초록
To reduce the demand for fossil fuel energy, one of the solutions is using an renewable energy sources, such as wind andsolar. Solar energy is increasingly becoming the hottest issue in recent years because of its merits in installation and operation. In2015, about 50.7 GW photovoltaic (PV) systems were installed around world. Many renewable energy organizations expect that thetotal PV system installation will be 60 GW in the coming year.[1] To sustain the long-term stability of the PV system, several instituteshave performed tests based on IEC standards, such as IEC 61215 for silicon crystalline PV modules and IEC 61646 for thin film PVmodules and IEC 61730-1&2 for safety tests. In the case of amorphous silicon thin film modules,[2,3] its performance can be loweredbecause its natural characteristics under sun light called, the Staebler-Wronski effect.[4,5] Therefore, some companies conduct lightsoaking tests to guarantee stable electric performance before shipment. On the other hand, in the case of having high degradationcharacteristics at the maximum power, this test could take much time for production and lead to an increase in product cost. To solvethis technical difficulty and obtain actual stable performance power of silicon-based amorphous solar modules, the current-inducedstabilization (CIS) technique was proposed and assessed.
Abstract
To reduce the demand for fossil fuel energy, one of the solutions is using an renewable energy sources, such as wind andsolar. Solar energy is increasingly becoming the hottest issue in recent years because of its merits in installation and operation. In2015, about 50.7 GW photovoltaic (PV) systems were installed around world. Many renewable energy organizations expect that thetotal PV system installation will be 60 GW in the coming year.[1] To sustain the long-term stability of the PV system, several instituteshave performed tests based on IEC standards, such as IEC 61215 for silicon crystalline PV modules and IEC 61646 for thin film PVmodules and IEC 61730-1&2 for safety tests. In the case of amorphous silicon thin film modules,[2,3] its performance can be loweredbecause its natural characteristics under sun light called, the Staebler-Wronski effect.[4,5] Therefore, some companies conduct lightsoaking tests to guarantee stable electric performance before shipment. On the other hand, in the case of having high degradationcharacteristics at the maximum power, this test could take much time for production and lead to an increase in product cost. To solvethis technical difficulty and obtain actual stable performance power of silicon-based amorphous solar modules, the current-inducedstabilization (CIS) technique was proposed and assessed.
참고문헌 (18)
- IEA PVPS, "Trends in 2016 in Photovoltaic Applications", IEA International Agency, Chapter 2(8), ~ (2016)
- JiEun Lee, "The characteristic analysis of TCO", p-layer interface in Amorphous Silicon Solar Cell, 2007, pp.3(4), 63~
- Jeeong Chul Lee, "Amorphous silicon thin-film solar cells with high open circuit voltage by using textured ZnO:Al front TCO", New&Renewable Energy, 2(3), pp.31~ (2006)
- Carlson, "Amorphous silicon solar cell", Appl. Phys. Lett., 28, pp.671~ (1976)
- Staebler Wronski, "Reversible conductivity changes in discharge-produced amorphous Si", Appl. Phys. Lett., 31, pp.292~ (1977)
- T. Yanagisawa, "Changes in the temperature coefficients of the characteristics of amorphous silicon solar cells subjected to light degradation and recovery", Solar Energy Materials & Solar Cells, 69, pp.287~ (2001)
- D. Caputo, "Degradation and annealing of amorphous silicon solar cells by current injection:experiment and modeling", Solar Energy Materials &Solar Cells, 59, pp.289~ (1999)
- A. Dasgupta, "Accelerated degradation in amorphous silicon solar cells by a combination of current injection and light insolation", Solar Energy Materials & Solar Cells, 55, pp.395~ (1998)
- 김경수, "옥외 설치된 비정질 실리콘 박막태양전지모듈의 전기적 출력 특성 분석", 한국태양에너지학회 논문집, 28(4), pp.62~67 (2008), 한국태양에너지학회
- J.I.Pankove, "Light-induced radiative recombination centers in hydrogenated amorphous silicon", Appl. Phys. Lett., 37, pp.705~ (1980)
- M.Stutzmann, "Light-induced metastable defects in hydrogenated amorphous silicon: A systematic study", Phys. Rev. B, 32, pp.23~ (1985)
- H.M.Branz, "Hydrogen collision model:Quantitative description of metastability in amorphous silicon", Phys. Rev.B, 59, pp.5498~ (1999)
- R.Biswas, "Mechanisms of metastability in hydrogenated amorphous silicon", Sol. Energy Mater. Sol. Cells, 78, pp.447~ (2003)
- G.Schumm, "Chemical equilibrium description of stable and metastable defect structures in a-Si:H", Phys.Rev, B49, pp.2427~ (1994)
- V.Na´dazˇdy, "Origin of charged gap states in a-Si:H and their evolution during light soaking", Phys. Rev. B, 69, pp.165213~ (2004)
- A.Klaver, "Modeling of light-induced degradation of amorphous silicon solar cells", Sol. Energy Mater. Sol. Cells, 92, pp.50~ (2008)
- "IEC 60904-9, Photovoltaic devices – Part 9: Solar simulator performance requirements", ~
- "IEC 61646, Thin-film terrestrial photovoltaic (PV)modules – Design qualification and type approval", ~