화력발전소용 슈퍼 듀플렉스 스테인리스 강(STS 329J4L) 조관 튜브및 핀-튜브재의 부식거동

Corrosion Behavior of Super Duplex Stainless Steel (STS 329J4L) Tubes and Fin-Tubes Used in Thermal Power Plant Applications

1

조회

0

다운로드

1

인용

0

참고문헌

키워드

주제분류금속공학

초록

Corrosion behaviors of laser-welded super duplex stainless steel (SDSS) tubes after exposure to an actual power plant environment for one year and those of fin-tube welded SDSS were evaluated. Results showed that corrosion damage on the back side of the SDSS tube in the direction of hot air was higher than that on the front side regardless of weldment location. However, corrosion damage showed no difference between weldment and base metal due to recovery of phase fraction in the weldment through post weld heat treatment (PWHT). Nevertheless, the SDSS tube showed severe corrosion damage along grain boundary due tosurface phase transformation (δ → γ) and Cr 2 N precipitation caused by PWHT with a high N 2 atmosphere. Corrosion resistance of the SDSS tube was recovered when degraded surface was removed. Corrosion sensitivity of a fin-tube increased significantly due to pre-existing crevice, unbalanced phase fraction, and σ phase precipitation adjacent to the fusion line. Although corrosion resistance was improved by recovered phase fraction and sufficient dissolution of σ phase during PWHT, corrosion reaction was concentrated at the pre-existing crevice. These results suggest that welding conditions for fin-tube steel should be optimized to improve corrosion resistance by removing pre-existing crevice in the weldment.

Abstract

Corrosion behaviors of laser-welded super duplex stainless steel (SDSS) tubes after exposure to an actual power plant environment for one year and those of fin-tube welded SDSS were evaluated. Results showed that corrosion damage on the back side of the SDSS tube in the direction of hot air was higher than that on the front side regardless of weldment location. However, corrosion damage showed no difference between weldment and base metal due to recovery of phase fraction in the weldment through post weld heat treatment (PWHT). Nevertheless, the SDSS tube showed severe corrosion damage along grain boundary due tosurface phase transformation (δ → γ) and Cr 2 N precipitation caused by PWHT with a high N 2 atmosphere. Corrosion resistance of the SDSS tube was recovered when degraded surface was removed. Corrosion sensitivity of a fin-tube increased significantly due to pre-existing crevice, unbalanced phase fraction, and σ phase precipitation adjacent to the fusion line. Although corrosion resistance was improved by recovered phase fraction and sufficient dissolution of σ phase during PWHT, corrosion reaction was concentrated at the pre-existing crevice. These results suggest that welding conditions for fin-tube steel should be optimized to improve corrosion resistance by removing pre-existing crevice in the weldment.

참고문헌 (33)

