Silicon carbide (SiC) fibers fabricated by melt-spinning, curing, and pyrolysis of polycarbosilane (PCS) as a ceramic precursor were used to fabricate the heat-generating mats by interaction with microwave. In this study, the effect of pyrolysis temperature on heat-generating temperature of SiC fiber mats was investigated to optimize the performance of mats via microstructure control in the fiber. SiC fibers synthesized at high pyrolysis temperature contained a relatively low oxygen content due to the residual oxygen release in the form of SiO and CO gases. The optimization of the elemental composition in SiC fiber by minimizing oxygen level enable the maximum heat-generating temperature and life-time of the SiC fiber mats under microwave. Also, the polymer-derived SiC fiber mats exhibited both oxidative- or thermal-degradation due to the nonuniform heat-generating by the edge effect under microwave.
Abstract
Silicon carbide (SiC) fibers fabricated by melt-spinning, curing, and pyrolysis of polycarbosilane (PCS) as a ceramic precursor were used to fabricate the heat-generating mats by interaction with microwave. In this study, the effect of pyrolysis temperature on heat-generating temperature of SiC fiber mats was investigated to optimize the performance of mats via microstructure control in the fiber. SiC fibers synthesized at high pyrolysis temperature contained a relatively low oxygen content due to the residual oxygen release in the form of SiO and CO gases. The optimization of the elemental composition in SiC fiber by minimizing oxygen level enable the maximum heat-generating temperature and life-time of the SiC fiber mats under microwave. Also, the polymer-derived SiC fiber mats exhibited both oxidative- or thermal-degradation due to the nonuniform heat-generating by the edge effect under microwave.
참고문헌 (24)
- C.A. Finch, "Encyclopedia of Textiles, Fibers, and Nonwoven Fabrics", pp.438~450 (1984), Wiley-Interscience
- T. F. Cooke, , J. Am. Ceram. Soc, 74(12), pp.2959~2978 (1991)
- Ji Yeon Park, "Characterization of the matrix phase of whisker growing-assisted CVI-SiCf", SiC composites, 2009, pp.10(3), 364~366[DOI]
- 길건영, "Densification of SiCf", SiC composites by electrophoretic infiltration combined with ultrasonication, 2011, pp.12(4), 371~375[DOI]
- B. Budiansky, , Phys. Solids, 34(2), pp.167~189 (1986)
- R. Naslain, , Compos. Sci. Technol, 64(2), pp.155~170 (2004)
- S. Schmidt, , Acta. Astronautica, 55(3-9), pp.409~420 (2004)
- T. Yamamura, , J. Mater. Sci, 23(7), pp.2589~2594 (1988)
- H. Yamaoka, , J. Mater. Sci, 34(6), pp.1333~1339 (1999)
- T. Ishikawa, , Nature, 391(19), pp.773~755 (1998)
- H. Ichikawa, , J. Mater. Sci, 6(4), pp.420~422 (1987)
- M. Takeda, , Compos. Sci. Technol, 59(6), pp.813~819 (1999)
- M. Takeda, , J. Am. Ceram. Soc, 83(5), pp.1063~1069 (2000)
- J. S. Hong, , J. Mater. Chem. A, 2(8), pp.2781~2793 (2014)
- J. S. Hong, , J. Appl. Polym. Sci, 132(47), pp.42687~ (2015)
- Khos-Erdene Khishigbayar, "Microwave-Assisted Heating of Electrospun SiC Fiber Mats", 한국세라믹학회지, 54(6), pp.499~505 (2017), 한국세라믹학회
- Khos-Erdene Khishigbayar, "Heating Behavior of Silicon Carbide Fiber Mat under Microwave", 한국세라믹학회지, 53(6), pp.707~711 (2016), 한국세라믹학회
- H. Tian, , Compo. Sci. Technol, 50(10), pp.202~208 (2014)
- B. Wang, , RSC Adv, 20(7), pp.12126~12132 (2018)
- Y. Sasaki, , J. Mater. Sci, 22(2), pp.443~448 (1987)
- K. Morishita, , Mater. Trans, 48(2), pp.111~116 (2007)
- M. takeda, , J. Nucl. Mater, 259-263, pp.1594~1599 (1998)
- S. Cao, , Cryst. Eng. Comm, 18(20), pp.3674~3682 (2016)
- Dong-Geun Shin, "Microstructure and properties of Web-type polycrystalline SiC fiber prepared by electrospinning and sintering of aluminum doped polycarbosilane", Journal of Ceramic Processing Research, 15(5), pp.298~304 (2014), 청정에너지연구소[DOI]