PURPOSE. Plasma activation of hydrophobic zirconia surfaces might be suitable to improve the bond strength of luting materials. The aim of this study was to analyze the influence of nonthermal argon-plasma on the shear bond strength (SBS) between zirconia and different combinations of 10-MDP adhesive systems and luting composites after artificial aging. MATERIALS AND METHODS. Two hundred forty Y-TZP specimens were ground automatically with 165 μm grit and water cooling. Half of the specimens received surface activation with nonthermal argon-plasma. The specimens were evenly distributed into three groups according to the adhesive systems ([Futurabond U, Futurabond M, Futurabond M + DCA], VOCO GmbH, Germany, Cuxhaven) and into further two subgroups according to the luting materials ([Bifix SE, Bifix QM], VOCO GmbH). Each specimen underwent artificial aging by thermocycling and water storage. SBS was measured in a universal testing machine. Statistical analysis was performed using ANOVA and Scheffè procedure with the level of significance set to 0.05. RESULTS. Surface activation with nonthermal plasma did not improve the bond strength between zirconia and the tested combinations of adhesive systems and luting materials. The plasma-activation trended to reveal higher bond strength if the self-etch luting material (Bifix SE) was used, irrespective of the adhesive system. CONCLUSION. Plasma-activation seems to be suitable to improve bond strength between zirconia and self-etch resin materials. However, further research is necessary to identify the influence of varying plasma-parameters.

Abstract

PURPOSE. Plasma activation of hydrophobic zirconia surfaces might be suitable to improve the bond strength of luting materials. The aim of this study was to analyze the influence of nonthermal argon-plasma on the shear bond strength (SBS) between zirconia and different combinations of 10-MDP adhesive systems and luting composites after artificial aging. MATERIALS AND METHODS. Two hundred forty Y-TZP specimens were ground automatically with 165 μm grit and water cooling. Half of the specimens received surface activation with nonthermal argon-plasma. The specimens were evenly distributed into three groups according to the adhesive systems ([Futurabond U, Futurabond M, Futurabond M + DCA], VOCO GmbH, Germany, Cuxhaven) and into further two subgroups according to the luting materials ([Bifix SE, Bifix QM], VOCO GmbH). Each specimen underwent artificial aging by thermocycling and water storage. SBS was measured in a universal testing machine. Statistical analysis was performed using ANOVA and Scheffè procedure with the level of significance set to 0.05. RESULTS. Surface activation with nonthermal plasma did not improve the bond strength between zirconia and the tested combinations of adhesive systems and luting materials. The plasma-activation trended to reveal higher bond strength if the self-etch luting material (Bifix SE) was used, irrespective of the adhesive system. CONCLUSION. Plasma-activation seems to be suitable to improve bond strength between zirconia and self-etch resin materials. However, further research is necessary to identify the influence of varying plasma-parameters.

참고문헌 (32)

