초록
열순환이 상아질 접착제의 결합 내구성에 미치는 영향문영훈김종률최경규박상진*경희대학교 대학원 치의학과 치과보존학교실THE EFFECT OF THERMOCYCLING ON THE DURABILITY OF DENTIN ADHESIVE SYSTEMSYoung-Hoon Moon, Jong-Ryul Kim, Kyung-Kyu Choi, Sang-Jin Park*
Abstract
열순환이 상아질 접착제의 결합 내구성에 미치는 영향문영훈김종률최경규박상진*경희대학교 대학원 치의학과 치과보존학교실THE EFFECT OF THERMOCYCLING ON THE DURABILITY OF DENTIN ADHESIVE SYSTEMSYoung-Hoon Moon, Jong-Ryul Kim, Kyung-Kyu Choi, Sang-Jin Park*
참고문헌 (51)
- "Clinical evaluation of a posterior composite 10-year report", 27, pp.130~19 (1999)
- "Seventeen year clinical study of ultraviolet-cured posterior composite class I and II restorations", 11, pp.135~142 (1999)
- "Nanoleakage: leakage within the hybrid layer", 20, pp.18~25 (1995)
- "Evidence of chemical bonding at biomaterial? hard tissue interfaces", 79, pp.709~714 (2000)
- "Total-etch, deproteinization and self-etching.", 29, pp.592~598 (2004)
- "Nanoleakage at the dentin adhesive-interface vs. microtensile bond strength", 24, pp.181~188 (1999)
- "Sixmonth storage-time evaluation of one-bottle adhesive systems to dentin", 15, pp.43~49 (2003)
- "Two mondes of nanoleakage expression in single-step adhesives", 81, pp.472~476 (2002)
- "The effect of storage and thermocycling ofthe shear bond strength of three dental adhesive", pp.745~752 (1991)
- "The dentine substrate: structure-and properties related to bonding", 25, pp.441~458 (1997)
- "In vitro aging of dental composites in-water-effect of conversion, filler volume, and filler", matrix coupling, 1998, pp.42, 465~472
- "Thermal cycling procedures forlaboratory testing of dental restorations", 27, pp.89~99 (1999)
- "Long-term Durability of dentine bonds made with a self-etching primer, in vivo.", 78, pp.906~911 (1999)
- "Microtensilebond strengths of seven-dentine adhesive systems", 16, pp.180~187 (2000)
- "Dentin bond durability after three years using a dentin bonding agent with and with-out priming", 12(5), pp.302~307 (1996)
- "The effect of long-termstorage on nano-leakage", 26, pp.609~616 (2001)
- "Itthagarun A. Single-step adhesives are permeable membranes", 30, pp.371~382 (2002)
- "Successful marginal adaptationof a dentin-enamel bonding system in vitro andvivo" (1994), 286-94
- "Comparative microtensile bond strength and SEM analysis of bonding to wet and dentin.", 13, pp.324~328 (2000)
- "Durability of resin dentin interfaces effects of surfacemoisture and adhesive solvent component", 20(7), pp.669~276 (2004)
- "Moisture spectrum of demineralizeddentin for different solvent -based adhesivesystem", 5, pp.183~192 (2003)
- "In vivo longtermdurability of the bond to dentin using two adhesivesystems", 4, pp.151~159 (2002)
- "Influence ofthermal cycling on dentin bond strength of two-stepbonding systems", 11, pp.118~122 (1998)
- "Evaluation of thermal cycling and mechanical loadingon bond strength of a self-etching primer system todentin", 18, pp.269~275 (2002)
- "Effect ofcavity configuration and ageing on the bonding effectivenessof six adhesives to dent in", 21, pp.110~124 (2005)
- "상아질 접착 후 저장기간에 따른 접착제의 접착력의 변화", 30(3), pp.204~205 (2006)
- "The durability of adhesion to phosphoric acid etched, wet dentine substrates", 14, pp.347~352 (1998)
- "International Organization for Standardization Dental materials-guidance on testing of adhesionto tooth structure" (1994)
- "In vivo degradation of resin-dentin bonds in humans over 1 to 3 years", 79, pp.1385~1391 (2000)
