composite-to-composite microtensile bond strength in the repair of a microfilled hybrid resin: effect of surface treatment and oxygen inhibition", J Adhes Dent, 9, pp.25~31 (2007)
- Fradeani M, "An 11-year clinical evaluation of leucite-reinforced glass-ceramic crowns: a retrospective study", Quintessence Int, 33, pp.503~510 (2002)
- Oh SC, "Strength and microstructure of IPS Empress 2 glass-ceramic after different treatments", Int J Prosthodont, 13, pp.468~472 (2000)
- Nakamura T, "Fracture resistance of pressable glass-ceramic fixed partial dentures", J Oral Rehabil, 29, pp.951~955 (2002)
- Chang JC, "Tensile bond strengths of composites to a gold-palladium alloy after thermal cycling", J Prosthet Dent, 87, pp.271~276 (2002)
- Andreatta Filho OD, "Study of thermocycling effect on the bond strength between an aluminous ceramic and a resin cement", J Appl Oral Sci, 13, pp.53~57 (2005)
- Borges GA, "Fracture loads of all-ceramic crowns under wet and dry fatigue conditions", J Prosthodont, 18, pp.649~655 (2009)
- Sobrinho LC, "Comparison of the wet and dry fatigue properties of all ceramic crowns", J Mater Sci Mater Med, 9, pp.517~521 (1998)
- Geerts SO, "Microleakage after thermocycling of three self-etch adhesives under resinmodified glass-ionomer cement restorations", Int J Dent, 2010, pp.728453~ (2010)
- Do Nascimento C, "Adhesive bond strength between a ceramic system and composite resin bonded by resinous cement submitted or not to thermocycling process", Minerva Stomatol, 57, pp.103~107 (2008)
- Arici S, "Effects of thermocycling on the bond strength of a resin-modified glass ionomer cement: an in vitro comparative study", Angle Orthod, 73, pp.692~696 (2003)
- Andreatta Filho OD, "Effect of thermocycling on the bond strength of a glass-infiltrated ceramic and a resin luting cement", J Appl Oral Sci, 11, pp.61~67 (2003)
- Qualtrough AJ, "An in vitro evaluation of the marginal integrity of a porcelain inlay system", Int J Prosthodont, 4, pp.517~523 (1991)