Effects of Electrolyte Concentration and Relative Cathode Electrode Area Sizes in Titania Film Formation by Micro-Arc Oxidation
1
조회
0
다운로드
0
인용
0
참고문헌
키워드
초록
MAO (micro-arc oxidation) is an eco-friendly convenient and effective technology to deposit high-quality oxide coatings on the surfaces of Ti, Al, Mg and their alloys. The roles of the electrolyte concentration and relative cathode electrode area sizes in the grown oxide film during titanium MAO were investigated. The higher the concentration of the electrolyte, the lower the RtotalA value. The oxide film produced by the lower concentration of the electrolyte is thinner and less uniform than the film by the higher concentration,which is thick and porous. The cathode area size must be bigger than the anode area size in order to minimize the voltage drop across the cathode. The ratio of the cathode area size to the anode area size must be bigger than 8. Otherwise, the cathode will be another source for voltage drop, which is detrimental to and slows down the oxide growth.
Abstract
MAO (micro-arc oxidation) is an eco-friendly convenient and effective technology to deposit high-quality oxide coatings on the surfaces of Ti, Al, Mg and their alloys. The roles of the electrolyte concentration and relative cathode electrode area sizes in the grown oxide film during titanium MAO were investigated. The higher the concentration of the electrolyte, the lower the RtotalA value. The oxide film produced by the lower concentration of the electrolyte is thinner and less uniform than the film by the higher concentration,which is thick and porous. The cathode area size must be bigger than the anode area size in order to minimize the voltage drop across the cathode. The ratio of the cathode area size to the anode area size must be bigger than 8. Otherwise, the cathode will be another source for voltage drop, which is detrimental to and slows down the oxide growth.
참고문헌 (17)
- A. Aladjem, , J. Mater. Sci., 8, pp.688~ (1973)
- J. Pouilleau, , Mater. Sci. Eng. B, 47, pp.235~ (1997)
- P. Kurze, , Cryst. Res. Technol., 21, pp.1603~ (1986)
- S. D. Brown, , Mater. Sci. Monogr. High Perf. Ceram. Films Coat., 67, pp.221~ (1991)
- A. L. Yerokhin, , Surf. Coat. Technol., 122, pp.73~ (1999)
- S. D. Brown, , J. Am. Ceram. Soc., 54, pp.384~ (1971)
- T. Haneda, , Zairyo Gijutsu, 11, pp.274~ (1993)
- V. S. Rudnev, , J. Electroanal. Chem., 497, pp.150~ (2001)
- X. Y. Liu, , Mater. Sci. Eng. R, 47, pp.49~ (2004)
- Y. M. Wang, , Mater. Chem. Phys., 90, pp.128~ (2005)
- L. H. Li, , Biomaterials, 25, pp.2867~ (2004)
- X. L. Zhu, , Biomaterials, 22, pp.2199~ (2001)
- X. L. Zhu, , J. Biomed. Mater. Res., 60, pp.333~ (2002)
- W. H. Song, , Biomaterials, 25, pp.3341~ (2004)
- G. Sundarajan, , Surf. Coat. Technol., 167, pp.269~ (2003)
- W. Xue, , Thin Solid Films, 372, pp.114~ (2000)
- 박경진, "Effect of Electrolyte Composition on Corrosion Behavior of PEO Treated AZ91 Mg Alloy", CORROSION SCIENCE AND TECHNOLOGY, 8(6), pp.228~232 (2009), 한국부식방식학회