Nanocrystalline materials have received much attention as advanced engineering materials with improved physical and mechanical properties. As nanomaterials possess high strength, high hardness, excellent ductility and toughness, undoubtedly, more attention has been paid to the application of nanomaterials. Nanopowders of Al2O3, TiO2 and MgO were fabricated by high energy ball milling. The simultaneous synthesis and sintering of nanostuctured MgAl2Ti3O10-Mg0.6Al0.8Ti1.6O5 composite from milled powders of 1.4Al2O3, 4.6TiO2 and 1.6MgO was investigated by the high-frequency induction heated sintering process. A highly dense nanostructured MgAl2Ti3O10-Mg0.6Al0.8Ti1.6O5 composite was produced with the simultaneous application of 80 MPa pressure and an induced current within one minute. The grain sizes and mechanical properties (hardness and fracture toughness) of MgAl2Ti3O10-Mg0.6Al0.8Ti1.6O5 composite sintered at 1100 o C were investigated.

Abstract

Nanocrystalline materials have received much attention as advanced engineering materials with improved physical and mechanical properties. As nanomaterials possess high strength, high hardness, excellent ductility and toughness, undoubtedly, more attention has been paid to the application of nanomaterials. Nanopowders of Al2O3, TiO2 and MgO were fabricated by high energy ball milling. The simultaneous synthesis and sintering of nanostuctured MgAl2Ti3O10-Mg0.6Al0.8Ti1.6O5 composite from milled powders of 1.4Al2O3, 4.6TiO2 and 1.6MgO was investigated by the high-frequency induction heated sintering process. A highly dense nanostructured MgAl2Ti3O10-Mg0.6Al0.8Ti1.6O5 composite was produced with the simultaneous application of 80 MPa pressure and an induced current within one minute. The grain sizes and mechanical properties (hardness and fracture toughness) of MgAl2Ti3O10-Mg0.6Al0.8Ti1.6O5 composite sintered at 1100 o C were investigated.

참고문헌 (27)

  1. S. H. Knickerbocker, , Am. Ceram. Soc. Bull, 72, pp.90~95 (1993)
  2. D. R. Bridged Holland, , Glass Technol, 26(6), pp.286~292 (1985)
  3. P. J. Howard, , Proc. Br. Ceram, 49, pp.37~41 (1992)
  4. Shaohong Wang, , Mater. Res. Bull, 38, pp.1367~1374 (2003)
  5. A. H. Kumar, "US Patent 4,301.324", ~ (1981)
  6. 손인진, "Properties and Pulsed Current Activated Consolidation of Nanostuctured MgSiO3-MgAl2O4 Composites", Metals and Materials International, 19(5), pp.1041~1045 (2013), 대한금속·재료학회[DOI]
  7. 곽승미, "볼 밀링한 분말의 펄스전류활성 소결에 의한 나노구조의 지르코니아 제조와 기계적 성질", 대한금속·재료학회지, 51(5), pp.341~348 (2013), 대한금속·재료학회[DOI]
  8. M. Sherif El-Eskandarany, , J. Alloys & Compounds, 305, pp.225~238 (2000)
  9. L Fu, , Scripta Materialia, 44, pp.1061~1068 (2001)
  10. K Niihara, "Advanced structural Inorganic Composite" (1990), Elsevier Scientific Publishing Co.
  11. S Berger, , Progress in Materials, 42, pp.311~320 (1997)
  12. Z Fang, , Int. J. of Refractory Met. & Hard Mater, 13, pp.297~303 (1995)
  13. A. I. Y. Tok, , Materials Science and Engineering A, 383, pp.229~234 (2004)
  14. Woon Jin Chung, "Thermal and Structural Role of Additives in P2O5-ZnO-Sb2O3 Glass for Low Expansion Sealing Materials", Metals and Materials International, 18(1), pp.109~113 (2012), 대한금속·재료학회
  15. 고인용, "고주파유도 가열에 의한 나노구조 MoSi_2-TaSi_2 복합재료 제조 및 기계적 특성", 대한금속·재료학회지, 50(5), pp.369~374 (2012), 대한금속·재료학회[DOI]
  16. 이건우, "고 에너지 볼 밀링이 알루미나 소결과 기계적 성질에 미치는 영향", 대한금속·재료학회지, 51(2), pp.95~100 (2013), 대한금속·재료학회[DOI]
  17. 박나라, "NiAl3 첨가가 (W,Ti)C 초경재료 소결 및 기계적 성질에 미치는 영향", 대한금속·재료학회지, 51(10), pp.753~759 (2013), 대한금속·재료학회[DOI]
  18. J. Jung, , Scripta Materialia, 56, pp.561~564 (2007)
  19. Seung-Mi Kwak, "Rapid synthesis and consolidation of nanostructured MgAl2O4 compound by pulsed current activated sintering and its mechanical properties", Journal of Ceramic Processing Research, 14(1), pp.65~69 (2013), 세라믹공정연구센터[DOI]
  20. 손인진, "The effect of milling time on the properties of binderless nanostuctured (W,Ti)C consolidated by pulsed current activated sintering", Journal of Ceramic Processing Research, 13(3), pp.272~277 (2012), 세라믹공정연구센터[DOI]
  21. 강현수, "고주파 유도 가열에 의한 급속 나노구조 MgTiO_3 화합물 합성 및 소결", 대한금속·재료학회지, 50(12), pp.891~896 (2012), 대한금속·재료학회[DOI]
  22. C. Suryanarayana, "X-ray Diffraction A Practical Approach" (1998), Plenum Press
  23. Z. Shen, , J. Am. Ceram. Soc, 85, pp.1921~1927 (2002)
  24. J. E. Garay, , Appl. Phys. Lett, 85, pp.573~575 (2004)
  25. J. R. Friedman, , Intermetallics, 12, pp.589~597 (2004)
  26. J. E. Garay, , Acta Mater, 51, pp.4487~4495 (2003)
  27. K. Niihara, , J. Mater. Sci. Lett, 1, pp.12~16 (1982)

관련 논문AI추천

이 간행물의 다른 논문 (10건)