HRSG 보일러 튜브 내면 스케일의 특성연구

A Study on Characteristics of HRSG Boiler Inner Tube Scale

3

조회

0

다운로드

0

인용

0

참고문헌

키워드

주제분류금속공학

초록

The thickness and chemical composition of oxides on heat recovery steam generator tubes of combined cycle power plant were examined in order to evaluate the corrosion of the tubes. Tubes were removed from the plant after actual operations for 21,482, 42,552 and 56,123 hours respectively. Thickness and growth rate of the oxide scale on reheater inner tube (SA213-T22) were very high compared to those other tubes. The oxide scale was about 250 ㎛ thick and uniform. The components of the scale were iron oxides. The oxide scale was mixed oxides consisting of magnetite(Fe3O4) and hematite(Fe2O3). The oxide on inner tube was removed using many kinds of chemicals and it was found that chelating agents were dissolved faster than other chemicals.

Abstract

The thickness and chemical composition of oxides on heat recovery steam generator tubes of combined cycle power plant were examined in order to evaluate the corrosion of the tubes. Tubes were removed from the plant after actual operations for 21,482, 42,552 and 56,123 hours respectively. Thickness and growth rate of the oxide scale on reheater inner tube (SA213-T22) were very high compared to those other tubes. The oxide scale was about 250 ㎛ thick and uniform. The components of the scale were iron oxides. The oxide scale was mixed oxides consisting of magnetite(Fe3O4) and hematite(Fe2O3). The oxide on inner tube was removed using many kinds of chemicals and it was found that chelating agents were dissolved faster than other chemicals.

참고문헌 (12)

  1. Study on chemical cleaning of HRSG tubes of combined cycle power plant, "H. G. Lim", KEPRI, ~ (2007)
  2. Program on Technology Innovation : Oxide Growth and Exfolliation on Alloys Exposed to Steam, "I.G.Wright", ~, pp.EPRI 1013666 (2007)
  3. Boiler and Heat Recovery Steam Generator Tube Failure : Theory and Practice, "R. B. Dooley", ~, pp.EPRI 1012757 (2007)
  4. S.R.Paterson, "Oxidation of Boiler Tubing" (1992), Aptech Engineering Services, Inc
  5. J. Stringer, "High-temperature corrosion problems in steam boilers", Corrosion in Fossil Fuel Systems, Proceeding, 83-5 (1983), The Electrochemical Society
  6. J. W. Siegmund, "Acid Cleaning Guidelines for Superheater-Reheaters and Main and Reheater Steam Piping", pp.1~ (1989), EPRI Solid Particle Erosion Of Utility Steam Turbines
  7. "Handbook of X-ray Diffraction Spectrometry" (1998), Rigaku Corp
  8. Buhrke, V. E, "A Practical Guide for the Preparation of Specimens for XRF and XRD Analysis" (1998), Wiley
  9. Jenkins, R, "Practical X-ray Spectrometry" (1973), Springer-Verlag
  10. Goldstein, J. I, "Scanning Electron Microscopy and X-Ray Microanalysis" (2003), Springer
  11. B. M. Seo, "A Study of On-Line Corrosion Monitoring in Chemical Cleaning Process", J. Corros. Sci. Soc. of Korea, 28, pp.245~ (1999)
  12. Turbine damage by solid particle erosion, "K.G. Reinhard", ~, pp.ASME paper No. 76-JPGC-Pwr-15 (1978)

이 간행물의 다른 논문 (4건)