본문 바로가기
KERD
논문KCI 등재

Fabrication of Ultra Fine β-phase Ti-Nb-Sn-HA Composite by Pulse Current Activated Sintering

1

조회

0

다운로드

2

인용

0

참고문헌

키워드

주제분류금속공학

초록

The β phase Ti-Nb-Sn-HA bio materials were successfully fabricated by high energy mechanical milling and pulse current activated sintering (PCAS). Ti-6Al-4V ELI alloy has been widely used as biomaterial. But the Al has been inducing Alzheimer disease and V is classified as toxic element. In this study, ultra fine sized Ti-Nb-Sn-HA powder was produced by high energy mechanical milling machine. The β phase Ti-Nb-Sn-HA powders were obtained after 12hr milling from α phase. And ultra fine grain sized Ti-Nb-Sn-HA composites could be fabricated using PCAS without grain growth. After sintering, the microstructures and phase-transformation of Ti-Nb-Sn-HA biomaterials were analyzed by scanning electron microscope (SEM) and X-ray diffraction (XRD). The relative density was obtained by Archimedes principle and the hardness was measured by Vickers hardness tester. The β-Ti phase was obtained after 12h milling. As result of hardness and relative density, 12h milled Ti-Nb-Sn-HA composite has the highest values.

Abstract

The β phase Ti-Nb-Sn-HA bio materials were successfully fabricated by high energy mechanical milling and pulse current activated sintering (PCAS). Ti-6Al-4V ELI alloy has been widely used as biomaterial. But the Al has been inducing Alzheimer disease and V is classified as toxic element. In this study, ultra fine sized Ti-Nb-Sn-HA powder was produced by high energy mechanical milling machine. The β phase Ti-Nb-Sn-HA powders were obtained after 12hr milling from α phase. And ultra fine grain sized Ti-Nb-Sn-HA composites could be fabricated using PCAS without grain growth. After sintering, the microstructures and phase-transformation of Ti-Nb-Sn-HA biomaterials were analyzed by scanning electron microscope (SEM) and X-ray diffraction (XRD). The relative density was obtained by Archimedes principle and the hardness was measured by Vickers hardness tester. The β-Ti phase was obtained after 12h milling. As result of hardness and relative density, 12h milled Ti-Nb-Sn-HA composite has the highest values.

참고문헌 (13)

  1. A. Nouri, , Mater. Sci. Eng, 485, pp.562~ (2008)
  2. G. He, , Biomater, 24, pp.5115~ (2003)
  3. M. Niinomi, , Mater. Sci.Eng, 100, pp.45~ (1988)
  4. S. Tria, , J. Alloys Compd, 483, pp.334~ (2009)
  5. 우기도, "통전가압활성소결에 의한 생체재료용 Ti-HA복합재료 제조 및 특성", 대한금속·재료학회지, 47(8), pp.508~515 (2009), 대한금속·재료학회
  6. 우기도, "Leaching 공정으로 제조한 표면 다 기공 Ti-HA 생체재료의 표면 조직 및 기계적 성질의 평가", 대한금속·재료학회지, 48(4), pp.369~375 (2010), 대한금속·재료학회
  7. Y. Okazaki, , Biomater, 19, pp.1197~ (1998)
  8. M. Long, , Biomater, 19, pp.1621~ (1998)
  9. Y.-L. Zhou, , J. Alloys Compd, 466, pp.535~ (2008)
  10. C. Q. Ning, , Biomater, 23, pp.2909~ (2002)
  11. C. Q. Ning, , Biomater, 25, pp.3379~ (2004)
  12. R. Sun, , Mater. Sci. Eng, 26, pp.31~ (2006)
  13. K. D. Woo, "Microstructures and Mechanical Properties of Biocompatible Ti-42 wt.%Nb P", M Alloy, 2008, pp.14(3), 327~333[DOI]