Statistical analysis of Vickers hardness and fracture toughness of repeated crack-healing SiC composite ceramics considering economics

2

조회

0

다운로드

3

인용

0

참고문헌

키워드

주제분류재료공학

초록

This study was carried out to evaluate the repeated crack-healing properties of SiC composite ceramics and to investigate and analyze the Vickers hardness and fracture toughness. SiC composite ceramics were able to heal repeated cracks, but this crackhealing was only suitable up to two times. The oxygen of the three-times crack-healed specimens increased 1158% over that of the as-received specimen. The surface oxide was found to be SiO2, Y2Si2O7, and Al5Y3O12. The Vickers hardness and fracture toughness decreased as the number of crack-healings increased, and the dispersion was increased as well. The Vickers hardness and fracture toughness were analyzed using the two-parameter Weibull statistics. It was concluded that the Weibull distribution can properly describe the Vickers hardness and the fracture toughness of SiC composite ceramics. Ceramic structures that can be repeatedly crack-healed can save costs due to reduced manufacturing costs, replacement costs, shutdowns, etc., which will ensure enormous economic efficiency.

Abstract

This study was carried out to evaluate the repeated crack-healing properties of SiC composite ceramics and to investigate and analyze the Vickers hardness and fracture toughness. SiC composite ceramics were able to heal repeated cracks, but this crackhealing was only suitable up to two times. The oxygen of the three-times crack-healed specimens increased 1158% over that of the as-received specimen. The surface oxide was found to be SiO2, Y2Si2O7, and Al5Y3O12. The Vickers hardness and fracture toughness decreased as the number of crack-healings increased, and the dispersion was increased as well. The Vickers hardness and fracture toughness were analyzed using the two-parameter Weibull statistics. It was concluded that the Weibull distribution can properly describe the Vickers hardness and the fracture toughness of SiC composite ceramics. Ceramic structures that can be repeatedly crack-healed can save costs due to reduced manufacturing costs, replacement costs, shutdowns, etc., which will ensure enormous economic efficiency.

참고문헌 (48)

