Influence of heat treatment on the microstructure and the physical and mechanical properties of dental highly translucent zirconia

2

조회

0

다운로드

0

인용

0

참고문헌

키워드

초록

PURPOSE. Microstructural and physico-mechanical characterization of highly translucent zirconia, prepared by milling technology (CAD-CAM) and repeated firing cycles, was the main aim of this in vitro study. MATERIALS AND METHODS. Two groups of samples of two commercial highly-translucent yttria-stabilized dental zirconia, VITA YZ-HTWhite (Group A) and Zolid HT + White (Group B), with dimensions according to the ISO 6872 “Dentistry - Ceramic materials”, were prepared. The specimens of each group were divided into two subgroups. The specimens of the first subgroups (Group A1 and Group B1) were merely the sintered specimens. The specimens of the second subgroups (Group A2 and Group B2) were subjected to 4 heat treatment cycles. The microstructural features (microstructure, density, grain size, crystalline phases, and crystallite size) and four mechanical properties (flexural strength, modulus of elasticity, Vickers hardness, and fracture toughness) of the subgroups (i.e. before and after heat treatment) were compared. The statistical significance between the subgroups (A1/A2, and B1/B2) was evaluated by the t-test. In all tests, P values smaller than 5% were considered statistically significant. RESULTS. A homogenous microstructure, with no residual porosity and grains sized between 500 and 450 nm for group A and B, respectively, was observed. Crystalline yttria-stabilized tetragonal zirconia was exclusively registered in the X-ray diffractograms. The mechanical properties decreased after the heat treatment procedure, but the differences were not statistically significant. CONCLUSION. The produced zirconia ceramic materials can be safely (i.e., according to the ISO 6872) used in extensive fixed prosthetic restorations, such as substructure ceramics for three-unit prostheses involving the molar restoration and substructure ceramics for prostheses involving four or more units. Consequently, milling technology is an effective manufacturing technology for producing zirconia substructures for dental fixed all-ceramic prosthetic restorations.

Abstract

PURPOSE. Microstructural and physico-mechanical characterization of highly translucent zirconia, prepared by milling technology (CAD-CAM) and repeated firing cycles, was the main aim of this in vitro study. MATERIALS AND METHODS. Two groups of samples of two commercial highly-translucent yttria-stabilized dental zirconia, VITA YZ-HTWhite (Group A) and Zolid HT + White (Group B), with dimensions according to the ISO 6872 “Dentistry - Ceramic materials”, were prepared. The specimens of each group were divided into two subgroups. The specimens of the first subgroups (Group A1 and Group B1) were merely the sintered specimens. The specimens of the second subgroups (Group A2 and Group B2) were subjected to 4 heat treatment cycles. The microstructural features (microstructure, density, grain size, crystalline phases, and crystallite size) and four mechanical properties (flexural strength, modulus of elasticity, Vickers hardness, and fracture toughness) of the subgroups (i.e. before and after heat treatment) were compared. The statistical significance between the subgroups (A1/A2, and B1/B2) was evaluated by the t-test. In all tests, P values smaller than 5% were considered statistically significant. RESULTS. A homogenous microstructure, with no residual porosity and grains sized between 500 and 450 nm for group A and B, respectively, was observed. Crystalline yttria-stabilized tetragonal zirconia was exclusively registered in the X-ray diffractograms. The mechanical properties decreased after the heat treatment procedure, but the differences were not statistically significant. CONCLUSION. The produced zirconia ceramic materials can be safely (i.e., according to the ISO 6872) used in extensive fixed prosthetic restorations, such as substructure ceramics for three-unit prostheses involving the molar restoration and substructure ceramics for prostheses involving four or more units. Consequently, milling technology is an effective manufacturing technology for producing zirconia substructures for dental fixed all-ceramic prosthetic restorations.

