Interest in aluminum alloys for the hydrogen valves of fuel cell electric vehicles (FCEVs) is growing due to the reduction in fuel efficiency by the high weight. However, when an aluminum alloy is used, deterioration in mechanical characteristics caused by hydrogen embrittlement and wear is regarded as a problem. In this investigation, the aluminum alloy used to prevent hydrogen embrittlement was subjected to surface treatments by performing hard anodizing and plasma ion nitriding processes. The hard anodized Al alloy exhibited brittleness in which the mechanical characteristics rapidly deteriorated due to porosity and defects of surface, resulting in a decrease in the ultimate tensile strength and modulus of toughness by 15.58 and 42.51%, respectively, as the hydrogen charging time increased from 0 to 96 hours. In contrast, no distinct nitriding layer in the plasma ion-nitrided Al alloy was observed due to oxide film formation and processing conditions. However, compared to 0 and 96 hours of hydrogen charging time, the ultimate tensile strength and modulus of toughness decreased by 7.54 and 13.32%, respectively, presenting excellent resistance to hydrogen embrittlement.
Abstract
Interest in aluminum alloys for the hydrogen valves of fuel cell electric vehicles (FCEVs) is growing due to the reduction in fuel efficiency by the high weight. However, when an aluminum alloy is used, deterioration in mechanical characteristics caused by hydrogen embrittlement and wear is regarded as a problem. In this investigation, the aluminum alloy used to prevent hydrogen embrittlement was subjected to surface treatments by performing hard anodizing and plasma ion nitriding processes. The hard anodized Al alloy exhibited brittleness in which the mechanical characteristics rapidly deteriorated due to porosity and defects of surface, resulting in a decrease in the ultimate tensile strength and modulus of toughness by 15.58 and 42.51%, respectively, as the hydrogen charging time increased from 0 to 96 hours. In contrast, no distinct nitriding layer in the plasma ion-nitrided Al alloy was observed due to oxide film formation and processing conditions. However, compared to 0 and 96 hours of hydrogen charging time, the ultimate tensile strength and modulus of toughness decreased by 7.54 and 13.32%, respectively, presenting excellent resistance to hydrogen embrittlement.
참고문헌 (46)
- Yue Hung, "Testing and evaluation of aluminum coated bipolar plates of pem fuel cells operating at 70°C", Journal of Power Sources, 163(1), pp.509~513 (2006), Elsevier BV[DOI]
- 이재봉, "하이드라진으로 환원시킨 그래핀을 코팅한 오스테나이트와 마르텐사이트스테인리스 강 고체고분자형 연료전지 금속 분리판의 전기화학적 특성 평가", CORROSION SCIENCE AND TECHNOLOGY, 15(2), pp.92~107 (2016), 한국부식방식학회[DOI]
- Yang Luo, "Development and application of fuel cells in the automobile industry", Journal of Energy Storage, 42, pp.103124~ (2021), Elsevier BV[DOI]
- 최예지, "알루미늄 1050 합금의 양극산화 시간에 따른 산화피막 성장 거동 및 부식 손상 연구", CORROSION SCIENCE AND TECHNOLOGY, 21(4), pp.282~289 (2022), 한국부식방식학회[DOI]
- Jarmila Woodtli, "Damage due to hydrogen embrittlement and stress corrosion cracking", Engineering Failure Analysis, 7(6), pp.427~450 (2000), Elsevier BV[DOI]
- Sp.G. Pantelakis, "Tensile and energy density properties of 2024, 6013, 8090 and 2091 aircraft aluminum alloy after corrosion exposure", Theoretical and Applied Fracture Mechanics, 33(2), pp.117~134 (2000), Elsevier BV[DOI]
- W.K Jang, "Effect of cathodic hydrogen charging on mechanical properties of Al 8090", Scripta Materialia, 40(4), pp.503~508 (1999), Elsevier BV[DOI]