  1. Nitin P. Padture, , Nature Materials, 15, pp.804~809 (2016)
  2. Steven J. Zinkle, , Fusion Engineering and Design, 74, pp.31~40 (2005)
  3. M. Singh, , Journal of Materials Science Letters, 17, pp.459~461 (1998)
  4. L. L. Snead, , Journal of Nuclear Materials, 417, pp.330~339 (2011)
  5. K. W. Nam, , Journal of Nuclear Materials, 417, pp.353~355 (2011)
  6. Y. Korous, , J. Am. Ceram. Soc, 83, pp.2788~2792 (2000)
  7. Y. W. Kim, , J. Am. Ceram. Soc, 86, pp.465~470 (2003)
  8. K. W Nam, , Materials Science and Engineering: A, 527, pp.3236~3239 (2010)
  9. K. W Nam, , Materials Science and Engineering : A, 527, pp.5400~5404 (2010)
  10. K. W Nam, , Materials Science and Engineering : A, 471, pp.102~105 (2007)
  11. K. Ando, , J. Eur. Ceram. Soc, 22, pp.1339~1346 (2002)
  12. K. Ando, , J. Am. Ceram. Soc, 85, pp.2268~2272 (2002)
  13. K. Ando, , J. Eur. Ceram. Soc, 23, pp.997~984 (2003)
  14. K. Ando, , Fatigue & Fract Eng Mat, 21, pp.119~122 (2002)
  15. K. Takahashi, , J. Am, Ceram, Soc, 88, pp.645~651 (2005)
  16. K. Takahashi, , Materials Science and Engineering A, 527, pp.3343~3348 (2010)
  17. H. S. Kim, , Materials Science and Engineering A, 483-484, pp.672~675 (2008)
  18. 남기우, "Crack-healing behavior and bending strength of Al2O3", SiC composite ceramics according to the amount of added Y2O3, 2010, pp.11(4), 471~474[DOI]
  19. T. Osada, , Journal of the European Ceramic Society, 27, pp.3261~3267 (2007)
  20. C. Zdenek, , Journal of the European Ceramic Society, 28, pp.1073~1077 (2008)
  21. S. K. Lee, , J. Euro. Ceram. Soc, 25, pp.3495~3502 (2005)
  22. W. Nakao, , J. Am. Ceram. Soc, 89, pp.1352~1357 (2006)
  23. K. Ando, , J. Euro. Ceram. Soc, 25, pp.549~558 (2005)
  24. K. Takahashi, , J. Am. Ceram. Soc, 86, pp.2143~2147 (2003)
  25. W. Nakao, , J. Euro. Ceram. Soc, 25, pp.3649~3655 (2005)
  26. W. Nakao, , J. Am. Ceram. Soc, 89, pp.1352~1357 (2006)
  27. F. F. Lange, , J. Am. Ceram. Soc, 53, pp.290~ (1970)
  28. T. E. Easler, , J. Am. Ceram. Soc, 64, pp.731~734 (1981)
  29. N. S. Jacobson, , J. Am. Ceram. Soc, 75, pp.1603~1611 (1992)
  30. 안석환, "Weibull statistical analysis on mechanical properties of immersed silicon carbide in acidic and alkaline solution", Journal of Ceramic Processing Research, 17(9), pp.994~998 (2016), 청정에너지연구소[DOI]
  31. Sang-Cheol Jeong, "Weibull statistical analysis on Vickers hardness of immersed Al2O3 ceramics in acidic and alkaline solution", Journal of Ceramic Processing Research, 18(7), pp.506~520 (2017), 청정에너지연구소[DOI]
  32. Seok-Hwan Ahn, "Temperature-dependent characteristics of weibull statistical analysis for vickers hardness of corroded Al2O3 ceramics", Journal of Ceramic Processing Research, 18(9), pp.646~658 (2017), 청정에너지연구소[DOI]
  33. G. R. Anstis, , J. Am. Ceram. Soc, 64, pp.533~538 (1981)
  34. A. Nastic, , J. Mater. Sci. Technol, 31, pp.773~783 (2015)
  35. P. Chantikul, , J. Am. Ceram. Soc, 64, pp.539~543 (1981)
  36. K. Strecker, , Mat. Res, 8, pp.121~124 (2005)
  37. G. D. Quinn, "Fracture toughness of ceramics by the Vickers indentation crack length method", Ceram. Eng. Sci. Proc., pp.45~62 (2007), John Wiley & Sons, Inc.
  38. D. Casellas, , J. Am. Ceram. Soc, 88, pp.1958~1963 (2005)
  39. Du Yongsheng, "Effect of heat treatment on the crystallization toughening of tailing-derived glass-ceramics", Journal of Ceramic Processing Research, 17(12), pp.1243~1248 (2016), 청정에너지연구소[DOI]
  40. M. C. Corrêa de Sá e Benevides de Moraes, , Mat. Res, 7, pp.643~649 (2004)
  41. K. Niihara, , J. Mat. Sci. Letters, 1, pp.13~16 (1982)
  42. A. Saghafi, , Theor. Appl. Fract. Mech, 52, pp.2~180 (2009)
  43. R. Langlois, , J. Mater. Sci. Letters, 10, pp.1049~1051 (1991)
  44. D. Wu, , J. Mater. Sci, 22, pp.1745~1746 (2003)
  45. J. Gong, , J. Mater. Sci. Letters, 16, pp.875~876 (1997)
  46. 남기우, "Effect of a colloidal SiO2 coating to crack healing and the bending strength of Si3N4 ceramics", Journal of Ceramic Processing Research, 11(1), pp.20~24 (2010), 청정에너지연구소[DOI]
  47. M. K. Kim, , Solid State Phenomena, 124-126, pp.719~722 (2007)
  48. K. W. Nam, , Materials Science and Engineering A, 527, pp.5400~5404 (2010)

관련 논문AI추천

이 간행물의 다른 논문 (25건)