본문 바로가기
KERD
논문KCI 등재

Anatomical Features Affecting Safranine Solution Permeability in Anthocephalus chinensis (Lam.) Rich. ex Walp.

0

조회

0

다운로드

0

인용

0

참고문헌

초록

Abstract

This report describes the wood anatomy and 1% safranine solution penetration depth in radial and longitudinal directions of Anthocephalus chinensis belonging to the family Rubiaceae native to Bangladesh. The wood of this species was mostly characterized by diffuse porous, vessel with simple perforation plate, vestured alternate intervessel pittings, relatively medium vessel elements and fiber, and nonseptate fiber with distinctly bordered pits at radial wall. The body ray cell was procumbent with 2 to over 4 rows of upright and square marginal cells. Sometimes, the rays with procumbent, square and upright cells were mixed. Latewood fiber was thin to thick walled while it was very thin walled in earlywood. Axial parenchyma was diffuse, vasicentric, 5-8 cells per parenchyma strand dominantly present. Liquid penetration depth was observed in radial and longitudinal directions at moisture level of 7.42%. Longitudinal penetration was found 6.3 times higher than radial penetration. The initial penetration rate of safranine solution was high, but gradually decreased during the course of time. Different anatomical features were found to be responsible for the variation of safranine solution penetration depth compared to Gmelina arborea.

참고문헌 (14)

  1. Ahmed, S. A, "Descriptions of the wood anatomy and safranine impregnation in Gmelina arborea Roxb. From Bangladesh", 18(2), pp.100~105 (2007)
  2. Baas, "P. and Z. Xinying. 1986. Wood anatomy of tree and shrubs form China. I. Oleaceae. IAWA Bull. n. s. 4", pp.141~159
  3. Bao, F, "On the permeability of main wood species in China", 53, pp.350~354 (1999)
  4. Brandis, "B. L. 1963. The Chemistry of Wood. Interscience Publishers", pp.767~
  5. Chong, S. H, "Safranine penetration path observed by optical microscope in four Korean pine wood species.", 18(2), pp.138~142 (2007)
  6. Chun, S. K, "Permeability and meniscus phenomenon in four Korean softwood species", 8(3), pp.56~60 (2006)
  7. Exley, "B. A. Meylan and B. G. Butterfield. 1977. A technique for obtaining clear cut surfaces on wood samples prepared for the scanning electron microscope. J. Microscopy. 110", pp.75~78
  8. Hillis, "W. E. 1987. Heartwood and Tree Exudates. Springer-Verlag", Berlin
  9. "IAWA Committee. 1989. IAWA list of microscopic features of hardwood identification. IAWA Bull. n..s. 10"
  10. Kumar, "S. and P. B. Dobriyal. 1993. Penetration indices of hardwoods a quantitative approach to define treatability. Wood Fiber Sci. 25"
  11. Troup, "R. S. 1921. The Silviculture of Indian Trees. Oxford", U.K. Clarendon Press.
  12. Wang, J. Z, "Treatability and durability of heartwood", pp.252~260 (1996), Madison, WI: USDA, Forest Service, Forest Products Laboratory
  13. Whitmore, "T. C. 1984. Tropical Rain Forests of the Far East. Oxford", U.K. Clarendon Press.
  14. Zabala, "N. Q. 1990. Silviculture of Anthocephalus chinensis. In Silviculture of species. Chittagong."

관련 논문AI추천

이 간행물의 다른 논문 (10건)