참고문헌 (41)

  1. Tang Z, "Clinical evaluation of monolithic zirconia crowns for posterior teeth restorations", Medicine(Baltimore), 98, pp.e17385~ (2019)
  2. Barão VA, "Factors to achieve aesthetics in all-ceramic restorations", J Craniofac Surg, 21, pp.2007~2012 (2010)
  3. Sen N, "Microstructural, physical, and optical characterization of high-translucency zirconia ceramics", J Prosthet Dent, 123, pp.761~768 (2020)
  4. Chevalier J, "Low-temperature degradation of zirconia and implications for biomedical implants annual review of materials research", Annu Rev Mater Res, 37, pp.1~2 (2007)
  5. Scott HG, "Phase relationships in the zirconia-yttria system", J Mater Sci, 10, pp.1527~1535 (1975)
  6. Saadaldin SA, "Synthesis of bioactive and machinable miserite glass-ceramics for dental implant applications", Dent Mater, 29, pp.645~655 (2013)
  7. Al-Amleh B, "Clinical trials in zirconia : a systematic review", J Oral Rehabil, 37, pp.641~652 (2010)
  8. Andreiotelli M, "Are ceramic implants a viable alternative to titanium implants? A systematic literature review", Clin Oral Implants Res, 20, pp.32~47 (2009)
  9. Al Jabbari YS, "Microstructural, mechanical, ionic release and tarnish resistance characterization of porcelain fused to metal Co-Cr alloys manufactured via casting and three different CAD-CAM techniques", J Prosthodont Res, 63, pp.150~156 (2019)
  10. Dimitriadis K, "Influence of heat-treatment cycles on the microstructure, mechanical properties, and corrosion resistance of co-cr dental alloys fabricated by selective laser melting", J Mater Eng and Perform, 30, pp.5252~5265 (2021)
  11. Kontonasaki E, "Monolithic zirconia: an update to current knowledge. optical properties, wear, and clinical performance", Dent J(Basel), 7, pp.90~ (2019)
  12. Griffin JD Jr, "Tooth in a bag : same-day monolithic zirconia crown", Dent Today, 32, pp.124~126 (2013)
  13. "ISO 6872. Dentistry - Ceramic materials", International Standards Organization (ISO), ~ (2008)
  14. Montazerian M, "Bioactive and inert dental glass-ceramics", J Biomed Mater Res A, 105, pp.619~639 (2017)
  15. Tong H, "Characterization of three commercial Y-TZP ceramics produced for their high-translucency, high-strength and high-surface area", Ceram Int, 42, pp.1077~1085 (2016)
  16. Dimitriadis K, "Effect of bonding agent on metal-ceramic bond strength between co-cr fabricated with selective laser melting and dental feldspathic porcelain", J Prosthodont, 28, pp.1029~1036 (2019)
  17. Sakar-Deliormanli A, "Microhardness and fracture toughness of dental materials by indentation method", J Biomed Mater Res B Appl Biomater, 76, pp.257~264 (2006)
  18. Žmak I, "Hardness and indentation fracture toughness of slip cast alumina and alumina-zirconia ceramics", Materials(Basel), 13, pp.122~ (2019)
  19. Holand W, "Glass-ceramic technology", pp.57~291 (2002), American Ceramic Society
  20. Stawarczyk B, "The effect of zirconia sintering temperature on flexural strength, grain size, and contrast ratio", Clin Oral Investig, 17, pp.269~274 (2013)
  21. Sakaguchi RL, "Craig's restorative dental materials", pp.253~270 (2012), Elsevier
  22. Amat NF, "Effect of sintering temperature on the aging resistance and mechanical properties of monolithic zirconia", J Mater Res Technol, 8, pp.1092~1101 (2019)
  23. De Souza GM, "Effect of accelerated aging on dental zirconia-based materials", J Mech Behav Biomed Mater, 65, pp.256~263 (2017)
  24. Lucas TJ, "Effect of grain size on the monoclinic transformation, hardness, roughness, and modulus of aged partially stabilized zirconia", Dent Mater, 31, pp.1487~1492 (2015)
  25. Pekkan G, "Comparative radiopacity of conventional and full-contour Y-TZP ceramics", Dent Mater J, 35, pp.257~263 (2016)
  26. El-Meliegy E, "Glasses and glass ceramics for medical applications", pp.109~131 (2012), Springer
  27. Baino F, "Ceramics, glass and glass-ceramics", pp.153~200 (2021), Springer
  28. Denry I, "State of the art of zirconia for dental applications", Dent Mater, 24, pp.299~307 (2008)
  29. Natali AN, "Dental biomechanics", pp.50~250 (2003), CRC Press
  30. Lin PJ, "Biomechanical design application on the effect of different occlusion conditions on dental implants with different positions-a finite element analysis", Appl Sci, 10, pp.5826~ (2020)
  31. Montazerian M, "History and trends of bioactive glass-ceramics", J Biomed Mater Res A, 104, pp.1231~1249 (2016)
  32. Zhang YR, "Review of research on the mechanical properties of the human tooth", Int J Oral Sci, 6, pp.61~69 (2014)
  33. Kinney JH, "The mechanical properties of human dentin : a critical review and re-evaluation of the dental literature", Crit Rev Oral Biol Med, 14, pp.13~29 (2003)
  34. Sakaguchi RL, "Craig's restorative dental materials", pp.69~80 (2018), Elsevier
  35. Mahoney EK, "Mechanical properties and microstructure of hypomineralised enamel of permanent teeth", Biomaterials, 25, pp.5091~5100 (2004)
  36. Solá-Ruíz MF, "Wear in antagonist teeth produced by monolithic zirconia crowns : a systematic review and meta-analysis", J Clin Med, 9, pp.997~ (2020)
  37. Esquivel-Upshaw JF, "Randomized clinical study of wear of enamel antagonists against polished monolithic zirconia crowns", J Dent, 68, pp.19~27 (2018)
  38. Mundhe K, "Clinical study to evaluate the wear of natural enamel antagonist to zirconia and metal ceramic crowns", J Prosthet Dent, 114, pp.358~363 (2015)
  39. Deval P, "A clinical comparative evaluation of the wear of enamel antagonist to monolithic zirconia and metal-ceramic crowns", Int J Prosthodont, 34, pp.744~751 (2021)
  40. Fischer H, "Fracture toughness of dental ceramics : comparison of bending and indentation method", Dent Mater, 18, pp.12~19 (2002)
  41. Dimitriadis K, "Glass-ceramics in the CaO-MgO-Al2O3-SiO2system as potential dental restorative materials", Int J Appl Ceram Technol, 18, pp.1938~1949 (2021)

