초록
UV-curable acrylic Pressure-sensitive adhesives (Acrylic PSAs) are used in many different parts in the world. A wafer manufacture process which is based on semiconductor industry is one thing. We have used acrylic PSAs whose thickness is different from 20 μm to 30 μm in wafer manufacture process so far. But as wafers become more thinner, acrylic PSAs are supposed to satisfy the requirements such as proper adhesion performance. The main purpose of this research is studying proper adhesion performance and UV-curing behavior of UV-curable acrylic PSAs with very thin thickness and then determining optimized conditions to raise the efficiency of thin wafer production. Acrylic PSAs contain 2-Ethylhexyl Acrylate (2-EHA), Acrylic Acid (AA) and Butyl Acrylate (BA). Ethyl acetate (EtAc) is used as solvent. The acrylic PSAs are obtained using solvent polymerization. Thickness of UV-curable acrylic PSAs is different from 10∼30 μm. By peel strength and probe tack, adhesion performance and UV curing behavior of acrylic PSA are concerned.
Abstract
UV-curable acrylic Pressure-sensitive adhesives (Acrylic PSAs) are used in many different parts in the world. A wafer manufacture process which is based on semiconductor industry is one thing. We have used acrylic PSAs whose thickness is different from 20 μm to 30 μm in wafer manufacture process so far. But as wafers become more thinner, acrylic PSAs are supposed to satisfy the requirements such as proper adhesion performance. The main purpose of this research is studying proper adhesion performance and UV-curing behavior of UV-curable acrylic PSAs with very thin thickness and then determining optimized conditions to raise the efficiency of thin wafer production. Acrylic PSAs contain 2-Ethylhexyl Acrylate (2-EHA), Acrylic Acid (AA) and Butyl Acrylate (BA). Ethyl acetate (EtAc) is used as solvent. The acrylic PSAs are obtained using solvent polymerization. Thickness of UV-curable acrylic PSAs is different from 10∼30 μm. By peel strength and probe tack, adhesion performance and UV curing behavior of acrylic PSA are concerned.
참고문헌 (18)
- "High-Density Pakaging (MCM, MCP, SIP): Market Analysis and Technology Trends", The Information Network, ~ (2005)
- D. Satas, "Handbook of Pressure Sensitive Adhesive Technology" (1999), Satas & Associates
- H. J. Kim, "Chemistry and Application of Adhesion", J. Adhesion and Interface (2002)
- 박지원, "조합기법을 활용한 아크릴 점착제의 점착물성 평가", 접착 및 계면, 10(3), pp.127~133 (2009), 한국접착및계면학회
- 유종민, "아크릴계 점착제와 초박형 웨이퍼소재와의 점착특성 - 아크릴 중합체의 측쇄의 영향 -", 접착 및 계면, 10(3), pp.134~140 (2009), 한국접착및계면학회
- H. S. Joo, , J. Adhesion and Interface, 6, pp.19~ (2005)
- A. Zosel, , Int. J. Adhes. Adhes, 18, pp.265~ (1998)
- J. Kajtna, , Int. J. Adhes. Adhes, 29, pp.186~ (2009)
- I. Benedek, "Pressure Sensitive Adhesives Technology" (1997), Maecel Decker
- K. Ebe, , J. Appl. Polym. Sci, 90, pp.436~ (2003)
- Z. Czech, , Int. J. Adhes. Adhes, 27, pp.49~ (2007)
- H. S. Do, , European Polymer Journal, 44, pp.3871~ (2008)
- Z. Czech, , European Polymer Journal, 40, pp.2221~ (2004)
- J. J. Park, "Korean Patent, 10-2000- 0035727", ~
- H. S. Do, "Korean Patent, 10-2004- 094902", ~
- K. Horigome, , J. Appl. Polym. Sci, 93, pp.2889~ (2004)
- 이명천, "자외선 경화형 점착제의 접착 및 재박리 특성", Korean Chemical Engineering Research(HWAHAK KONGHAK), 46(1), pp.76~81 (2008), 한국화학공학회
- Z. Czech, , Int. J. Adhes. Adhes, 24, pp.533~ (2004)