Characteristics of coating films synthesized by a sol-gel reaction using nanosized boehmite

0

조회

0

다운로드

0

인용

0

참고문헌

키워드

주제분류재료공학

초록

We investigated the properties of organic-inorganic hybrid coating films prepared by a sol-gel reaction using a nanosized boehmite sols. The sol was synthesized as a protective coating, functional coating, binder, etc. The sol was prepared from spherically shaped boehmite, and a mixture of spherical and fibrous shaped boehmite. Sol solutions were used to deposit onto substrates by way of a dip-coating process. In order to investigate the surface hydrophobicity, roughness and transmittance of coating films, a contact angle meter, a surface profiler and a UV-Vis spectrophotometer were used. In addition, surface modification of boehmite was investigated by a FT-IR spectrometer. Contact angle and surface roughness of coating films gradually increased with increasing reaction time due to the gelation of the sol by successive condensation reactions. The transmission rate of coating films within the visible-wavelength region was greater than 90% when the reaction time was less than 48 h. FT-IR measurement showed the spectra of condensation of MTMS and boehmite.

Abstract

We investigated the properties of organic-inorganic hybrid coating films prepared by a sol-gel reaction using a nanosized boehmite sols. The sol was synthesized as a protective coating, functional coating, binder, etc. The sol was prepared from spherically shaped boehmite, and a mixture of spherical and fibrous shaped boehmite. Sol solutions were used to deposit onto substrates by way of a dip-coating process. In order to investigate the surface hydrophobicity, roughness and transmittance of coating films, a contact angle meter, a surface profiler and a UV-Vis spectrophotometer were used. In addition, surface modification of boehmite was investigated by a FT-IR spectrometer. Contact angle and surface roughness of coating films gradually increased with increasing reaction time due to the gelation of the sol by successive condensation reactions. The transmission rate of coating films within the visible-wavelength region was greater than 90% when the reaction time was less than 48 h. FT-IR measurement showed the spectra of condensation of MTMS and boehmite.

참고문헌 (11)

  1. Y.J. Du, , Prog. Org. Coat, 41, pp.226~232 (2001)
  2. T.P. Chou, , J. Non-Cryst. Solids, 290, pp.153~162 (2001)
  3. M.S. Lee, , J. Sol-Gel Sci. Tech, 24, pp.175~180 (2002)
  4. J.M. Gomez-Vega, , J. Biomed. Mater. Res, 56, pp.382~389 (2002)
  5. M. Guglielmi, , J. Sol-Gel Sci. Tech, 8, pp.443~449 (1997)
  6. R.A. Weimer, , Appl. Phys. Lett, 51, pp.1179~1181 (1987)
  7. J.A. Calderon-Guillen, , Surf. Coat. Tech, 190, pp.110~114 (2006)
  8. P.M. Glaser, , J. Non-Cryst. Solids, 63, pp.209~221 (1984)
  9. K. Tadanaga, , Sci. Pure Appl. Chem, 31, pp.107~111 (1994)
  10. R. Nass, , Non- Cryst. Solids, 121, pp.370~374 (1990)
  11. 구상만, "Bohemite 나노졸을 이용한 내구성 코팅재료의 제조와 특성에 관한 연구", 공업화학, 17(6), pp.580~585 (2006), 한국공업화학회

관련 논문AI추천

이 간행물의 다른 논문 (16건)