  1. Rosentritt M, "Influence of resilient support of abutment teeth on fracture resistance of all-ceramic fixed partial dentures: an in vitro study", Int J Prosthodont, 24, pp.465~468 (2011)
  2. Aladag A, "Effect of different cleaning regimens on the adhesion of resin to saliva-contaminated ceramics", J Prosthodont, 24, pp.136~145 (2015)[DOI]
  3. Kohorst P, "Loadbearing capacity of all-ceramic posterior four-unit fixed partial dentures with different zirconia frameworks", Eur J Oral Sci, 115, pp.161~166 (2007)[DOI]
  4. Zhang Y, "Edge chipping and flexural resistance of monolithic ceramics", Dent Mater, 29, pp.1201~1208 (2013)[DOI]
  5. Chen L, "Evaluation of silica-coating techniques for zirconia bonding", Am J Dent, 24, pp.79~84 (2011)
  6. Tolga Külünk, "The effect of alumina and aluminium nitride coating by reactive magnetron sputtering on the resin bond strength to zirconia core", The Journal of Advanced of Prosthodontics, 5(4), pp.382~387 (2013), 대한치과보철학회[DOI]
  7. Pott PC, "Influence of 10-MDP adhesive system on shear bond strength of zirconia-composite interfaces", J Dent Mater Tech, 4, pp.117~126 (2015)
  8. Pott PC, "Influence of artificial aging on the shear bond strength of zirconiacomposite interfaces after pretreatment with new 10-MDP adhesive systems", J Dent Mater Tech, 5, pp.1~9 (2016)
  9. Koizumi H, "Bonding of resin-based luting cements to zirconia with and without the use of ceramic priming agents", J Adhes Dent, 14, pp.385~392 (2012)
  10. Saker S, "Effect of different surface treatments on adhesion of In-Ceram Zirconia to enamel and dentin substrates", J Adhes Dent, 15, pp.369~376 (2013)
  11. Canullo L, "Zirconia-composite bonding after plasma of argon treatment", Int J Prosthodont, 27, pp.267~269 (2014)[DOI]
  12. Noro A, "Influence of hydrophilic pre-treatment on resin bonding to zirconia ceramics", Bull Tokyo Dent Coll, 56, pp.33~39 (2015)[DOI]
  13. Wu CC, "Enhanced hydrophilicity and biocompatibility of dental zirconia ceramics by oxygen plasma treatment", Materials (Basel), 8, pp.684~699 (2015)[DOI]
  14. Tabari K, "The impact of plasma treatment of Cercon zirconia ceramics on adhesion to resin composite cements and surface properties", J Laser Med Sci, 8, pp.56~61 (2017)[DOI]
  15. dos Santos DM, "Aging effect of atmospheric air on zirconia surfaces treated by nonthermal plasma", J Adhes Dent, 17, pp.413~419 (2015)
  16. Casucci A, "Morphological analysis of three zirconium oxide ceramics: Effect of surface treatments", Dent Mater, 26, pp.751~760 (2010)[DOI]
  17. Denry IL, "Microstructural and crystallographic surface changes after grinding zirconia-based dental ceramics", J Biomed Mater Res B Appl Biomater, 76, pp.440~448 (2006)
  18. Kawai Y, "Phase transformation of zirconia ceramics by hydrothermal degradation", Dent Mater J, 30, pp.286~292 (2011)[DOI]
  19. Nakamura T, "The effect of adding silica to zirconia to counteract zirconia's tendency to degrade at low temperatures", Dent Mater J, 30, pp.330~335 (2011)[DOI]
  20. de Gee AF, "True linear polymerization shrinkage of unfilled resins and composites determined with a linometer", Dent Mater, 9, pp.11~14 (1993)[DOI]
  21. Gostemeyer G, "Influence of cooling rate on zirconia", veneer interfacial adhesion, 2010, pp.6, 4532~4538
  22. Ernst CP, "Influence of different luting concepts on long term retentive strength of zirconia crowns", Am J Dent, 22, pp.122~128 (2009)
  23. Lindgren J, "Effect of surface treatments and aging in water on bond strength to zirconia", Oper Dent, 33, pp.675~681 (2008)[DOI]
  24. Ozcan M, "Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging", Dent Mater J, 27, pp.99~104 (2008)[DOI]
  25. Valverde GB, "Surface characterisation and bonding of Y-TZP following non-thermal plasma treatment", J Dent, 41, pp.51~59 (2013)[DOI]
  26. 박찬, "The effect of plasma on shear bond strength between resin cement and colored zirconia", The Journal of Advanced of Prosthodontics, 9(2), pp.118~123 (2017), 대한치과보철학회[DOI]
  27. Liu T, "Nonthermal plasma enhanced bonding of resin cement to zirconia ceramic", Clin Plasma Med, 4, pp.50~55 (2016)[DOI]
  28. Henningsen A, "Changes in surface characteristics of titanium and zirconia after surface treatment with ultraviolet light or non-thermal plasma", Eur J Oral Sci, 126, pp.126~134 (2018)[DOI]
  29. Kitayama S, "Effect of primer treatment on bonding of resin cements to zirconia ceramic", Dent Mater, 26, pp.426~432 (2010)[DOI]
  30. Foxton RM, "Durability of resin cement bond to aluminium oxide and zirconia ceramics after air abrasion and laser treatment", J Prosthodont, 20, pp.84~92 (2011)[DOI]
  31. Ito Y, "Influence of atmospheric pressure low-temperature plasma treatment on the shear bond strength between zirconia and resin cement", J Prosthodont Res, 60, pp.289~293 (2016)[DOI]
  32. Hallmann L, "Effect of surface modifications on the bond strength of zirconia ceramic with resin cement resin", Dent Mater, 32, pp.631~639 (2016)[DOI]

관련 논문AI추천

The effect of plasma on shear bond strength between resin cement and colored zirconia박찬, 박상원, 신진호, 유승환, 윤귀덕, 임현필, 지민경대한치과보철학회 · The Journal of Advanced of Prosthodontics2017 · 제9권 제2호Effect of non-thermal plasma on the shear bond strength of resin cements to Polyetherketoneketone (PEKK)류재준, 박진홍, 송소연, 신상완, 이정열, Wilmart Labriaga대한치과보철학회 · The Journal of Advanced of Prosthodontics2018 · 제10권 제6호In vitro shear bond strength between fluorinated zirconia ceramic and resin cementsCanan Akay, Kadriye Sapmaz, Merve Çakırbay Tanış, Murat Şen, Pınar Akkaş Kavaklı, Turgut Cihan Akçaboy대한치과보철학회 · The Journal of Advanced of Prosthodontics2018 · 제10권 제3호The effect of alumina and aluminium nitride coating by reactive magnetron sputtering on the resin bond strength to zirconia coreÖzgür Öztürk, Şafak Külünk, Şengül Danişman, Seniha Baba, Soner Savaş, Tolga Külünk대한치과보철학회 · The Journal of Advanced of Prosthodontics2013 · 제5권 제4호Effect of atmospheric plasma versus conventional surface treatments on the adhesion capability between self-adhesive resin cement and titanium surfaceEmre Mumcu, Emre Seker, Mehmet Ali Kilicarslan, Pelin Ozkan, Sule Tugba Deniz대한치과보철학회 · The Journal of Advanced of Prosthodontics2015 · 제7권 제3호Effect of universal adhesive pretreatments on the bond strength durability of conventional and adhesive resin cements to zirconia ceramic권태엽, 김영경, 박진우, 이두형, Seung-Hee Han대한치과보철학회 · The Journal of Advanced of Prosthodontics2024 · 제16권 제2호

이 간행물의 다른 논문 (10건)