가압소결로 제조된 YSZ-30 vol.% WC 복합체 세라믹스의 상형성 거동과 기계적 특성
Phase Formation and Mechanical Property of YSZ‒30 vol.% WC Composite Ceramics Fabricated by Hot Pressing
1
조회
0
다운로드
0
인용
0
참고문헌
키워드
초록
YSZ (Y2O3-stabilized zirconia)-based ceramics have excellent mechanical properties, such as high strength and wear resistance. In the application, YSZ is utilized in the bead mill, a fine-grinding process. YSZ-based parts, such as the rotor and pin, can be easily damaged by continuous application with high rpm in the bead mill process. In that case, adding WC particles improves the tribological and mechanical properties. YSZ-30 vol.% WC composite ceramics are manufactured via hot pressing under different pressures (10/30/60 MPa). The hot-pressed composite ceramics measure the physical properties, such as porosity and bulk density values. In addition, the phase formation of these composite ceramics is analyzed and discussed with those of physical properties. For the increased applied pressure of hot pressing, the tetragonality of YSZ and the crystallinity of WC are enhanced. The mechanical properties indicate an improved tendency with the increase in the applied pressure of hot pressing.
Abstract
YSZ (Y2O3-stabilized zirconia)-based ceramics have excellent mechanical properties, such as high strength and wear resistance. In the application, YSZ is utilized in the bead mill, a fine-grinding process. YSZ-based parts, such as the rotor and pin, can be easily damaged by continuous application with high rpm in the bead mill process. In that case, adding WC particles improves the tribological and mechanical properties. YSZ-30 vol.% WC composite ceramics are manufactured via hot pressing under different pressures (10/30/60 MPa). The hot-pressed composite ceramics measure the physical properties, such as porosity and bulk density values. In addition, the phase formation of these composite ceramics is analyzed and discussed with those of physical properties. For the increased applied pressure of hot pressing, the tetragonality of YSZ and the crystallinity of WC are enhanced. The mechanical properties indicate an improved tendency with the increase in the applied pressure of hot pressing.
참고문헌 (19)
- F. Riley, "Structural Ceramics", pp.313~ (2009), Cambridge University Press
- B. Basu, "Advanced Structural Ceramics", pp.175~ (2009), John Wiley & Sons, Inc
- M. W. Barsoum, "Fundamentals of Ceramics", pp.383~ (2003), Taylor &Francis Group
- O. Vasylkiv, , Mater. Trans, 44, pp.2235~ (2003)
- 최재형, "고온가압소결을 이용한 YSZ-TiC 세라믹스 복합체의 제조와 특성", 한국분말재료학회지, 28(5), pp.381~388 (2021), 한국분말재료학회
- 남민수, "3Y-TZP", WC 복합체의 소결 방식에 따른 특성비교, 2022, pp.29(5), 424~431[DOI]
- B. Basu, , J. Alloys Compos, 372, pp.278~ (2004)
- D. Jiang, , J. Eur. Ceram. Soc, 27, pp.1247~ (2007)
- M. Grigoriev, , Mater. Sci. Eng, 116, pp.012002~ (2016)
- J. H. Choi, , Ceram. Int, 49, pp.13414~ (2023)
- B. Basu, , J. Am. Ceram. Soc, 89, pp.2405~ (2006)
- N. Ünal, , J. Eur. Ceram. Soc, 31, pp.2267~ (2011)
- Z. Pędzich, "Tungsten Carbide: Processing and Applications", pp.81~ (2012), IntechOpen
- S. Huang, , Mater. Sci. Eng. A, 527, pp.584~ (2010)
- P. Angerer, , Int. J. Refract. Met. Hard Mater, 25, pp.280~ (2007)
- R. Yamanoglu, , Powder Metall, 61, pp.178~ (2018)
- M. N. Rahaman, "Ceramic Processing and Sintering" (1995), Marcel Dekker, Inc
- J. Chevalier, , J. Am. Ceram. Soc, 92, pp.1901~ (2009)
- F. J. Paneto, , Int. J. Refract. Met. Hard Mater, 48, pp.365~ (2015)