초록
Abstract
Statement of problems. Conventional feldspathic porcelain is used extensively as a restorative material and it is subjected to grinding and polishing during fabrication and delivery procedures. There is still considerable controversy concerning the best methods to achieve the strongest porcelain restorations after such adjustments. Purpose. The objective of this study was to investigate the effects of (1) overglazing, (2) selfglazing, and (3) fine polishing on the flexural strength and fracture toughness of feldspathic dental porcelain. Material and method. Ninety porcelain disks were prepared for flexural strength test and sixty porcelain disks were fabricated for fracture toughness test. Specimens were divided into three groups for each test as follows: 1) overglazed 2) self-glazed 3) polished. The flexural strength of feldspathic porcelains was determined by ring-on-ring biaxial flexural strength test. The fracture toughness values of three experimental groups were obtained by indentation fracture toughness test. Results. The flexural strength of overglazed group was significantly higher than that of selfglazed and polished group (P<0.05), while the difference between self-glazed and polished group was not significant (P>0.05). The fracture toughness values of overglazed and polished group were significantly higher than that of self-glazed group (P<0.05), while the difference between overglazed and polished group was not significant (P>0.05). Conclusions. This results supported the use of polishing as an alternative to glazing metal ceramic restorations, as it was not detrimental in flexural strength and fracture toughness. But, under the conditions of this study, overglazing was the ideal surface finishing method of feldspathic dental porcelain.
참고문헌 (60)
- "The reinforcement ofdental porcelain with ceramic oxides", 119, pp.251~5 (1965)
- "The shrink-free ceramic crown", 49, pp.182~7 (1983)
- "The castable ceramiccrown", 4, pp.32~46 (1984)
- "Magnesia ceramic jacket crowns", 29, pp.719~23 (1985)
- "All-ceramic bridges with the slip castingtechnique", paris, pp.~1988 (1988)
- "Heatpressed ceramics:Technology and strength", 5, pp.9~16 (1992)
- "Effect of surface finishon the flexural strength of feldspathic andaluminous dental ceramics", 8, pp.311~9 (1995)
- "High strength ceramics", 18(2), pp.97~106 (1987)
- "Flexural strengthof feldspathic porcelain treated with ion exchange,overglaze,and polishing", 71, pp.468~72 (1994)
- "The science and art of dental ceramics The nature of dental ceramics and theirclinical use", 1 (1979), Quintessence Publishing Co
- "The nature of machining damage onbrittle materials", 385, pp.461~75 (1993)
- "Scanning electronmicroscopy and profilometer evaluation ofglazed and polished dental porcelain", 9, pp.452~8 (1996)
- "The influence of surfaceroughness and surface-free energy on supra- andsubgingival plaque formation in man", 22, pp.1~14 (1995)
- "The influenceof surface free energy and surface roughnesson early plaque formation", 17, pp.138~44 (1990)
- "Studies on the wear ofporcelain,enamel and gold", 25, pp.299~306 (1971)
- "The reinforcement ofdental porcelain with ceramic oxides", 119, pp.251~67 (1965)
- "Effects of laboratory finishing techniqueson the mechanical properties of dental ceramics", 69, pp.1039~45 (1987)
- "An evaluation of porcelainstrength and the effect of surface treatment", 61, pp.446~51 (1989)
- "A comparisonof glazed and polished dental porcelain", 2, pp.524~9 (1989)
- "The effect of glaze on porcelain strength", 8, pp.203~7 (1992)
- "Effects offlaw size and auto-glaze treatment on porcelainstrength", 75(6), pp.1414~7 (1996)
- "Effects ofgrinding,polishing and overglazing on the flexurestrength of a high-leucite feldspathic porcelain", 9, pp.30~7 (1996)
- "Influence of test method onfailure stress of brittle dental materials", 69, pp.1791~9 (1990)
- "Biaxial flexuretests of ceramic substrates", 7, pp.188~94 (1972)
- "Deflection of centrally loaded thin circular elasticplates on equally spaced point supports", 70, pp.227~44 (1966)
- "Biaxial flexure tests for ceramics", 59, pp.1193~7 (1980)
- "Apparent fracture toughnessof dental porcelain with a metal substructure", 4, pp.187~90 (1988)
- "Studies on fracture toughness of dental ceramics", 17, pp.551~63 (1990)
- "Acritical evaluation of indentation techniques for measuringfracture toughness", pp.533~8 (1981)
- "The abrasive effect of glazed and polished porcelain on the wear ofhuman enamel and the influence of carbonated softdrinks on the rate of wear", pp.269~82 (1997)
- "Roughness of pontic materialsand dental plaque", 23, pp.407~11 (1970)
- "Clinical discrimination between autoglazed andpolished porcelain surfaces", 64, pp.631~5 (1990)
- "A study of porcelainsurfaces as utilized in fixed prosthodontics", 34, pp.314~9 (1975)
- "An improved biaxial flexure testfor ceramics", 59, pp.551~3 (1980)
- "Measurement of tensile strength of ceramics", 51(2), pp.111~ (1968)
- "Review:Uniaxial compressive testsand the validity of indirect tensile strength", 25, pp.757~80 (1990)
- "Relative flexuralstrength of dental restorative ceramics", 6, pp.181~4 (1990)
- "Relative flexural strengthof six new ceramic materials", 8, pp.239~46 (1995)
- "Dynamic fatigue oftreated high-silica glass:explanation by crack tipblunting", 70, pp.377~82 (1987)
- "Dental Ceramics-Proceedings of the FirstInternational Symposium on Ceramics", pp.83~141 (1983)
- "Transverse strength of aluminousand feldspathic porcelain", 53, pp.683~90 (1974)
- "Surface roughnessand flexural strength of self-glazed,polished,andreglazed In-Ceram", Vitadur Alpha porcelain laminates, 2000, pp.13, 66~71
- "The strength of two-phaseceramic", glass materials, 1968, pp.3, 629~34
- "Perspectives on strength", 11, pp.103~10 (1995)
- "Fracture mechanics principles", 11, pp.111~2 (1995)
- "Failure Analysis of Brittle Materials Advances in Ceramics", pp.28~ (1990)
- "Design data for engineeringceramics:A review of the flexural test", 74, pp.2037~66 (1991)
- "Fracture surface energy of glass", 52, pp.99~105 (1969)
- "Fracturetoughness of commercial dental porcelains", 2, pp.58~62 (1986)
- "Fracture mechanics applied to brittlematerials ASTM STP678" (1978)
- "Occurrence of crack formation duringVickers indentation as a measure of the toughnessof hard metals", 33, pp.629~33 (1962)
- "Effect of firing temperatureand water exposure on crack propagation inunglazed porcelain", 68, pp.1075~81 (1989)
- "Post indentation slow growthof radial cracks in glasses", 64 (1981)
- "Thermal expansion of dental alloysand porcelains", 14, pp.435~46 (1980)
- "Effect of cooling rate onleucite volume fraction in dental porcelains", 70, pp.137~9 (1991)
- "Isothermal anneal effecton microcrack density around leucite particlesin dental porcelain", 73, pp.1221~7 (1994)
- "A study of flaw size in porcelain" (1994)
- "Influence of tempering and contraction mismatchon crack development in ceramic surfaces", 70, pp.131~6 (1989)
- "The science of ceramicmachining and surface finishing Ⅲ NationalBureau of Standards", pp.352~60 (1977)
- "Residual stress in machined ceramic surfaces", pp.44~7 (1986)