열화한 STS316L에 대한 Cr-free 코팅액의 내식특성

Corrosion Resistance Characteristics of Cr-free Coating Solution for Degraded STS316L

0

조회

0

다운로드

5

인용

0

참고문헌

키워드

주제분류해양공학

초록

In this study, we developed a Cr-free organic/inorganic hybrid solution and investigated its coating properties on degraded STS316L. Both the OIBD-1 solution and OIBD-2 solution had excellent corrosion resistance and adhesion ability. However, the solution had some problems in a boiling water environment. In addition, the flexibility was excellent, and the scratch resistance was relatively good.

Abstract

In this study, we developed a Cr-free organic/inorganic hybrid solution and investigated its coating properties on degraded STS316L. Both the OIBD-1 solution and OIBD-2 solution had excellent corrosion resistance and adhesion ability. However, the solution had some problems in a boiling water environment. In addition, the flexibility was excellent, and the scratch resistance was relatively good.

참고문헌 (16)

  1. Atanda1, P., "Sensitization Study of Normalized 316L Stainless Steel", Journal of Minerals & Materials Characterization & Engineering, 9(1), pp.13~23 (2010)
  2. ASTM, "Standard Test Methods for Measuring Adhesion by Tape Test", ASTM D3359-09, 1~8 (2009)
  3. Clarke, W. L., "Comparative Methods for Measuring Degree of Sensitization in Stainless Steel", ASTM STP, 656, pp.99~132 (1978)
  4. Kim, B. T., "A Study on Evaluation of Degree of Sensitization in AISI 304 Stainless Steel and Its Welding Heat Affected Zone", Journal of Corrosion Science Society of Korea, 17(2), pp.99~109 (1998)
  5. Kim, H. P., "A Review of Sensitization of Stainless Steel", Journal of Corrosion Science Society of Korea, 27(1), pp.52~64 (1998)
  6. Kim, J. R., "Corrosion Resistance of Cold Rolled Carbon Steel by Treating Organic", Inorganic Hybrid Coating Solution, 2012, pp.36(4), 405~412
  7. Lee, H. G., "The Effect of Sensitization on Corrosion Behavior of AISI 316 Stainless Steel", Journal of Corrosion Science Society of Korea, 19(2), pp.87~95 (1990)
  8. Lim, U. J., "Effect of Sensitization on the Corrosion Characteristics of STS 304 Pipe", Corrosion and Protection, 6(1), pp.9~13 (2007)
  9. Nam, K. W., "Tribology of Si3N4 Ceramics according to an Amount of Additive SiO2 Nano Colloid", Transactions of the Korean Society of Mechanical Engineers A, 35(3), pp.267~272 (2011)
  10. 남기우, "유", 무기 하이브리드 코팅액에 의한 냉간압연강판의 열처리 온도에 따른 내식특성, 2011, pp.25(6), 56~59[DOI]
  11. 남기우, "크롬 프리 친환경 유", 무기 하이브리드 코팅액에 의한 냉연강판의 내식특성, 2013, pp.27(2), 33~38[DOI]
  12. Rashid, M. W. A., "Formation of Cr23C6 during the Sensitization of AISI 304Stainless Steel and its Effect to Pitting Corrosion", International Journal of Electrochemical Science, 7, pp.9465~9477 (2012)
  13. 서현수, "Cr-free 코팅액에 의한 아연도금강판의 열처리 온도에 따른 내식특성", 한국해양공학회지, 24(5), pp.60~66 (2010), 한국해양공학회
  14. 서현수, "Cr-free 코팅액에 의한 아연도금강판의 건조시간에 따른 내식특성", 한국해양공학회지, 24(5), pp.67~74 (2010), 한국해양공학회
  15. 서현수, "Si 변성 유", 무기 하이브리드 코팅액에 의한 아연도금강판의 내식특성, 2011, pp.25(1), 32~38[DOI]
  16. Tsai, N. S., "The Size of the Sensitization Zone in 304 Stainless Steel Welds", Journal of Materials for Energy Systems, 6(1), pp.33~37 (1984)

관련 논문AI추천

이 간행물의 다른 논문 (11건)