본문 바로가기
KERD
논문KCI 등재

Synthesis and characterization of Y1XVO4 : EuX 3+ nanoparticles by using starch as an impregnating matrix

0

조회

0

다운로드

4

인용

0

참고문헌

키워드

주제분류재료공학

초록

The nano-sized Y1XVO4 : EuX3+ powders were synthesized by impregnation method using starch and metal salts(Y;YCl3 • 6H2O,V;VOSO4 • 6H2O, Eu;EuCl3 • 6H2O) as starting materials. The synthesized powders were characterized by XRD, FE-SEM andPhotoluminescence. The particle size of the powders were controlled by preparation conditions, such as heat treatmenttemperature and concentration of Eu ion. As a result of the various synthesis conditions, 30 ~ 100 nm sized homogeneousY1XVO4 : EuX3+ particles were obtained at 600-800 oC for 3 hour. Crystallization and the growth of particles were acceleratedwith increasing sintering temperature and concentration of Eu ion. Crystallization of Y1XVO4 : EuX3+ started around 500 oC,which the temperature is pyrolysis of starch, tetragonal phase generated at 600 oC. Moreover, above 600 oC, heat treatment timehad influence on particle growth, and change of the concentration of Eu ion had also influence on growth of a crystal. Emissionintensity of Y1XVO4 : EuX3+ particles were enhanced with increasing heat treatment temperature and concentration of Eu ion.

Abstract

The nano-sized Y1XVO4 : EuX3+ powders were synthesized by impregnation method using starch and metal salts(Y;YCl3 • 6H2O,V;VOSO4 • 6H2O, Eu;EuCl3 • 6H2O) as starting materials. The synthesized powders were characterized by XRD, FE-SEM andPhotoluminescence. The particle size of the powders were controlled by preparation conditions, such as heat treatmenttemperature and concentration of Eu ion. As a result of the various synthesis conditions, 30 ~ 100 nm sized homogeneousY1XVO4 : EuX3+ particles were obtained at 600-800 oC for 3 hour. Crystallization and the growth of particles were acceleratedwith increasing sintering temperature and concentration of Eu ion. Crystallization of Y1XVO4 : EuX3+ started around 500 oC,which the temperature is pyrolysis of starch, tetragonal phase generated at 600 oC. Moreover, above 600 oC, heat treatment timehad influence on particle growth, and change of the concentration of Eu ion had also influence on growth of a crystal. Emissionintensity of Y1XVO4 : EuX3+ particles were enhanced with increasing heat treatment temperature and concentration of Eu ion.

참고문헌 (19)

  1. C. H. Huang, , Opt. Comm, 224, pp.1~4 (2003)
  2. Q. Mingxin, , Appl. Opt. Vol, 32(12), pp.2085~2086 (1993)
  3. Y. Wang, , Mat. Res. Bull, 41, pp.2147~2153 (2006)
  4. Y. Liu, , J. Allo. and Comp, 653, pp.126~134 (2015)
  5. Y. -S. Chang, , J. Lumin, 129, pp.1181~1185 (2009)
  6. A. Huignard, , J. Phys. Chem, 107(28), pp.6754~6759 (2003)
  7. 장재영, "고상법으로 합성한 YVO4:Eu3+ 적색 형광체의 비대칭비와 발광 특성", 전기전자재료학회논문지, 25(4), pp.298~303 (2012), 한국전기전자재료학회
  8. M. N. Luwang, , J. Mater. Chem, 21, pp.5326~5337 (2011)
  9. V. B. Bhatkar, , IJESIT, 2(1), pp.426~432 (2013)
  10. 최성호, "수열합성에 의해 제조된 YVO₄:Eu³+ 형광체의 발광특성", 한국재료학회지, 18(10), pp.511~514 (2008), 한국재료학회
  11. B. A. Miura, , J. Lumin, 159, pp.93~99 (2015)
  12. K. Uematsu, , J. Allo. and Comp, 408-412, pp.860~863 (2006)
  13. 박우정, "Luminescence characterization of YVO₄: Eu³+, Bi³+ red phosphor by rapid microwave heating synthesis", 한국결정성장학회지, 18(4), pp.169~173 (2008), 한국결정성장학회
  14. L. Yanhong, , J. Solid. Sta. Chem, 178, pp.645~649 (2005)
  15. W.M. Yen, "Phorphos handbook", pp.192~ (2007), CRC Press
  16. M. Yun, , J. Lumin, 68, pp.335~339 (1996)
  17. F. W. Kang, , Chin. Phys. Lett, 28(10), pp.4~ (2011)
  18. B. F. dos Santos Jr., , Solid State Science, 42, pp.45~51 (2015)
  19. Y. Y. Zuo, , J. Lumin, 132, pp.61~63 (2012)

관련 논문AI추천

이 간행물의 다른 논문 (14건)