초록
The upconversion (UC) photoluminescence of Er3+/Yb3+ co-doped SrMoO4 (SrMoO4 : Er3+/Yb3+) nanoparticles were successfully synthesized via a cyclic microwave-assisted metathetic (MAM) route. Well-crystallized SrMoO4 : Er3+/Yb3+ nanoparticles (100- 500 nm) were formed after heat treatment at 600 ο C for 3 h and showed a fine and homogeneous morphology. With excitation at 980 nm, SrMoO4 : Er3+/Yb3+# exhibited a strong 525-nm emission band and a weak 550-nm emission band in the green region and a weak 655-nm emission band in the red region. The Raman spectra of SrMoO4 : Er3+, SrMoO4 : Er3+/Yb3+ and SrMoO4 : Er3+/Yb3+# nanoparticles indicated additional strong peaks at both higher frequencies (564, 524, 456 and 403 cm-1) and lower frequencies (294, 251 and 220 cm-1).
Abstract
The upconversion (UC) photoluminescence of Er3+/Yb3+ co-doped SrMoO4 (SrMoO4 : Er3+/Yb3+) nanoparticles were successfully synthesized via a cyclic microwave-assisted metathetic (MAM) route. Well-crystallized SrMoO4 : Er3+/Yb3+ nanoparticles (100- 500 nm) were formed after heat treatment at 600 ο C for 3 h and showed a fine and homogeneous morphology. With excitation at 980 nm, SrMoO4 : Er3+/Yb3+# exhibited a strong 525-nm emission band and a weak 550-nm emission band in the green region and a weak 655-nm emission band in the red region. The Raman spectra of SrMoO4 : Er3+, SrMoO4 : Er3+/Yb3+ and SrMoO4 : Er3+/Yb3+# nanoparticles indicated additional strong peaks at both higher frequencies (564, 524, 456 and 403 cm-1) and lower frequencies (294, 251 and 220 cm-1).
참고문헌 (27)
- M. Wang, , Nanomedicine: Nanotech. Biology, and Medicine, 7, pp.710~729 (2011)
- A. Shalav, , Solar Ener. Mat. &Solar Cells, 91, pp.829~842 (2007)
- C. Zhang, , J. Rare Earths, 28, pp.807~819 (2010)
- J. C. Sczancoski, , Chem. Eng. J, 140, pp.632~637 (2008)
- T. Thongtem, , J. Alloys & Comp, 506, pp.475~481 (2010)
- T. Thongtem, , J. Nanopart. Res, 12, pp.2287~2294 (2010)
- J. Sun, , J. Phys. Chem. of Solids, 72, pp.207~213 (2011)
- J. Sun, , J. Rare Earths, 28, pp.219~221 (2010)
- V. K. Komarala, , Chem. Phys. Lett, 490, pp.189~193 (2010)
- X. Lin, , Solid State Science, 13, pp.579~583 (2011)
- L. Y. Zhou, , J. Solid State Chem, 181, pp.1337~1341 (2008)
- J. Liu, , Optical Mat, 29, pp.1591~1595 (2007)
- X. Li, , J. Alloys & Comp, 478, pp.684~686 (2009)
- D. Gao, , Mat. Chem. Phys, 126, pp.391~397 (2011)
- Y. Yang, , J. Alloys & Comp, 509, pp.845~848 (2011)
- F. B. Cao, , Thin Solid Films, 519, pp.7971~7976 (2011)
- Y. Jin, , J. Alloys &Comp, 509, pp.L348~L351 (2011)
- F. Yu, , Mat. Res. Bull, 46, pp.1327~1332 (2011)
- F. Lei, , J. Sol. Sta. Chem, 181, pp.855~862 (2008)
- Z. J. Zhang, , Mat. Sci. Eng. B, 145, pp.34~40 (2007)
- N. Niu, , Mat. Res. Bull, 46, pp.333~339 (2011)
- J. Zhang, , Inorg. Chem. Comm, 14, pp.1723~1727 (2011)
- C. S. Lim, , Mat. Chem. Phys, 131, pp.714~718 (2012)
- S. Das, , Bull. Mat. Sci, 32, pp.1~13 (2009)
- K. P. F. Siqueira, , J. Mat. Sci, 45, pp.6083~6093 (2010)
- P. Parhi, , J. Alloys & Compd, 465, pp.380~386 (2008)
- V. Thangadurai, , Mat. Sci. Eng. B, 106, pp.228~233 (2004)