Additively manufactured (AM) Ti-6Al-4V alloys exhibit a dominant acicular martensite phase (α\'), which is characterized by an unstable energy state and highly localized corrosion susceptibility. Electrochemical critical localized corrosion temperature (E-CLCT, ISO 22910: 2020) and electrochemical critical localized corrosion potential (E-CLCP, ISO AWI 4631: 2021) were measured to analyze the localized corrosion resistance of the AM Ti-6Al-4V alloy. Although E-CLCP was measured under mild corrosive conditions such as human body, the validity of evaluating localized corrosion resistance of AM titanium alloys was demonstrated by comparison with E-CLCT. However, the mechanisms of resistance to localized corrosion on the as-received and heat-treated AM Ti-6Al-4V alloys under E-CLCT and E-CLCP differ at various temperatures because of differences in properties under localized corrosion and repassivation. The E-CLCT is mainly measured for initiation of localized corrosion on the AM titanium alloys based on temperature, whereas the E-CLCP yields repassivation potential of re-generated passive films of AM titanium alloys after breaking down.

Abstract

Additively manufactured (AM) Ti-6Al-4V alloys exhibit a dominant acicular martensite phase (α\'), which is characterized by an unstable energy state and highly localized corrosion susceptibility. Electrochemical critical localized corrosion temperature (E-CLCT, ISO 22910: 2020) and electrochemical critical localized corrosion potential (E-CLCP, ISO AWI 4631: 2021) were measured to analyze the localized corrosion resistance of the AM Ti-6Al-4V alloy. Although E-CLCP was measured under mild corrosive conditions such as human body, the validity of evaluating localized corrosion resistance of AM titanium alloys was demonstrated by comparison with E-CLCT. However, the mechanisms of resistance to localized corrosion on the as-received and heat-treated AM Ti-6Al-4V alloys under E-CLCT and E-CLCP differ at various temperatures because of differences in properties under localized corrosion and repassivation. The E-CLCT is mainly measured for initiation of localized corrosion on the AM titanium alloys based on temperature, whereas the E-CLCP yields repassivation potential of re-generated passive films of AM titanium alloys after breaking down.

참고문헌 (19)

  1. F. H. Froes, , Adv. Mater. Res., 1019, pp.19~ (2014)[DOI]
  2. Timothy J. Horn, "Overview of Current Additive Manufacturing Technologies and Selected Applications", Science Progress, 95(3), pp.255~282 (2012), SAGE Publications[DOI]
  3. Nianwei Dai, "Distinction in corrosion resistance of selective laser melted Ti-6Al-4V alloy on different planes", Corrosion Science, 111, pp.703~710 (2016), Elsevier BV[DOI]
  4. 서동일, "마이크로 드로플릿 셀 기법과 임계공식온도 측정 기법을 이용한 적층가공 Ti-6Al-4V 합금의 내식성 평가", CORROSION SCIENCE AND TECHNOLOGY, 17(3), pp.129~137 (2018), 한국부식방식학회[DOI]
  5. 이재봉, "NaCl과 NaBr수용액에서 적층가공으로 제조된 Ti-6Al-4V 합금의 공식 저항성 비교", CORROSION SCIENCE AND TECHNOLOGY, 18(3), pp.110~116 (2019), 한국부식방식학회[DOI]
  6. Dong-Il Seo, "Corrosion Characteristics of Additive-Manufactured Ti-6Al-4V Using Microdroplet Cell and Critical Pitting Temperature Techniques", Journal of The Electrochemical Society, 166(13), pp.C428~C433 (2019), The Electrochemical Society[DOI]
  7. Dong-Il Seo, "Effects of competitive anion adsorption (Br− or Cl−) and semiconducting properties of the passive films on the corrosion behavior of the additively manufactured Ti–6Al–4V alloys", Corrosion Science, 173, pp.108789~ (2020), Elsevier BV[DOI]
  8. Mohammed I. Abdulsalam, "Crevice Corrosion of Titanium in High Temperature-Concentrated Chloride Environments", Journal of Materials Engineering and Performance, 16(6), pp.736~740 (2007), Springer Science and Business Media LLC[DOI]
  9. "Corrosion of metals and alloys —Determination of the critical crevice temperature (CCT)for stainless steels under potentiostatic control", ISO, 2015
  10. Jae‑Bong Lee, "Evaluating Corrosion Resistance of Additive-Manufactured Ti–6Al–4V Using Electrochemical Critical Localized Corrosion Temperature", Metals and Materials International, 26(1), pp.39~45 (2020), 대한금속·재료학회[DOI]
  11. "ISO/22910: 2020, Corrosion of metals and alloys —measurement of the electrochemical critical localized corrosion temperature (E-CLCT) for Ti alloys fabricated via the additive manufacturing method" (2020)[URL]
  12. "ISO/17475 : 2005, Electrochemical test methods —Guidelines for conducting potentiostatic and potentiodynamic polarization measurements" (2005)[URL]
  13. "ASTM G192, Standard Test Method for Determining the Crevice Repassivation Potential of Corrosion-Resistant Alloys Using a Potentiodynamic-Galvanostatic-Potentiostatic Technique" (2014)[URL]
  14. "Corrosion of metals and alloys — Measurement of the Electrochemical Critical Localized Corrosion Potential (E-CLCP) for Biomedical Ti Alloys Fabricated via Additive Manufacturing Method", ISO AWI 4631, ~ (2021)
  15. J.-B. Lee, , Met. Mater. Inter. (2021)
  16. D. -I. Seo, , J. Electrochem. Soc, 167, pp.101509~ (2020)[DOI]
  17. Chee Meng Benjamin Ho, "A Review on 3D Printed Bioimplants", International Journal of Precision Engineering and Manufacturing, 16(5), pp.1035~1046 (2015), 한국정밀공학회
  18. F.X. Gil Mur, "Influence of tempering temperature and time on the α′-Ti-6Al-4V martensite", Journal of Alloys and Compounds, 234(2), pp.287~289 (1996), Elsevier BV[DOI]
  19. Nianwei Dai, "Corrosion behavior of selective laser melted Ti-6Al-4 V alloy in NaCl solution", Corrosion Science, 102, pp.484~489 (2016), Elsevier BV[DOI]