NaOCl로 처리된 치수강 상아질에서 sodium ascorbate가 미세인장결합강도에 미치는 영향
INFLUENCE OF SODIUM ASCORBATE ON MICROTENSILE BOND STRENGTHS TO PULP CHAMBER DENTIN TREATED WITH NAOCL
2
조회
0
다운로드
2
인용
0
참고문헌
키워드
초록
The purpose of this study was to evaluate the influence of sodium ascorbate on microtensile bond strengths of total-etching adhesive system to pulp chamber dentin treated with NaOCl. Pulp chambers of extracted human non-caries permanent molars were treated as follows: group 1, with 0.9% NaCl; group 2, with 5.25% NaOCl; group 3, with 5.25% NaOCl and 10% sodium ascorbate for 1min; group 4, with 5.25% NaOCl and 10% sodium ascorbate for 1 min and 10ml of water; group 5, with 5.25% NaOCl and 10% sodium ascorbate for 5 min; group 6, with 5.25% NaOCl and 10% sodium ascorbate for 5 min and 10ml of water; group 7, with 5.25% NaOCl and 10% sodium ascorbate for 10 min; group 8, with 5.25% NaOCl and 10% sodium ascorbate for 10 min and 10ml of water. Treated specimens were dried, bonded with a total-etching adhesive system (Single bond), restored with a composite resin(Z250) and kept for 24h at 100% humidity to measure the microtensile bond strength. NaOCl-treated group (group 2) demonstrated significantly lower strength than the other groups. No significant difference in microtensile bond strengths was found between NaCl-treated group (group 1) and sodium ascorbatetreated groups (group 3-8). The results of this study indicated that dentin treated with NaOCl reduced the microtensile bond strength of Single bond. Application of 10% sodium ascorbate restored the bond strength of Single bond on NaOCl-treated dentin. Application time of sodium ascorbate did not have a significant effect.
Abstract
The purpose of this study was to evaluate the influence of sodium ascorbate on microtensile bond strengths of total-etching adhesive system to pulp chamber dentin treated with NaOCl. Pulp chambers of extracted human non-caries permanent molars were treated as follows: group 1, with 0.9% NaCl; group 2, with 5.25% NaOCl; group 3, with 5.25% NaOCl and 10% sodium ascorbate for 1min; group 4, with 5.25% NaOCl and 10% sodium ascorbate for 1 min and 10ml of water; group 5, with 5.25% NaOCl and 10% sodium ascorbate for 5 min; group 6, with 5.25% NaOCl and 10% sodium ascorbate for 5 min and 10ml of water; group 7, with 5.25% NaOCl and 10% sodium ascorbate for 10 min; group 8, with 5.25% NaOCl and 10% sodium ascorbate for 10 min and 10ml of water. Treated specimens were dried, bonded with a total-etching adhesive system (Single bond), restored with a composite resin(Z250) and kept for 24h at 100% humidity to measure the microtensile bond strength. NaOCl-treated group (group 2) demonstrated significantly lower strength than the other groups. No significant difference in microtensile bond strengths was found between NaCl-treated group (group 1) and sodium ascorbatetreated groups (group 3-8). The results of this study indicated that dentin treated with NaOCl reduced the microtensile bond strength of Single bond. Application of 10% sodium ascorbate restored the bond strength of Single bond on NaOCl-treated dentin. Application time of sodium ascorbate did not have a significant effect.
참고문헌 (22)
- Gutmann JL, "The dentine-root complex : anatomic and biologic considerations in restoring endodontically treated teeth", J Prosthet Dent, 67, pp.458~467 (1992)
- Wagnild GW, "Pathways of the pulp in : Restoration of endodontically treated tooth", pp.691~717 (1994), Mosby
- Ray HA, "Periapical status of endodontically treated teeth in relation to the technical qualty of the root filling and the coronal restoration", Int Endod J, 28, pp.12~18 (1995)
- Ausiello P, "Fracture resistance of endodontically-treated premolars adhesively restored", Am J Dent, 10, pp.237~241 (1995)
- Hernandez R, "Resistance to fracture of endodontically treated premolars restored with new generation dentine bonding systems", Int Endod J, 27, pp.281~284 (1995)
- Belli S, "Adhesive sealing of the pulp chamber", J Endod, 27, pp.521~526 (2001)
- 임연아, "도말층 제거와 상아질의 부위가 치수강 내부 상아질에 대한 수종 상아질 결합제의 전단결합성질에 미치는 영향", 대한치과보존학회지, 24, pp.465~472 (1999)
- 조주연, "AH-26 및 산화아연유지놀 근관실러가 상아질에 대한 복합레진의 전단결합강도에 미치는 영향", 대한치과보존학회지, 31(3), pp.147~152 (2006), 대한치과보존학회
- Nikaido T, "Bond strength to endodontically-treated teeth", Am J Dent, 12, pp.177~180 (1999)
- Lai SC, "Reversal of compromised bonding to oxidized etched dentin", J Dent Res, 80(10), pp.1919~1924 (2001)
- Mirris MD, "Effects of sodium hypochlorite and RC-Prep on bond strengths of resin cement to endodontic surfaces", J Endod, 27(12), pp.753~757 (2001)
- Vongphan N, "Effects of sodium ascorbate on microtensile bond strength of total-etching adhesive system to NaOCl treated dentine", J Dent, 33(8), pp.689~695 (2005)
- Rueggeberg FA, "The effect of oxygen inhibition on an unfilled", filled composite system, 1990, pp.69, 1652~1658
- Weston CH, "Effects of time and concentration of sodium ascorbate on reversal of NaOCl-induced reduction in bond strengths", J Endod, 33(7), pp.879~881 (2007)
- Gutteridge JM, "Biological origin of free radicals, and mechanisms of antioxidant protection", Chem Biol Interact, 91, pp.133~140 (1994)
- VanDuijn MM, "Erythrocytes reduce extracellular ascorbate free radicals using intracellular ascorbate as an electron donor", J Biol Chem, 275, pp.27720~27725 (2000)
- Torneck CD, "Adhesion of light-cured composite resin to bleached and unbleached bovine dentin", Endod Dent Traumatol, 6, pp.97~103 (1990)
- Inai N, "Adhesion between collagen depleted dentin and dentin adhesives", Am J Dent, 11, pp.123~127 (1998)
- Pioch T, "Interfacial micromorphology and tensile bond strength of dentin bonding systems after NaOCl treatment", J Adhes Dent, 1, pp.135~142 (1999)
- Frankenberger R, "Dentin bond strength and marginal adaption after NaOCl pre-treatment", Oper Dent, 25, pp.40~45 (2000)
- Prati C, "Effect of removal of surface collagen fibrils on resin-dentin bonding", Dent Mater, 15, pp.323~321 (1999)
- Rose RC, "Biology of free radical scavengers : an evaluation of ascorbate", FASEB J, 7, pp.1135~1142 (1993)