초록
The optimum powder to ball ratio was examined, which is one of the important conditions in reactive mechanical grinding processing. Yttria (Y2O3)-stabilized zirconia (ZrO2) (YSZ), Ni, and graphene were chosen as additives to enhance the hydriding and dehydriding rates of Mg. Samples with a composition of 92.5 wt% Mg + 2.5 wt% YSZ + 2.5 wt% Ni + 2.5 wt% graphene (designated as Mg-2.5YSZ-2.5Ni-2.5graphene) were prepared by grinding in hydrogen atmosphere. Mg-2.5YSZ-2.5Ni2.5graphene had a high effective hydrogen-storage capacity of almost 7 wt% (6.85 wt%) at 623 K in 12 bar H2 at the second cycle (n = 2). Mg-2.5YSZ-2.5Ni-2.5graphene contained Mg2Ni phase after hydriding-dehydriding cycling. Mg-2.5YSZ-2.5Ni2.5graphene had a larger quantity of hydrogen absorbed for 60 min, Ha (60 min), than Mg-2.5Ni-2.5graphene and Mg2.5graphene. The addition of YSZ also increased the initial dehydriding rate and the quantity of hydrogen released for 60 min, Hd (60 min), compared with those of Mg-2.5Ni-2.5graphene. Y2O3-stabilized ZrO2, Ni, and graphene-added Mg had a higher initial hydriding rate and a larger Ha (60 min) than Fe2O3, MnO, or Ni and Fe2O3-added Mg at n = 1.
Abstract
The optimum powder to ball ratio was examined, which is one of the important conditions in reactive mechanical grinding processing. Yttria (Y2O3)-stabilized zirconia (ZrO2) (YSZ), Ni, and graphene were chosen as additives to enhance the hydriding and dehydriding rates of Mg. Samples with a composition of 92.5 wt% Mg + 2.5 wt% YSZ + 2.5 wt% Ni + 2.5 wt% graphene (designated as Mg-2.5YSZ-2.5Ni-2.5graphene) were prepared by grinding in hydrogen atmosphere. Mg-2.5YSZ-2.5Ni2.5graphene had a high effective hydrogen-storage capacity of almost 7 wt% (6.85 wt%) at 623 K in 12 bar H2 at the second cycle (n = 2). Mg-2.5YSZ-2.5Ni-2.5graphene contained Mg2Ni phase after hydriding-dehydriding cycling. Mg-2.5YSZ-2.5Ni2.5graphene had a larger quantity of hydrogen absorbed for 60 min, Ha (60 min), than Mg-2.5Ni-2.5graphene and Mg2.5graphene. The addition of YSZ also increased the initial dehydriding rate and the quantity of hydrogen released for 60 min, Hd (60 min), compared with those of Mg-2.5Ni-2.5graphene. Y2O3-stabilized ZrO2, Ni, and graphene-added Mg had a higher initial hydriding rate and a larger Ha (60 min) than Fe2O3, MnO, or Ni and Fe2O3-added Mg at n = 1.
참고문헌 (43)
- 송명엽, "Formation of a High Pressure Form of Magnesium Hydride γ-MgH2 by Mechanical Grinding under Low Hydrogen Pressure", 대한금속·재료학회지, 51(2), pp.119~123 (2013), 대한금속·재료학회[DOI]
- Y. Wang, , Int. J. Hydrogen Energy, 44(29), pp.15239~15245 (2019)
- S. Niyomsoan, , Int. J. Hydrogen Energy, 44(29), pp.23257~23266 (2019)
- M. Y. Song, , Int. J. Hydrogen Energy, 44(29), pp.3779~3789 (2019)
- Y. J. Kwak, , J. Nanosci. Nanotech, 18(9), pp.6040~6046 (2018)
- M. Y. Song, , Mater. Res. Bull, 108, pp.23~31 (2018)
- Young Jun Kwak, "Development of a Hydrogen Uptake-Release Mg-Based Alloy by Adding a Polymer CMC (Carboxymethylcellulose, Sodium Salt) via Reaction-Accompanying Milling", Metals and Materials International, 24(5), pp.1181~1190 (2018), 대한금속·재료학회[DOI]
- 홍성현, "Hydrogen Storage Characteristics of Melt Spun Mg-23.5Ni-xCu Alloys and Mg-23.5Ni-2.5Cu Alloy Mixed with Nb_2O_5 and NbF_5", 대한금속·재료학회지, 49(4), pp.298~303 (2011), 대한금속·재료학회
- J. J. Reilly, , Inorg. Chem, 7(11), pp.2254~2256 (1968)
- J. M. Boulet, , J. Less-Common Met, 89, pp.151~161 (1983)
- W. Oelerich, , J. Alloys Compd, 322, pp.L5~L9 (2001)
- Z. Dehouche, , J. Alloys Compd, 347, pp.319~323 (2002)
- G. Barkhordarian, , Scripta Materialia, 49, pp.213~217 (2003)
- G. Barkhordarian, , J. Alloys Compd, 407(1-2), pp.249~255 (2006)