  1. J.-O. Nilsson, "Super duplex stainless steels", Materials Science and Technology, 8(8), pp.685~700 (1992), SAGE Publications[DOI]
  2. Wu Min, "Temperature dependence of precipitation mechanism of intragranular χ phase in super duplex stainless steel S32750", Materials Letters, 287, pp.129304~ (2021), Elsevier BV[DOI]
  3. Chenzhi Li, "Effect of flue gas desulfurization gypsum addition on critical chloride content for rebar corrosion in fly ash concrete", Construction and Building Materials, 286, pp.122963~ (2021), Elsevier BV[DOI]
  4. Liqiang Qi, "Removal of Chlorine Ions from Desulfurization Wastewater by Modified Fly Ash Hydrotalcite", ACS Omega, 5(49), pp.31665~31672 (2020), American Chemical Society (ACS)[DOI]
  5. R.A Perren, "Corrosion resistance of super duplex stainless steels in chloride ion containing environments: investigations by means of a new microelectrochemical method", Corrosion Science, 43(4), pp.707~726 (2001), Elsevier BV[DOI]
  6. C.-O.A Olsson, "Passive films on stainless steels—chemistry, structure and growth", Electrochimica Acta, 48(9), pp.1093~1104 (2003), Elsevier BV[DOI]
  7. A. Rajesh Kannan, "Insight into the microstructural features and corrosion properties of wire arc additive manufactured super duplex stainless steel (ER2594)", Materials Letters, 270, pp.127680~ (2020), Elsevier BV[DOI]
  8. Dong Min Cho, "Corrosion behaviors according to the welding process of superduplex stainless steel welded tubes: Gas tungsten arc welding vs. laser beam welding", Corrosion Science, 216, pp.111108~ (2023), Elsevier BV[DOI]
  9. 이준호, "화력발전용 슈퍼 듀플렉스 스테인리스 강 조관재의 용접 후 열처리 조건이 국부부식 저항성에 미치는 영향", 한국표면공학회지, 54(5), pp.248~259 (2021), 한국표면공학회
  10. M. Sangsuriyun, "Optimization of high-frequency resistance welding process using mechanical property of finned tube SA-192 steel", Journal of Engineering and Applied Sciences, 15, pp.607~ (2020)
  11. R. Kocurek, "Manufacturing Technologies of Finned Tubes", Advances in Materials Sciences, 13(3), pp.26~ (2013), Walter de Gruyter GmbH[DOI]
  12. M.E. Wilms, "The effect of σ-phase precipitation at 800°C on the corrosion resistance in sea-water of a high alloyed duplex stainless steel", Corrosion Science, 36(5), pp.871~881 (1994), Elsevier BV[DOI]
  13. M. Sadeghian, "Effect of heat input on microstructure and mechanical properties of dissimilar joints between super duplex stainless steel and high strength low alloy steel", Materials & Design, 60, pp.678~684 (2014), Elsevier BV[DOI]
  14. R. G. Barrows, "A modified system for predicting σ formation", Metallurgical Transactions, 3(11), pp.2889~2893 (1972), Springer Science and Business Media LLC[DOI]
  15. Haijun Wang, "Study on heat transfer performance of fin-and-tube heat exchanger with elliptical fins", Journal of Energy Storage, 56, pp.105956~ (2022), Elsevier BV[DOI]
  16. Rawad Deeb, "Numerical analysis of the effect of longitudinal and transverse pitch ratio on the flow and heat transfer of staggered drop-shaped tubes bundle", International Journal of Heat and Mass Transfer, 183, pp.122123~ (2022), Elsevier BV[DOI]
  17. 조동민, "슈퍼 듀플렉스 스테인리스강(UNS S32506) 레이저 조관용접 튜브의 용접 후 열처리에 따른 부식거동", 한국표면공학회지, 54(3), pp.102~111 (2021), 한국표면공학회
  18. "ASTM G48-03, Standard Test Methods for Pitting and Crevice Corrosion Resistance of Stainless Steels and Related Alloys by Use of Ferric Chloride Solution", ASTM International, ~ (2003)
  19. Eiji Akiyama, "Hydrogen entry into Fe and high strength steels under simulated atmospheric corrosion", Electrochimica Acta, 56(4), pp.1799~1805 (2011), Elsevier BV[DOI]
  20. Saya Ajito, "Effect of Iron Rust on Hydrogen Uptake during Steel Corrosion under an Aqueous NaCl Droplet", ISIJ International, 61(4), pp.1186~1193 (2021), Iron and Steel Institute of Japan[DOI]
  21. Tooru Tsuru, "Hydrogen entry into steel during atmospheric corrosion process", Corrosion Science, 47(10), pp.2431~2440 (2005), Elsevier BV[DOI]
  22. Riad Badji, "Phase transformation and mechanical behavior in annealed 2205 duplex stainless steel welds", Materials Characterization, 59(4), pp.447~453 (2008), Elsevier BV[DOI]
  23. Ying Han, "Investigation on hot deformation behavior of 00Cr23Ni4N duplex stainless steel under medium–high strain rates", Materials Characterization, 62(2), pp.198~203 (2011), Elsevier BV[DOI]
  24. Vahid A Hosseini, "A novel arc heat treatment technique for producing graded microstructures through controlled temperature gradients", Materials & Design, 121, pp.11~23 (2017), Elsevier BV[DOI]
  25. Andrea Putz, "Microstructure investigation of duplex stainless steel welds using arc heat treatment technique", Welding in the World, 64(7), pp.1135~1147 (2020), Springer Science and Business Media LLC[DOI]
  26. Jin Sung Park, "Effects of reducing atmospheres of bright annealing on the surface and corrosion characteristics of super duplex stainless steel tubes", Surface and Coatings Technology, 423, pp.127621~ (2021), Elsevier BV[DOI]
  27. Kazuhiro Ogawa, "Modelling of Nitride Precipitation during Isothermal Heating after Rapidly Cooled from High Temperature in Duplex Stainless Steel", ISIJ International, 62(8), pp.1725~1730 (2022), Iron and Steel Institute of Japan[DOI]
  28. Y. Zhao, "Strategies for nitrogen control during the production of interstitial-free steel", Ironmaking & Steelmaking, 45(6), pp.485~491 (2017), Informa UK Limited[DOI]
  29. T. L. Christiansen, "High Temperature Solution Nitriding of Stainless Steels; Current Status and Future Trends", HTM Journal of Heat Treatment and Materials, 75(2), pp.69~82 (2020), Walter de Gruyter GmbH[DOI]
  30. Afrooz Barnoush, "Direct observation of hydrogen-enhanced plasticity in super duplex stainless steel by means of in situ electrochemical methods", Scripta Materialia, 62(5), pp.242~245 (2010), Elsevier BV[DOI]
  31. R. N. Gunn, "Duplex stainless steels: microstructure, properties and applications", pp.26~ (1997), Abington publishing
  32. Vahid A. Hosseini, "Microstructure and functionality of a uniquely graded super duplex stainless steel designed by a novel arc heat treatment method", Materials Characterization, 139, pp.390~400 (2018), Elsevier BV[DOI]
  33. Raphaël Marin, "Solidification path and phase transformation in super-austenitic stainless steel UNS S31254", IOP Conference Series: Materials Science and Engineering, 529(1), pp.012008~ (2019), IOP Publishing