- "Influence of thermal cycles in water on flexuralstrength of laboratory-processed composite resin", pp.703~707 (2001)
- "Microleakage of compomer class V restorations: effect of load cycling, thermal cycling, and cavity shape differences", 83, pp.194~203 (2000)
- "The effect oftherm- cycling in microleakage analysis"
- ".Mixed class V restorations:the potentialsof dentine bonding agent" (1990), 263-270
- "Bonding to caries-affected dentin using self-etching primers", 12, pp.309~314 (1999)
- "Dental adhesives of the future", 4, pp.91~103 (2002)
- "A critical review of the durability of adhesion to tooth tissue: methods and results", 84(2), pp.118~132 (2005)
- "The effect of six years of water storage on resin composite bonding to human dentin", 69(1), pp.25~32 (2004)
- "복합레진에 대한 자가부식형 접착제의적합성에 관한 연구", 31 (2006)
- "Microtensile bond strength of a total-etch 3-step and a self-etch 1-step dentin bonding system through 15-month waterstorage", 5, pp.47~56 (2003)
- "Relation between watercontent in acetone", alcohol-based primer and interfacialultrastructure, 1998, pp.26, 147~156
- "The effects ofadhesive thickness on polymerization contraction stressof composite", 79, pp.812~817 (2000)
- "Comparative study onadhesive performance of functional monomers", 83(6), pp.454~458 (2004)
- "Seven-year dentin bond strengths of a total-andself-etch system", 113(3), pp.265~270 (2005)
- "One-year clinical performance of a resin- modifiedglass ionomer and a resin composite restorative materialin unprepared Class V restorations", 27(2), pp.112~116 (2002)
- "Clinical evaluation of a self-etching and aone-bottle adhesive system at two years", 31, pp.527~534 (2003)
- "Degradation patterns of different adhesives and bondingprocedures", 66(1), pp.324~330 (2003)
- "Effect ofdelayed activation of light-cured resin composites onbonding of all-in-one adhesives", 3(3), pp.207~225 (2001)
- "The effect of adhesives with various degrees ofhydrophilicity on resin ceramic bond durability", 20, pp.778~787 (2004)
- "Effects of storage media on mechanical properties ofadhesive systems", 17(2), pp.104~108 (2004)
- "Effect of resin hydrophilicity andwater storage on resin strength", 25, pp.5789~2596 (2004)
- "Effect of resin hydrophilicity and temperature on watersorption of dental adhesive resins", 27(9), pp.1695~1703 (2006)
관련 논문AI추천
산부식형 상아질 접착제의 접착 내구성에 관한 연구박상진, 박상혁, 정미라, 최기운대한치과보존학회 · Restorative Dentistry and Endodontics2007 · 제32권 제4호레진시멘트의 접착 내구성에 관한 연구김종률, 박상혁, 조민우, 최경규대한치과보존학회 · Restorative Dentistry and Endodontics2007 · 제32권 제4호중간레진의 친수성이 상아질 접착에 미치는 영향김용성, 박상혁, 최경규, 최기운대한치과보존학회 · Restorative Dentistry and Endodontics2007 · 제32권 제5호상아질-복합레진 접착계면의 파괴거동에 대한 연구류길주, 박상진, 최경규, 최기운대한치과보존학회 · Restorative Dentistry and Endodontics2007 · 제32권 제3호Cyanate methacrylate가 상아질 결합강도에 미치는 영향김향경, 박상진, 최경규, 최기운대한치과보존학회 · Restorative Dentistry and Endodontics2007 · 제32권 제3호열순환이 상아질접착제처리 후 미세누출에 미치는 영향에 관한 연구유승훈대한턱관절교합학회 · 구강회복응용과학지2008 · 제24권 제2호
이 간행물의 다른 논문 (7건)
2단계 자가 산부식 접착제와 결합된 광중합과 화학중합 복합레진의 법랑질 접착한세희, 조영곤, 김은성pp. 169-179레진전색제의 마모저항성에 대한 평가김수미, 조영곤, 한세희pp. 180-190Mineral trioxide aggregate (MTA)가 치주인대 섬유아세포에서 분비되는 cytokine과 성장인자 TGF- β1, FGF-2 발현에 미치는 영향백승호, 권지윤, 배광식, 이우철, 임성삼, 강명회pp. 191-197수산화칼슘 적용에 따른 상아질 접착제의 접착강도 변화에 관한 연구박노훈, 박상진, 박상혁, 최기운pp. 198-207상아질-복합레진 접착계면의 파괴거동에 대한 연구박상진, 최경규, 최기운, 류길주pp. 208-221