- E. Serra, "Alumina sputtered on MANET as an effective deuterium permeation barrier", Journal of Nuclear Materials, 257(2), pp.194~198 (1998), Elsevier BV[DOI]
- S.W. Cai, "Study on the inhibition of hydrogen embrittlement of 7050 aluminum alloy in humid air by MAO coating", Anti-Corrosion Methods and Materials, 67(4), pp.387~394 (2020), Emerald[DOI]
- Yizhe Chen, "Analysis of Hydrogen Embrittlement on Aluminum Alloys for Vehicle-Mounted Hydrogen Storage Tanks: A Review", Metals, 11(8), pp.1303~ (2021), MDPI AG[DOI]
- 황현규, "수소연료전지 자동차의 수소밸브용 알루미늄 합금의 저변형율인장실험에 의한 수소취화특성 연구", CORROSION SCIENCE AND TECHNOLOGY, 21(6), pp.503~513 (2022), 한국부식방식학회[DOI]
- "Military Specification MIL-A-8625F, Anodic Coatings for Aluminum and Aluminum Alloys", Naval Air Warfare Center Aircraft Division Lakehurst, ~ (1993)
- Michaela Remešová, "Effects of anodizing conditions and the addition of Al2O3", PTFE particles on the microstructure and the mechanical properties of porous anodic coatings on the AA1050 aluminium alloy, 2020, pp.513, 145780~[DOI]
- Jiru Qin, "Transitions in porous oxide morphologies on AA2024-T3 anodized under high currents and low temperatures: Impact on corrosion behaviour", Electrochimica Acta, 428, pp.140927~ (2022), Elsevier BV[DOI]
- N.C.T. Martins, "Electrodeposition and characterization of polypyrrole films on aluminium alloy 6061-T6", Electrochimica Acta, 53(14), pp.4754~4763 (2008), Elsevier BV[DOI]
- Jihun Oh, "The role of electric field in pore formation during aluminum anodization", Electrochimica Acta, 56(11), pp.4044~4051 (2011), Elsevier BV[DOI]
- Seyyed Hasan Mohitfar, "Characteristics and tribological behavior of the hard anodized 6061-T6 Al alloy", Journal of Alloys and Compounds, 842, pp.155988~ (2020), Elsevier BV[DOI]
- I.C. Chung, "Effect of current density and concentration on microstructure and corrosion behavior of 6061 Al alloy in sulfuric acid", Surface and Coatings Technology, 313, pp.299~306 (2017), Elsevier BV[DOI]
- Francy Catalina García Rueda, "Electrochemical polymerization of polypyrrole coatings on hard-anodized coatings of the aluminum alloy 2024-T3", Electrochimica Acta, 347, pp.136272~ (2020), Elsevier BV[DOI]
- N. Tsyntsaru, "Mechanical and frictional behaviour of nano-porous anodised aluminium", Materials Chemistry and Physics, 148(3), pp.887~895 (2014), Elsevier BV[DOI]
- J. S. Zamarripa-Pina, "Increase in hardness and chloride corrosion resistance of 6061 aluminum alloy by pulsed plasma nitriding", International Journal of Emerging Technology and Advanced Engineering, 3, pp.348~ (2013)
- Yun-Keun Shim, "The properties of AlN prepared by plasma nitriding and plasma source ion implantation techniques", Surface and Coatings Technology, 131(1-3), pp.345~349 (2000), Elsevier BV[DOI]
- K. Taherkhani, "Composite coatings created by new method of active screen plasma nitriding on aluminium alloy 6061", Journal of Alloys and Compounds, 741, pp.1247~1257 (2018), Elsevier BV[DOI]
- C.A. Figueroa, "On the hydrogen etching mechanism in plasma nitriding of metals", Applied Surface Science, 253(4), pp.1806~1809 (2006), Elsevier BV[DOI]
- N. Renevier, "A way to decrease the nitriding temperature of aluminium: the low-pressure arc-assisted nitriding process", Surface and Coatings Technology, 116-119, pp.380~385 (1999), Elsevier BV[DOI]
- P Nageswara Rao, "Effect of annealing on microstructure and mechanical properties of Al 6061 alloy processed by cryorolling", Materials Science and Technology, 29(1), pp.76~82 (2013), SAGE Publications[DOI]
