To improve the grinding efficiency of silicon nitride ceramic balls and save processing costs, the pretreatment of hydrofluoricacid that corrodes silicon nitride was introduced into the grinding process based on the chemical characteristics of siliconnitride ceramics that are not resistant to hydrofluoric acid. This paper mainly discusses the effect of hydrofluoric acidpretreatment on the corrosion and grinding of silicon nitride ceramic balls. Through comparison experiments of grindingsilicon nitride balls before and after corrosion, it is found that hydrofluoric acid can effectively destroy the structure andreduce the strength of silicon nitride ceramic on the surface. After pretreatment, the grinding removal efficiency of siliconnitride ceramic balls was significantly improved, the ball diameter variation was reduced, and there was no effect on theproperties of silicon nitride ceramic. This processing method is expected to be applied to the mass production of silicon nitrideceramic balls.
Abstract
To improve the grinding efficiency of silicon nitride ceramic balls and save processing costs, the pretreatment of hydrofluoricacid that corrodes silicon nitride was introduced into the grinding process based on the chemical characteristics of siliconnitride ceramics that are not resistant to hydrofluoric acid. This paper mainly discusses the effect of hydrofluoric acidpretreatment on the corrosion and grinding of silicon nitride ceramic balls. Through comparison experiments of grindingsilicon nitride balls before and after corrosion, it is found that hydrofluoric acid can effectively destroy the structure andreduce the strength of silicon nitride ceramic on the surface. After pretreatment, the grinding removal efficiency of siliconnitride ceramic balls was significantly improved, the ball diameter variation was reduced, and there was no effect on theproperties of silicon nitride ceramic. This processing method is expected to be applied to the mass production of silicon nitrideceramic balls.
참고문헌 (29)
- Wei Liting, "Mechanical, dielectric properties and thermal shock resistance of porous Si2N2O", Si3N4 composite ceramics, 2018, pp.19(2), 126~129[DOI]
- Yuan Lu, "Effects of α-Si₃N₄ seeds and sintering additives on properties of porous silicon nitride ceramics fabricated by carbothermal reduction", Journal of Ceramic Processing Research, 9(6), pp.657~660 (2008), 청정에너지연구소[DOI]
- Seok-Hwan Ahn, "Bending strength and wear characteristics of Si3N4 composites containing additives SiO2 and TiO2", Journal of Ceramic Processing Research, 22(1), pp.54~60 (2021), 청정에너지연구소[DOI]
- G. Levesque, , Int. J. Solids Struct, 45(25-26), pp.6301~6315 (2008)
- Y.H. Wu, , Key Eng. Mater, 291-292 (2005)
- T. Kurobe, , J. Jpn. Soc. Precis. Eng, 62(12), pp.1773~1777 (1996)
- B.H. Lv, , Adv. Mater. Res, 69-70, pp.69~73 (2009)[DOI]
- N. Umehara, , Int. Mach. Tool. Manu, 46(2), pp.151~169 (2006)
- T. H. C. Childs, , Tribol. Int, 28(6), pp.341~348 (1995)
- B. H. Lv, , Mater. Sci. Forum, 532, pp.460~463 (2006)
- K. R. Mikeska, , J. Am. Ceram. Soc, 83(5), pp.1160~1164 (2000)
- H. Klemm, , J. Am. Ceram. Soc, 93(6), pp.1501~1522 (2010)
- M. Herrmann, , J. Ceram. Soc. Jpn, 114(1335), pp.1069~1075 (2006)
- J. Schilm, , J. Eur. Ceram. Soc, 24(8), pp.2319~2327 (2004)
- M. Herrmann, , J. Am. Ceram. Soc, 96(10), pp.3009~3022 (2013)
- Ah Hyun Oh, "Fabrication of silicon carbide particles from recycled polysilicon photovoltaic cells", Journal of Ceramic Processing Research, 21(4), pp.400~406 (2020), 청정에너지연구소[DOI]
- Sang-Cheol Jeong, "Weibull statistical analysis on Vickers hardness of immersed Al2O3 ceramics in acidic and alkaline solution", Journal of Ceramic Processing Research, 18(7), pp.506~520 (2017), 청정에너지연구소[DOI]
- J. R. Frade, , J. Mater. Sci, 32(10), pp.2727~2733 (1997)
- M. Herrmann, , Ceram. Int, 35(2), pp.797~802 (2009)
- R. Conradt, , J. Am. Ceram. Soc, 91(3), pp.728~735 (2008)
- G. A. C. M. Spierings, , J. Mater. Sci, 22(5), pp.1869~1874 (1987)
- J. R. Frade, , J. Am. Ceram. Soc, 78(1), pp.90~96 (1995)
- T. A. Michalske, , J. Am. Ceram. Soc, 66(4), pp.284~288 (1983)
- M. Herrmann, , J. Eur. Ceram. Soc, 23(4), pp.585~594 (2003)
- J. Schilm, , J. Eur. Ceram. Soc, 27(12), pp.3573~3588 (2007)
- B. Seipel, , Ceram. Int, 30(2), pp.267~271 (2004)
- T. Sato, , J. Mater. Sci, 23(10), pp.3440~3446 (1988)
- S. W. Sharkawy, , Corros. Sci, 40(7), pp.1119~1129 (1998)
- J. H. Gong, "Fracture mechanics of ceramics" (2001), Tsinghua University Press