Effects of sodium dodecyl sulfate surfactant on up-conversion luminescence of Er3+/Yb3+ -codoped NaLa (MoO4)2 nanocolloidal phosphor prepared by pulsed laser ablation in water

2

조회

0

다운로드

0

인용

0

참고문헌

키워드

주제분류재료공학

초록

Er3+/Yb3+-codoped NaLa(MoO4)2 colloidal nanocrystals were synthesized by pulsed laser ablations in de-ionized water andsodium dodecyl sulfate (NaC12H25SO4, SDS) aqueous solution for up-conversion (UC) luminescence bio-labeling applications. The influences of the SDS molecules on the crystallinities, crystal morphologies, crystallite sizes, and UC luminescence propertiesof the prepared Er3+/Yb3+-codoped NaLa(MoO4)2 colloidal nanocrystals were investigated in detail. Under a 980-nm excitation,the Er3+/Yb3+-codoped nanocolloidal NaLa(MoO4)2 suspension exhibited a weak red emission near 670 nm and strong green UCemissions at 530 and 550 nm, corresponding to the intra 4f transitions of Er3+ (4F9/2, 2H11/2 , 4S3/2)→Er3+ (4I15/2). When the SDSsolution was used, a smaller average crystallite size, narrower size distribution, and enhanced UC luminescence were observed. These characteristics were attributed to the amphoteric SDS molecules attached to the positively charged Er3+/Yb3+-codopedNaLa(MoO4)2 colloidal nanocrystals, effectively occupying the oxygen defect on their surfaces. The Er3+/Yb3+-codopednanocrystalline NaLa(MoO4)2 suspension prepared in the SDS solution exhibited a remarkably strong green emission visibleto the naked eyes.

Abstract

Er3+/Yb3+-codoped NaLa(MoO4)2 colloidal nanocrystals were synthesized by pulsed laser ablations in de-ionized water andsodium dodecyl sulfate (NaC12H25SO4, SDS) aqueous solution for up-conversion (UC) luminescence bio-labeling applications. The influences of the SDS molecules on the crystallinities, crystal morphologies, crystallite sizes, and UC luminescence propertiesof the prepared Er3+/Yb3+-codoped NaLa(MoO4)2 colloidal nanocrystals were investigated in detail. Under a 980-nm excitation,the Er3+/Yb3+-codoped nanocolloidal NaLa(MoO4)2 suspension exhibited a weak red emission near 670 nm and strong green UCemissions at 530 and 550 nm, corresponding to the intra 4f transitions of Er3+ (4F9/2, 2H11/2 , 4S3/2)→Er3+ (4I15/2). When the SDSsolution was used, a smaller average crystallite size, narrower size distribution, and enhanced UC luminescence were observed. These characteristics were attributed to the amphoteric SDS molecules attached to the positively charged Er3+/Yb3+-codopedNaLa(MoO4)2 colloidal nanocrystals, effectively occupying the oxygen defect on their surfaces. The Er3+/Yb3+-codopednanocrystalline NaLa(MoO4)2 suspension prepared in the SDS solution exhibited a remarkably strong green emission visibleto the naked eyes.

참고문헌 (34)

  1. N. Menyuk, , Appl. Phys. Lett, 21, pp.159~165 (1972)
  2. P. Li, , Adv. Mater, 21, pp.1945~1948 (2009)
  3. L. Wang, , Angew. Chem. Int. Ed, 44, pp.6054~6057 (2005)
  4. Shalav, , Energy Mater. Sol. Cell, 91, pp.829~842 (2007)
  5. E. Downing, , Science, 273, pp.1185~1189 (1996)
  6. G. Glaspell, , J. Phys. Chem. C, 112, pp.11527~11531 (2008)
  7. T. Anh, , J. Nanomat, pp.48247~43857 (2007)
  8. A. B. Campos, , Appl. Phys. Lett, 91, pp.051923~ (2007)
  9. L. Macalik, , J. alloys Compd, 341, pp.226~232 (2002)
  10. Y. W. Wei, , J. Alloys Compd, 484, pp.529~534 (2009)
  11. L. H. C. Andrade, , J. Phys. Condens. Matter, 18, pp.7883~7894 (2006)
  12. M. S. Sibbald, , J. Phys. Chem, 100, pp.4672~4678 (1996)
  13. J. Heddersen, , Appl. Spectrosc, 47, pp.1959~1964 (1993)
  14. A. V. Simakin, , Chem. Phys. Lett, 348, pp.182~186 (2001)
  15. R. A. Ganeev, , Opt. Commun, 240, pp.437~448 (2004)
  16. G. A. Shafeev, , Appl. Phys. A, 78, pp.307~309 (2004)
  17. Iwabuchi, , J. Phys. Chem. B, 108, pp.10863~10871 (2004)
  18. K. V. Anikin, , Chem. Phys. Lett, 366, pp.357~360 (2002)
  19. R. A. Ganeev, , Appl. Phys. B, 80, pp.595~601 (2005)
  20. T. Tsuji, , Appl. Surf. Sci, 243, pp.214~219 (2005)
  21. K. M. Kim, , J. Alloy. Compd, 576, pp.195~200 (2013)
  22. K. Cho, , J. Vac. Sci. & Tech. B, 33, pp.041201~ (2015)
  23. Kyoungwon Cho, "Pulsed-laser-assisted Synthesis of a Tm3+", Yb3+ Co-doped CaMoO4 Colloidal Nanocrystal and Its Upconversion Luminescence, 2016, pp.68(1), 22~27[DOI]
  24. 이정일, "Synthesis of Scheelite Structural Yb3+, Er3+ Co-doped NaLa(MoO4)2 and Its Green Upconversion Luminescence", Journal of the Korean Physical Society, 65(10), pp.1644~1648 (2014), 한국물리학회
  25. R. Chadha, , Spectrochim. Acta A, 150, pp.664~670 (2015)
  26. H. Vatanparast, , Colloid. Surface A, 513, pp.430~441 (2017)
  27. K. Cho, , J. Nanosci. Nanotechnol, 16, pp.6344~6349 (2016)
  28. V. A. Ageev, , J. Appl. Spectr, 64, pp.683~688 (1997)
  29. T. Sakka, , J. Chem. Phys, 112, pp.8645~8653 (2000)
  30. Y. -H. Chen, , Colloid. Surface A, 197, pp.133~139 (2002)
  31. F. Auzel, , Chem. Rev, 104, pp.139~174 (2004)
  32. F. Wang, , Chem. Soc. Rev, 38, pp.976~989 (2009)
  33. J. -H. Zeng, , Adv. Mater, 17, pp.2119~2123 (2005)
  34. G. -S. Yi, , J. Mater. Chem, 15, pp.4460~4464 (2005)

관련 논문AI추천

이 간행물의 다른 논문 (13건)