Lateral Conduction of Preservative Solution in Larix kaempferi Woods

0

조회

0

다운로드

0

인용

0

참고문헌

키워드

초록

An experiment was conducted to observe the 5% CCFZ solution penetration depth through ray parenchyma and ray tracheid of Larix kapempferi. Moisture content was adjusted 28% for both sapwood and heartwood. Even though the moisture content was same, heartwood was 1.3 times less permeable than sapwood and the difference was found statistically significant. Due to anatomical differences between ray parenchyma and ray tracheid, ray parenchyma was about 1.3 times more permeable than ray tracheid. Penetration speed was high initially and it decreased rapidly in course of time.

Abstract

An experiment was conducted to observe the 5% CCFZ solution penetration depth through ray parenchyma and ray tracheid of Larix kapempferi. Moisture content was adjusted 28% for both sapwood and heartwood. Even though the moisture content was same, heartwood was 1.3 times less permeable than sapwood and the difference was found statistically significant. Due to anatomical differences between ray parenchyma and ray tracheid, ray parenchyma was about 1.3 times more permeable than ray tracheid. Penetration speed was high initially and it decreased rapidly in course of time.

참고문헌 (16)

  1. Ahmed, S. A, "Essential oil penetration depth in Prunus sargentii Rehder", J. Korea Furniture Society, 18(4), pp.307~311 (2007)
  2. Ahmed, S. A, "Anatomical features affecting safranine solution permeability in Anthocephalus chinensis (Lam.) Rich. ex Walp", J. Korea Furniture Society, 18(4), pp.261~267 (2007)
  3. Ahmed, S. A, "Descriptions of the wood anatomy and safranine impregnation in Gmelina arborea Roxb. from Bangladesh", J. Korea Furniture Society, 18(2), pp.100~105 (2007)
  4. Ahmed, S. A, "Ray parenchyma and ray tracheid structure of four Korean pine wood species", J. Korea Furniture Society, 17(4), pp.101~107 (2006)
  5. Ahmed, S. A, "Effect of pressure on liquid absorbance in main wood species of Pinaceae grown in Korea using safranine under vacuum", J. Korea Furniture Society, 16(2), pp.2~11 (2005)
  6. Bamberr, A. K, "and heartwood: A review", Forestry Abstr, 46(9), pp.567~580 (1985)
  7. Browning,B.L, "The Chemistry of Wood", pp.48~ (1963), Interscience Publishers
  8. Chun, S. K, "Permeability and meniscus phenomenon in four Korean softwood species", For. Stud. China, 8(3), pp.56~60 (2006)
  9. Desch, H. E, "Timber: Structure, Properties, Conversion and Use", pp.306~ (1996), Macmillan Press Ltd.
  10. Eaton, R.A, "Wood: decay pests and protection" (1993), Chapman & Hall
  11. Erickson,H.D, "Permeability of southern pine wood-A review", Wood Science, 2(3), pp.149~158 (1970)
  12. Krahmerr, R. L, "Changes in coniferous wood cells associated with heartwood formation", Tappi, 46(1), pp.42~49 (1963)
  13. McQuire,A.J, "Radial permeability of tim", 박사, pp.1970
  14. Usta, I, "Radial permeability of sitka spruce as affected by wood structure", IAWA J, 24(2), pp.197~204 (2003)
  15. Walker, J. C. F, "Primary Wood Processing", pp.595~ (1993), Chapman and Hall
  16. Wirspa, V. J, "Penetration of neutral sulphite cooking liquors into yellow birch wood", Tappi, 33(5), pp.225~231 (1950)

이 간행물의 다른 논문 (8건)