- O. Friedrichs, , Scripta Materialia, 54(7), pp.1293~1297 (2006)
- O. Friedrichs, , Acta Materialia, 54(1), pp.105~110 (2006)
- K. F. Aguey-Zinsou, , Mat. Res. Bull, 41(6), pp.1118~1126 (2006)
- M. Y. Song, , J. Alloys Compd, 340, pp.256~262 (2002)
- S. Long, , J. Alloys Compd, 580(Supplement 1), pp.S167~S170 (2013)
- S. Long, , J. Alloys Compd, 615(Supplement 1), pp.S684~S688 (2014)
- 송준일, "Powder characteristics of Fe2O3 nanopowder agglomerates fabricated by high energy ball milling at various speed and spray-drying processes", Journal of Ceramic Processing Research, 19(4), pp.279~284 (2018), 청정에너지연구소[DOI]
- 박철우, "Effects of high-energy ball milling of commercial Y2O3 powders on their densification using spark plasma sintering", Journal of Ceramic Processing Research, 19(2), pp.179~182 (2018), 청정에너지연구소[DOI]
- 심수만, "Characterization of NiO nanoparticle coating on YSZ powder prepared by precipitation", Journal of Ceramic Processing Research, 19(1), pp.1~4 (2018), 청정에너지연구소[DOI]
- 홍성현, "MgH2 and Ni-Coated Carbon-Added Mg Hydrogen-Storage Alloy Prepared by Mechanical Alloying", 대한금속·재료학회지, 54(2), pp.125~131 (2016), 대한금속·재료학회[DOI]
- 송명엽, "Enhancement of Hydrogen Storage Characteristics of Mg by Addition of Nickel and Niobium (V) Fluoride via Mechanical Alloying", 대한금속·재료학회지, 54(3), pp.210~216 (2016), 대한금속·재료학회[DOI]
- 송명엽, "Hydrogen Storage Characteristics of Metal Hydro-Borate and Transition Element-Added Magnesium Hydride", 대한금속·재료학회지, 54(7), pp.503~509 (2016), 대한금속·재료학회[DOI]
- 권성남, "Hydrogen Storage and Release Properties of Transition Metal-Added Magnesium Hydride Alloy Fabricated by Grinding in a Hydrogen Atmosphere", 대한금속·재료학회지, 54(7), pp.510~518 (2016), 대한금속·재료학회[DOI]
- M. Y. Song, , Int. J. Hydrogen Energy, 35, pp.10366~10372 (2010)
- 송명엽, "Comparison of the Hydrogen Release Properties of Zn(BH4)2-Added MgH2 Alloy and Zn(BH4)2 and Ni-Added MgH2 Alloy", 대한금속·재료학회지, 56(3), pp.244~251 (2018), 대한금속·재료학회
- M. Y. Song, , J. Alloys Compd, 270, pp.164~167 (1998)
- M. Y. Song, , Bull. Mater. Sci, 37(4), pp.831~835 (2014)
- M. Y. Song, , J. Alloys Compd, 415, pp.266~270 (2006)
- S.N. Kwon, "Improvement of the hydrogen absorption and desorption kinetics of Mg by catalytic effects of Fe2O3 and Ni", M.E., pp.2008
- 송명엽, "Fe2O3, MnO, and VCl3-added Mg composites by reactioninvolving grinding processing for hydrogen storage", Journal of Ceramic Processing Research, 19(3), pp.211~217 (2018), 청정에너지연구소[DOI]
- Myoung Youp Song, "TiCl3 and Ni-added Mg prepared by reactive mechanical grinding processing and comparison with Fe2O3 and Niadded Mg", Journal of Ceramic Processing Research, 20(2), pp.173~181 (2019), 청정에너지연구소[DOI]
- 홍성현, "Hydrogen Absorption and Release Properties of MgH2, Mg2Ni, and Ni-Added Mg via Reactive Mechanical Grinding", 대한금속·재료학회지, 56(2), pp.155~162 (2018), 대한금속·재료학회[DOI]
- 송명엽, "Development of a Mg-Based Alloy with a Hydrogen-Storage Capacity of 7 wt% by Adding a Polymer CMC via Transformation-Involving Milling", 대한금속·재료학회지, 56(5), pp.392~399 (2018), 대한금속·재료학회
- 송명엽, "Hydrogen Storage Properties of Mg-Graphene Composites", 대한금속·재료학회지, 56(7), pp.524~531 (2018), 대한금속·재료학회[DOI]
- 송명엽, "Hydrogen Uptake and Release Characteristics of Mg-xTaF5-xVCl3 (x=1.25, 2.5, and 5)", 대한금속·재료학회지, 56(8), pp.611~619 (2018), 대한금속·재료학회[DOI]
- 송명엽, "Raising the Dehydrogenation Rate of a Mg-CMC (Carboxymethylcellulose, Sodium Salt) Composite by Alloying Ni via Hydride-Forming Milling", 대한금속·재료학회지, 56(8), pp.620~627 (2018), 대한금속·재료학회[DOI]
- 송명엽, "Hydrogen Storage Properties of Mg Alloy Prepared by Incorporating Polyvinylidene Fluoride via Reactive Milling", 대한금속·재료학회지, 56(12), pp.878~884 (2018), 대한금속·재료학회[DOI]