초록
It is essential to select materials with excellent mechanical properties to prevent chemical and mechanical damage to the surfaces of materials used in machines and structures and to extend their lifespan. Co-based stellite alloy, which has wear resistance, heat resistance, and corrosion resistance, is essential for products used in harsh environments. However, due to the problem of enormous costs, research on hard facing, which uses a stellite coating layer only on the contact surface, is urgently required. Currently, high-facing research on Stellite coating layers is focused on powder, and GMAW research using wire is relatively lacking. In this study, welding experiments were performed to form stable weld beads using stellite 6 welding wire, and the correlation between parameters and weld beads was analyzed. A CMT welder was used to minimize the heat effect on the base material.
Abstract
It is essential to select materials with excellent mechanical properties to prevent chemical and mechanical damage to the surfaces of materials used in machines and structures and to extend their lifespan. Co-based stellite alloy, which has wear resistance, heat resistance, and corrosion resistance, is essential for products used in harsh environments. However, due to the problem of enormous costs, research on hard facing, which uses a stellite coating layer only on the contact surface, is urgently required. Currently, high-facing research on Stellite coating layers is focused on powder, and GMAW research using wire is relatively lacking. In this study, welding experiments were performed to form stable weld beads using stellite 6 welding wire, and the correlation between parameters and weld beads was analyzed. A CMT welder was used to minimize the heat effect on the base material.
참고문헌 (11)
- S. Houdkova, "Microstructure and Sliding Wear Properties of HVOF Sprayed, Laser Remelted and Laser Clad Stellite 6 Coatings", Surf. Coat. Technol, 318(25), pp.129~141 (2017)
- M. Kiehl, "Coaxial Laser Cladding of Cobalt-Base Alloy Stellite 6 on Grey Cast Iron Analysis of the Microstructural and Mechanical Properties Depending on the Laser Power", JMEPEG, 32, pp.3821~3838 (2023)
- 박나라, "Wear Characteristics of Stellite6 and NOREM02 Hardfaced SKD61 Hot Working Tool Steel at the Elevated Temperature", International Journal of Precision Engineering and Manufacturing, 15(12), pp.2549~2558 (2014), 한국정밀공학회
- 정경호, "PTA법에 의한 스텔라이트 12합금 육성층의 미세조직 및 경도에 미치는 시효처리의 영향", 한국마린엔지니어링학회지, 26(1), pp.68~75 (2002), 한국마린엔지니어링학회
- Mousavi B., "Slurry Erosion Characteristics of Stellite 6 on AISI 316 and AISI 410 Stainless Steels", 대한용접접합학회지, 38(6), pp.584~592 (2020), 대한용접접합학회[DOI]
- 이호진, "전자빔을 이용한 Stellite21 분말 예열공정에 관한 기초 연구", 한국정밀공학회지, 33(5), pp.419~425 (2016), 한국정밀공학회
- U. D. Oliveira, "Residual stress analysis in Co-based laser clad layers by laboratory X-rays and synchrotron diffraction techniques", Surface & Coatings Technology, 201, pp.533~542 (2006)
- J. S. Oh, "Effect of Post-heat Treatment on Fatigue Strength of Thermally-Sprayed Stellite Alloy on Steel", Journal of Korean Powder Metallurgy Institute, 12(2), pp.106~111 (2005)
- 신종철, "몰리브덴을 첨가하여 PTAW법으로 육성된 Stellite 6 합금의 미세조직 특성평가", 한국표면공학회지, 35(4), pp.241~248 (2002), 한국표면공학회
- Y. Z. Zhu, "Plasma cladding of Stellite 6 powder on Ni76Crl9AlTi exhausting valve", Transactions of Nonferrous Metals Society of China, 17, pp.35~40 (2007)
- 이충우, "CMT 공정조건에 따른 용접부 특성 분석", 한국기계기술학회지, 25(1), pp.11~16 (2023), 한국기계기술학회[DOI]