관련 논문AI추천

Mechanical behavior and microstructural characterization of different zirconia polycrystals in different thicknessesKiara Serafini Dapieve, Laura Viviana Calvache Arcila, Luiz Felipe Valandro, Marco Antonio Bottino, Nathália de Carvalho Ramos, Renata Marques de Melo, Tiago Moreira Bastos Campos대한치과보철학회 · The Journal of Advanced of Prosthodontics2021 · 제13권 제6호An experimental study on hydrothermal degradation of cubiccontaining translucent zirconiaChaimongkon Peampring, Santiphab Kengtanyakich대한치과보철학회 · The Journal of Advanced of Prosthodontics2020 · 제12권 제5호Grain size, crystalline phase and fracture toughness of the monolithic zirconiaChuchai Anunmana, Kodchakorn Bocam, Trinuch Eiampongpaiboon대한치과보철학회 · The Journal of Advanced of Prosthodontics2022 · 제14권 제5호The effects of repetitive firing processes on the optical, thermal, and phase formation changes of zirconiaAlper Ozdogan, Hatice Ozdemir대한치과보철학회 · The Journal of Advanced of Prosthodontics2020 · 제12권 제1호Influence of heating rate on the flexural strength of monolithic zirconiaCaner Ozturk, Ersan Celik대한치과보철학회 · The Journal of Advanced of Prosthodontics2019 · 제11권 제4호Mechanical properties and microstructure of mullite modified zirconia ceramic for dental applicationsFuqiang Zhang, Jing Li, Limin Gao, Ying Li청정에너지연구소 · Journal of Ceramic Processing Research2011 · 제12권 제6호

이 간행물의 다른 논문 (6건)