관련 논문AI추천

화력발전용 슈퍼 듀플렉스 스테인리스 강 조관재의 용접 후 열처리 조건이 국부부식 저항성에 미치는 영향김성진, 박진성, 이준호, 조동민, 홍승갑한국표면공학회 · 한국표면공학회지2021 · 제54권 제5호슈퍼 듀플렉스 스테인리스강(UNS S32506) 레이저 조관용접 튜브의 용접 후 열처리에 따른 부식거동김성진, 박진성, 조동민, 홍승갑, 황중기한국표면공학회 · 한국표면공학회지2021 · 제54권 제3호SDSS (Super Duplex Stainless Steel) 강관의 미세조직 및 부식특성에 미치는 열처리 온도의 영향이면학, 이인섭, 임태홍, 천창석, 한윤호한국표면공학회 · 한국표면공학회지2015 · 제48권 제6호황산 수용액 내 듀플렉스 스테인리스강 (UNS S32205)의 부식거동에 미치는 용접프로세스 및 필거압연 공정의 영향한국재료부식학회 · CORROSION SCIENCE AND TECHNOLOGY2025 · 제24권 제5호소둔 및 용접후열처리가 슈퍼 오스테나이트계 스테인리스강의 부식거동에 미치는 영향김성진, 박진성, 윤덕빈, 조동민, 홍승갑한국재료부식학회 · CORROSION SCIENCE AND TECHNOLOGY2021 · 제20권 제6호Corrosion Properties of Duplex Stainless Steels - STS329LD and STS329J3L - for the Seawater Systems in Nuclear Power Plant김영식, 박흥배, 안상곤, 장윤영, 장현영한국재료부식학회 · CORROSION SCIENCE AND TECHNOLOGY2011 · 제10권 제2호

이 간행물의 다른 논문 (9건)