초록

Mechanical properties of Y2O3-containing tetragonal ZrO2 polycrystals(Y-TZP) were investigated. Several additives were used to modify the hardness and fracture toughness of Y-TZP. The effects of these individual additives were discussed and their interactions were also analysed. Each additive, such as CoO, Fe2O3, MnO2 was found to deteriorate the mechanical properties of Y-TZP when it was used singly. But the fracture toughness of Y-TZP was significantly improved when these additives and Al2O3 were added in combination at a certain ratio. The addition of CoO, Fe2O3 and MnO2 into Y-TZP resulted in the more complex behavior of fracture toughness and hardness. The specimen with 1.5 wt%-Fe2O3, 3.0 wt% -Al2O3 and 1.5 wt%-CoO showed the monoclinic to tetragonal phase ratio of 18% and the highest toughness of 10.8 MPaㆍm1/2 with Vickers hardness of 1201 kgf/mm2. However, the toughness decreased as the ratio increased and macrocracks developed beyond the ratio of 25%. Sample No. 16 is improved high Physical and Mechanical Properties.

Abstract

Mechanical properties of Y2O3-containing tetragonal ZrO2 polycrystals(Y-TZP) were investigated. Several additives were used to modify the hardness and fracture toughness of Y-TZP. The effects of these individual additives were discussed and their interactions were also analysed. Each additive, such as CoO, Fe2O3, MnO2 was found to deteriorate the mechanical properties of Y-TZP when it was used singly. But the fracture toughness of Y-TZP was significantly improved when these additives and Al2O3 were added in combination at a certain ratio. The addition of CoO, Fe2O3 and MnO2 into Y-TZP resulted in the more complex behavior of fracture toughness and hardness. The specimen with 1.5 wt%-Fe2O3, 3.0 wt% -Al2O3 and 1.5 wt%-CoO showed the monoclinic to tetragonal phase ratio of 18% and the highest toughness of 10.8 MPaㆍm1/2 with Vickers hardness of 1201 kgf/mm2. However, the toughness decreased as the ratio increased and macrocracks developed beyond the ratio of 25%. Sample No. 16 is improved high Physical and Mechanical Properties.

참고문헌 (11)

  1. O. Yamamoto, "Electrical Conductivity of Polycrystalline Tetragonal Zirconia ZrO2-M2O3 (M=Sc, Y, Yb)", J. Mater. Sci. Lett, 8, pp.198~200 (1989)
  2. P. Duran, "Preparation, Sintering and Properties of Translucent Er2O3-Doped Tetragonal Zirconia", J.Am. Ceram. Soc., 72(11), pp.2088~2093 (1989)
  3. T. Masaki, "Mechanical Properties of Toughened ZrO2 - Y2O3 Ceramics", J.Am.Ceram. Soc., 69(8), pp.638~640 (1986)
  4. E.C. Subbarao, "Zirconia-an Overview, in Science and Technology of Zirconia", pp.1~24 (1981), The American Ceramic Society
  5. W.Pada, "Zirconia Stabilized with a Mixture of the Rare Earth Oxides", J.Eur.Ceram. Soc., 10, pp.453~459 (1992)
  6. M.V. Swain, "Strength Limitation of Transformation Toughened Zirconia Alloys", J. Am. Ceram. Soc., 69(7), pp.511~518 (1986)
  7. D. Michel, "Fracture of Metastable Tetragonal Zirconia Crystals", J. Mater. Sci, 18, pp.2618~2628 (1983)
  8. 정의영, "반도체 산업의 성과 분석을 통한 메모리 산업의 미래 전략 도출", (사)디지털산업정보학회 논문지, 11(4), pp.1~12 (2015), (사)디지털산업정보학회[DOI]
  9. 박상혁, "성공적인 6차산업을 위한 가치사슬 모형과 빅데이터 활용 방안", (사)디지털산업정보학회 논문지, 11(2), pp.141~152 (2015), (사)디지털산업정보학회[DOI]
  10. 김정주, "부분안정화 지르코니아 요업체의 상변태에 따른 미세구조 및 기계적 성질", 요업재료의 과학과 기술, 3(3), pp.217~223 (1988)
  11. J. H. Lee, "Fabrication and Characteristics of Y-TZP", Ce-TZP Structural Ceramics, 1996, pp.33(10), 1177~1185

관련 논문AI추천

이 간행물의 다른 논문 (20건)