Hardness is a characteristic value that indicates resistance to partial deformation or abrasion of the material surface. It is easyto measure, and data can quickly be obtained. It also shows correlation with mechanical properties, such as tensile strength. Al2O3/SiC composite with three concentrations of silicon carbide was sintered, and heat-treated at three differenttemperatures. The Vickers hardness of the as-received specimen and the heat-treatment specimen was analyzed by Weibullstatistics, and its probability distribution characteristics were evaluated. Since an oxide layer was formed on the surface bythe heat-treatment, the hardness of the specimen having high temperature heat-treatment was low. The shape parameter andthe mean Vickers hardness decreased as the heat-treatment temperature increased, and the scale parameters showed smallerthan those of the as-received specimen. The scale parameters of the 1,473 K specimen were larger than those of the as-receivedspecimen, but those of the (1,573 and the 1,673) K specimens were smaller than those of the as-received specimen. The entireshape parameters, except for the 1,673 K specimen of AS15Y3, were smaller than those of the as-received specimen, and thedispersions were large.
Abstract
Hardness is a characteristic value that indicates resistance to partial deformation or abrasion of the material surface. It is easyto measure, and data can quickly be obtained. It also shows correlation with mechanical properties, such as tensile strength. Al2O3/SiC composite with three concentrations of silicon carbide was sintered, and heat-treated at three differenttemperatures. The Vickers hardness of the as-received specimen and the heat-treatment specimen was analyzed by Weibullstatistics, and its probability distribution characteristics were evaluated. Since an oxide layer was formed on the surface bythe heat-treatment, the hardness of the specimen having high temperature heat-treatment was low. The shape parameter andthe mean Vickers hardness decreased as the heat-treatment temperature increased, and the scale parameters showed smallerthan those of the as-received specimen. The scale parameters of the 1,473 K specimen were larger than those of the as-receivedspecimen, but those of the (1,573 and the 1,673) K specimens were smaller than those of the as-received specimen. The entireshape parameters, except for the 1,673 K specimen of AS15Y3, were smaller than those of the as-received specimen, and thedispersions were large.
참고문헌 (29)
- F.F. Lange, , J. Am. Ceram. Soc., 53, pp.420~421 (1970)[DOI]
- T.K. Gupta, , J. Am. Ceram. Soc., 59, pp.259~262 (1976)[DOI]
- J. Zhao, , J. Am. Ceram. Soc., 76, pp.503~510 (1993)[DOI]
- A.M. Thompson, , J. Am. Ceram. Soc., 78, pp.567~571 (1995)[DOI]
- J.E. Moffatt, , Br. Ceram. Trans., 95, pp.23~29 (1996)
- I.A. Chou, , J. Am. Ceram. Soc., 81, pp.1203~1208 (1998)
- 남기우, "Y2O3 첨가량에 의한 Al2O3 복합재 세라믹스의 균열 균열 치유와 고온 굽힘강도 특성", 대한기계학회논문집 A, 31(11), pp.1108~1114 (2007), 대한기계학회
- H.S. Kim, , Mater. Sci. Eng. A, 483-484, pp.672~675 (2008)[DOI]
- F.F. Lange, , J. Am. Ceram. Soc., 53, pp.290~ (1970)[DOI]
- S.K. Lee, , J. Euro. Ceram. Soc., 2005, pp.569~576 (2005)
- K.W. Nam, , Mater. Sci. Eng. A, 527, pp.3236~3239 (2010)[DOI]
- K. Niihara, , J. Am. Ceram. Soc., 99, pp.974~982 (1991)[DOI]
- 박승원, "소결보조재 Al2O3 및 Y2O3 종류에 따른 사이알론 세라믹스의 특성", 동력시스템공학회지, 12(3), pp.50~54 (2008), 한국동력기계공학회
- 남기우, "고강도 사이알론의 균열치유와 고온강도 특성", 대한기계학회논문집 A, 33(09), pp.957~962 (2009), 대한기계학회
- Y.Z. Zhang, , J. Am. Ceram. Soc., 1998, pp.1861~1868 (1998)
- K. Ando, , Fatigue Fract. Engng. Mater. Struct., 21, pp.119~122 (1998)
- K. Houjou, , J. Euro. Ceram. Soc., 24, pp.2329~2338 (2004)[DOI]
- 남기우, "Effect of a colloidal SiO2 coating to crack healing and the bending strength of Si3N4 ceramics", Journal of Ceramic Processing Research, 11(1), pp.20~24 (2010), 청정에너지연구소[DOI]
- Ki Woo Nam, "Wear characteristics of Si3N4", SiC composite ceramics with added SiO2 colloid, 2012, pp.13(5), 571~574[DOI]
- K. Houjou, , J. Soc. Mater. Sci. (Jap.), 58, pp.510~515 (2009)[DOI]
- K. Houjou, , Inter. J. Struct. Intergrity, 3, pp.41~52 (2012)[DOI]
- 문창권, "SiCf", SiC 복합재의 마모 및 마찰에 의해 발생된 탄성파 특성, 2014, pp.34(1), 23~30[DOI]
- 김선진, "와이블 통계 해석에 의한 ZrO2 복합 세라믹스의 기계적 특성", 대한기계학회논문집 A, 39(10), pp.955~962 (2015), 대한기계학회
- 안석환, "Rolling contact fatigue strength of shot peened zirconia composites", Journal of Ceramic Processing Research, 17(4), pp.365~368 (2016), 청정에너지연구소[DOI]
- 정상철, "Weibull statistical analysis on Vickers hardness of corroded ZrO2 composites ceramics", Journal of Ceramic Processing Research, 17(10), pp.1088~1094 (2016), 청정에너지연구소[DOI]
- Seok-Hwan Ahn, "Weibull distribution for Vickers hardness of peened ZrO2 ceramics according to shot sizes", Journal of Ceramic Processing Research, 18(6), pp.425~430 (2017), 청정에너지연구소[DOI]
- M. Nakatani, , J. Euro. Ceram. Soc., 28, pp.1251~1257 (2008)[DOI]
- K. Takahashi, , J. Euro. Ceram. Soc., 25, pp.1953~1959 (2005)[DOI]
- K. Houjou, , J. Euro. Ceram. Soc., 25, pp.559~567 (2005)[DOI]