Materials of choice for offshore structures and the marine industry have been increasingly favoring materials that offer high strength-to-weight ratios. One of the most promising families of light-weight materials is titanium alloys, but these do have two potential Achilles’ heels: (i) the passive film may not form or may be unstable in low oxygen environments, leading to rapid corrosion; and (ii) titanium is a strong hydride former, making it vulnerable to hydrogen embrittlement (cracking) at high temperatures in low oxygen environments. Unfortunately, such environments exist at deep sea well-heads; temperatures can exceed 120 °C, and oxygen levels can drop below 1 ppm. The present study demonstrates the results of investigations into the corrosion behavior of a range of titanium alloys, including newly developed alloys containing rare earth additions for refined microstructure and added strength, in artificial seawater over the temperature range of 25 °C to 200 °C. Tests include potentiodynamic polarization, crevice corrosion, and U-bend stress corrosion cracking.
Abstract
Materials of choice for offshore structures and the marine industry have been increasingly favoring materials that offer high strength-to-weight ratios. One of the most promising families of light-weight materials is titanium alloys, but these do have two potential Achilles’ heels: (i) the passive film may not form or may be unstable in low oxygen environments, leading to rapid corrosion; and (ii) titanium is a strong hydride former, making it vulnerable to hydrogen embrittlement (cracking) at high temperatures in low oxygen environments. Unfortunately, such environments exist at deep sea well-heads; temperatures can exceed 120 °C, and oxygen levels can drop below 1 ppm. The present study demonstrates the results of investigations into the corrosion behavior of a range of titanium alloys, including newly developed alloys containing rare earth additions for refined microstructure and added strength, in artificial seawater over the temperature range of 25 °C to 200 °C. Tests include potentiodynamic polarization, crevice corrosion, and U-bend stress corrosion cracking.
참고문헌 (14)
- D. J. Blackwood, , Electrochim. Acta, 34, pp.875~ (1989)
- D. J. Blackwood, , Electrochim. Acta, 33, pp.1143~ (1988)
- D. J. Blackwood, , Electrocim. Acta, 34, pp.1401~ (1989)
- L. M. Young, , Metall. Mater. Trans. A, 26, pp.1257~ (1995)
- A. M. Alvarez, , Acta Mater, 52, pp.4161~ (2004)
- D. G. Kolman, , Corros. Sci, 42, pp.1863~ (2000)
- N. Rajendran, , Mater. Corros, 58, pp.334~ (2007)
- D. J. Blackwood, , Electrochim. Acta, 46, pp.563~ (2000)
- D. W. Shoesmith, "Shreir's Corrosion", pp.2042~ (2009), Elsevier Science
- Y. Li, "Private communication" (2014), National University of Singapore
- J. S. Lee, , J. Electrochem. Soc, 151, pp.B423~ (2004)
- M. I. Abdulsalam, , Corros. Sci, 47, pp.1336~ (2005)
- B. P. Cai, , Corros. Sci, 52, pp.3235~ (2010)
- B. Balakrisnan, , M. Eng, pp.1998