- Masahiro Okumiya, "Surface modification of aluminum using ion nitriding and fluidized bed", Surface and Coatings Technology, 142-144, pp.235~240 (2001), Elsevier BV[DOI]
- E. I. Meletis, "Formation of aluminum nitride by intensified plasma ion nitriding", Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films, 9(4), pp.2279~2284 (1991), American Vacuum Society[DOI]
- Robert A. Youngman, "Luminescence Studies of Oxygen‐Related Defects In Aluminum Nitride", Journal of the American Ceramic Society, 73(11), pp.3238~3246 (1990), Wiley[DOI]
- Leland Rosenberger, "XPS analysis of aluminum nitride films deposited by plasma source molecular beam epitaxy", Surface and Interface Analysis, 40(9), pp.1254~1261 (2008), Wiley[DOI]
- Wen-Yang Chang, "Nanomechanical properties of array TiO2 nanotubes", Microporous and Mesoporous Materials, 145(1-3), pp.87~92 (2011), Elsevier BV[DOI]
- Tatsuya Kikuchi, "Advanced hard anodic alumina coatings via etidronic acid anodizing", Surface and Coatings Technology, 326, pp.72~78 (2017), Elsevier BV[DOI]
- M. Shahzad, "Influence of anodizing process on fatigue life of machined aluminium alloy", Procedia Engineering, 2(1), pp.1015~1024 (2010), Elsevier BV[DOI]
- Richard J. Anton, "Dynamic Vickers indentation of brittle materials", Wear, 239(1), pp.27~35 (2000), Elsevier BV[DOI]
- Y Yamada-Takamura, "Hydrogen permeation barrier performance characterization of vapor deposited amorphous aluminum oxide films using coloration of tungsten oxide", Surface and Coatings Technology, 153(2-3), pp.114~118 (2002), Elsevier BV[DOI]
- E. Serra, "Hydrogen Permeation Measurements on Alumina", Journal of the American Ceramic Society, 88(1), pp.15~18 (2004), Wiley[DOI]
- Wenhai Song, "A study of hydrogen permeation in aluminum alloy treated by various oxidation processes", Journal of Nuclear Materials, 246(2-3), pp.139~143 (1997), Elsevier BV[DOI]
- M. Asadipoor, "Macro- and microscale investigations of hydrogen embrittlement in X70 pipeline steel by in-situ and ex-situ hydrogen charging tensile tests and in-situ electrochemical micro-cantilever bending test", Materials Science and Engineering: A, 772, pp.138762~ (2020), Elsevier BV[DOI]
- Jie Wang, "Performances of AlN coatings as hydrogen isotopes permeation barriers", Fusion Engineering and Design, 102, pp.94~98 (2016), Elsevier BV[DOI]
- Abdul Wasy, "Argon plasma treatment on metal substrates and effects on diamond‐like carbon (DLC) coating properties", Crystal Research and Technology, 49(1), pp.55~62 (2013), Wiley[DOI]
- Hyung-Seop Shin, "Influence of Specimen Surface Roughness on Hydrogen Embrittlement Induced in Austenitic Steels during In-Situ Small Punch Testing in High-Pressure Hydrogen Environments", Metals, 11(10), pp.1579~ (2021), MDPI AG[DOI]
- Jinwoo Kim, "Roughening improves hydrogen embrittlement resistance of Ti-6Al-4V", Acta Materialia, 220, pp.117304~ (2021), Elsevier BV[DOI]
- Yuhshi Fukumoto, "New constructional steels and structural stability", Engineering Structures, 18(10), pp.786~791 (1996), Elsevier BV[DOI]
- J. Michalska, "Hydrogen Damage in Superaustenitic 904L Stainless Steels", Journal of Materials Engineering and Performance, 23(8), pp.2760~2765 (2014), Springer Science and Business Media LLC[DOI]
- W. M. Mook, "Compressive stress effects on nanoparticle modulus and fracture", Physical Review B, 75(21), pp.1~ (2007), American Physical Society (APS)[DOI]
- W.W. Gerberich, "Scale effects for strength, ductility, and toughness in “brittle” materials", Journal of Materials Research, 24(3), pp.898~906 (2009), Springer Science and Business Media LLC[DOI]